Surface coverage-limited hydrogen uptake into nickel under cathodic charging

被引:7
|
作者
Jiang, Lai [1 ]
Demkowicz, Michael J. [1 ]
机构
[1] Texas A&M Univ, Dept Mat Sci & Engn, College Stn, TX 77843 USA
关键词
Hydrogen; Nickel; Cathodic charging; Surface coverage; Adsorption; Absroption; THERMAL-DESORPTION SPECTROSCOPY; EVOLUTION KINETICS; DIFFUSION; 1ST-PRINCIPLES; STEEL; EMBRITTLEMENT; BEHAVIOR; HYDRIDES; NI(111); ENTRY;
D O I
10.1016/j.corsci.2022.110280
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We investigate hydrogen (H) uptake into 50 mu m-thick pure nickel (Ni) foils under cathodic charging in 1 M H2SO4 solution. We measure H concentration using melt extraction as a function of charging time and overpotential. For every overpotential, H concentration reaches a time-independent, equilibrium value after ~8 h of charging. The measured H concentrations are systematically lower than expected for the applied overpotentials and approach an upper bound asymptotically as a function of charging current density. To rationalize these findings, we propose that H uptake is surface H coverage-dependent and reaches an upper limit when the sample surface becomes saturated with H. Saturation of surface coverage, in turn, occurs when the dominant H evolution re-action (HER) pathway switches from Volmer-Tafel to Volmer-Heyrovsky.
引用
收藏
页数:9
相关论文
共 50 条