The mechanism of critical strain and serration type of the serrated flow in Mg-Nd-Zn alloy

被引:44
|
作者
Wang, W. H. [1 ,2 ]
Wu, D. [1 ]
Shah, S. S. A. [1 ]
Chen, R. S. [1 ]
Lou, C. S. [2 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Grp Magnesium Alloys & Their Applicat, Shenyang 110016, Peoples R China
[2] Shenyang Ligong Univ, Sch Mat Sci & Engn, Shenyang 110159, Peoples R China
基金
中国国家自然科学基金;
关键词
Serrated flow; Magnesium alloy; Portevin-Le Chatelier (PLC); Serration type; Critical strain; MODIFIED 9CR-1MO STEEL; TENSILE PROPERTIES; BEHAVIOR; TEMPERATURE; MAGNESIUM; MICROSTRUCTURE;
D O I
10.1016/j.msea.2015.09.100
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In present research the serrated flow has been observed successfully after a critical amount of strain. Two relationships between the critical strain and temperature i.e. normal and inverse, corresponding to each serration type were studied. In order to investigate systematically the onset of serrated flow and serration type in NZ31 alloy, samples in solutionized condition were tensile tested at the temperature ranging from 100 degrees C to 300 degrees C with the strain rate ranging from 1 x 10(-4) s(-1) to 1 x 10(-2) s(-1). Results showed that normal critical strain appeared with type A and B serrated flow at temperature from 150 degrees C to 250 degrees C, and inverse critical strain appeared with type Cat temperature from 275 degrees C to 300 degrees C. Through analyzing the mechanism of three serration types, we found that the production of serration required improvement in diffusion for solute atoms for pinning process at low temperature, and enhance the moving ability of dislocations for unpinning process at high temperature, which need the assistance of the strain and stress respectively. So, in this work, the critical strain for pinning and the critical stress for unpinning processes were defined, which give a better explanation to the variation tendency of two definitions in accordance with temperature. Furthermore, this relationship results in the critical strain for onset of serrated flow changing from normal to inverse and corresponding different serrations. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:214 / 221
页数:8
相关论文
共 50 条
  • [41] The mechanism for the serrated flow induced by Suzuki segregation in a Ni alloy
    Jiang, Zhouwen
    Zhu, Lilong
    Yu, Lianxu
    Sun, Baoan
    Cao, Yang
    Zhao, Yonghao
    Zhang, Yong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 820
  • [42] Investigation of serrated flow behaviour in Al-10Mg alloy
    Kumar, S
    Rao, KVN
    Surappa, MK
    MATERIALS SCIENCE AND TECHNOLOGY, 2001, 17 (01) : 113 - 115
  • [43] Prediction of flow stress of Mg-Nd-Zn-Zr alloy during hot compression
    Wu Wen-xiang
    Jin Li
    Dong Jie
    Ding Wen-jiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (05) : 1169 - 1175
  • [44] Effect of heat treatment on strain–controlled fatigue behavior of cast Mg–Nd–Zn–Zr alloy
    Zhenming Li
    Qigui Wang
    Alan A.Luo
    Jichun Dai
    Hui Zou
    Liming Peng
    Journal of Materials Science & Technology, 2018, 34 (11) : 2091 - 2099
  • [45] Serration Flow Behavior with Abnormal Strain Rate Sensitivity of Fine-Grained Mg-0.8 Wt Pct Ca Alloy
    Peng, Qiuming
    Fu, Hui
    Xiao, Wenlong
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2013, 44A (10): : 4469 - 4474
  • [46] Serration Flow Behavior with Abnormal Strain Rate Sensitivity of Fine-Grained Mg-0.8 Wt Pct Ca Alloy
    Qiuming Peng
    Hui Fu
    Wenlong Xiao
    Metallurgical and Materials Transactions A, 2013, 44 : 4469 - 4474
  • [47] Effects of Precipitation State on Serrated Flow in Al-Mg(-Zn) Alloys
    Matsumoto, Katsushi
    Aruga, Yasuhiro
    Tsuneishi, Hidemasa
    Iwai, Hikaru
    Mizuno, Masataka
    Araki, Hideki
    MATERIALS TRANSACTIONS, 2016, 57 (07) : 1101 - 1108
  • [48] Effects of precipitation state on serrated flow in Al-Mg(-Zn) alloys
    Materials Research Laboratory, Kobe Steel, Ltd., 1-5-5 Takatsukadai, Nishi-ku, Kobe-shi, Hyogo
    651-2271, Japan
    不详
    不详
    不详
    Keikinzoku J Jpn Inst Light Met, 8 (331-338):
  • [49] Texture and mechanical behavior evolution of age-hardenable Mg-Nd-Zn extrusions during aging treatment
    Ma, Lan
    Mishra, Raja K.
    Peng, Liming
    Luo, Alan A.
    Ding, Wenjiang
    Sachdev, Anil K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 529 : 151 - 155