Study of welding peak temperatures on microstructures and hardness of heat affected zone in 2024-T3 aluminium alloy

被引:5
|
作者
Chen, C. S. [2 ]
Yang, J. G. [3 ]
Tan, A. H. [1 ]
机构
[1] Ching Yun Univ, Dept Mech Engn, Jhongli 320, Taiwan
[2] Lunghwa Sci & Technol Univ, Dept Mech Engn, Guai Shan 333, Taiwan
[3] Chung Shan Inst Sci & Technol, Lungtan, Taiwan
关键词
Aluminium; Welding peak temperatures; Heat affected zone; Gleeble simulation; Microstructure; Hardness; STIR WELDED-JOINTS; MG ALLOYS; FRICTION; BEHAVIOR; FRACTURE; CRACKING;
D O I
10.1179/174328408X374676
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of welding thermal cycle peak temperatures and post-weld heat treatments on the microstructures and mechanical properties of the heat affected zone (HAZ) for 2024-T3 aluminium alloy have been investigated by Gleeble HAZ simulation. Differential scanning calorimetry (DSC) in conjunction with transmission electron microscopy (TEM) is used to characterise the HAZ microstructures. The welded HAZ in the region of peak temperature 414 degrees C has the lowest hardness after natural aged temper, which is primarily due to the precipitation and coarsening of stable S phases. When the peak temperature of welded HAZ is larger than 414 degrees C, the hardness of HAZ increasing with an increasing peak temperature can be seen, which is due to higher peak temperature thermal cycles treatment inducing the dissolution of precipitations in the matrix, and, after the natural aging treatment, Guinier-Preston (GPB) and GPB2 zones precipitating out in the matrix again can be seen. Post-weld T81 artificial aging (PWAA-T81) heat treatment has no effect on improving the HAZ hardness; the HAZ hardness of the 2024-T3 alloy obtained by PWAA-T81 is less than that obtained by natural aging, and its lowest hardness is shifted to the region of peak temperature, which is 452 degrees C, because overaging induces coarse and sparse amounts of stable S phase.
引用
收藏
页码:896 / 904
页数:9
相关论文
共 50 条
  • [21] Augmented Laser Impact Welding: A New Process Demonstration in Welding Aluminum Alloy 2024-T3
    Thurston, Brian
    Lewis, Troy
    Li, Jianxiong
    Vivek, Anupam
    Daehn, Glenn
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (21) : 12031 - 12042
  • [22] Effect of trivalent chromium process on fatigue lifetime of 2024-T3 aluminium alloy
    Akanou, Myriam
    Saillard, Romain
    Fori, Benoit
    Blanc, Christine
    Odemer, Gregory
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 743 : 322 - 326
  • [23] Effect of contact geometry on fretting fatigue life of aluminium alloy 2024-T3
    Farrahi, GH
    Majzoobi, GH
    Chinekesh, H
    INDIAN JOURNAL OF ENGINEERING AND MATERIALS SCIENCES, 2005, 12 (04) : 331 - 336
  • [24] Influence of pre-treatments on the surface condition of 2024-T3 aluminium alloy
    Pires, I
    Quintino, L
    Rangel, CM
    Thompson, GE
    Skeldon, P
    Zhou, X
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 2000, 78 : 179 - 185
  • [25] Deformation and dissipated energies for high cycle fatigue of 2024-T3 aluminium alloy
    Giancane, S.
    Chrysochoos, A.
    Dattoma, V.
    Wattrisse, B.
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2009, 52 (02) : 117 - 121
  • [26] Friction stir spot welding of 2024-T3 aluminum alloy with SiC nanoparticles
    Paidar, Moslem
    Sarab, Mahsa Laali
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2016, 30 (01) : 365 - 370
  • [27] Friction stir spot welding of 2024-T3 aluminum alloy with SiC nanoparticles
    Moslem Paidar
    Mahsa Laali Sarab
    Journal of Mechanical Science and Technology, 2016, 30 : 365 - 370
  • [28] Comparative study of spot welding and firiction stir spot welding of Al 2024-T3
    Fahmy M.H.
    Abdel-Aleem H.A.
    Elkousy M.R.
    Abdel-Elraheem N.M.
    Key Engineering Materials, 2019, 786 : 104 - 118
  • [29] A study on the corrosion fatigue characteristics of Al 2024-T3 alloy
    Duan, RC
    Shi, HJ
    ADVANCES IN FRACTURE AND FAILURE PREVENTION, PTS 1 AND 2, 2004, 261-263 : 1343 - 1348
  • [30] Corrosion protection of aluminium alloy 2024-T3 in 0.05 M NaCl by cerium cinnamate
    Shi, Hongwei
    Han, En-Hou
    Liu, Fuchun
    CORROSION SCIENCE, 2011, 53 (07) : 2374 - 2384