Formation of nanostructured LaMg2Ni by rapid quenching and intensive milling and its hydrogen reactivity

被引:14
|
作者
Teresiak, A. [1 ]
Uhlemann, M. [1 ]
Gebert, A. [1 ]
Thomas, J. [1 ]
Eckert, J. [1 ]
Schultz, L. [1 ]
机构
[1] IFW Dresden, Leibniz Inst Solid State & Mat Res Dresden, D-01171 Dresden, Germany
关键词
X-ray diffraction; Metal hydrides; Rapid solidification; Gas-solid reactions; Crystal structure; Mg-Ni-La; Y ALLOYS; MICROSTRUCTURE; LA; PERFORMANCE; ELECTRODES; ABSORPTION; HYDRIDE; SYSTEM; TI;
D O I
10.1016/j.jallcom.2009.02.127
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The formation of the nanostructured orthorhombic LaMg2Ni phase using the melt-spinning and the intensive ball milling routes has been studied for the La25Mg50Ni25 and La20Mg50Ni30 compositions. By controlled heat treatment of glassy melt-spun ribbons the formation of the LaMg2Ni phase proceeds at T-A >= 220 degrees C (T-A = annealing temperature) for La25Mg50Ni25 via the initial formation of LaMg3, but occurs for La20Mg50Ni30 already at T-A >= 200 degrees C in a single reaction. Crystallite sizes of LaMg2Ni of approximate to 30 nm were achieved. The formation enthalpies of LaMg2Ni were estimated to Delta H = -320.8 kJ/mol for La25Mg50Ni25 and Delta H = -230.0 kJ/mol for La20Mg50Ni30. Intensive ball milling of inductively molten master alloys using a planetary RETSCH mill for 30 h resulted in a crystallite size reduction, e.g. up to 15 nm for LaMg2Ni. The formation of the complex hydride LaMg2NiH7 was studied for both alloy compositions by annealing rapidly quenched and crystallised as well as intensively ball milled powder under hydrogen. However, the most effective method for achieving the complex hydride as single phase was found to be intensive ball milling in a planetary RETSCH mill under a 0.5 MPa hydrogen atmosphere. The hydride formation reaction was completed within 3 h for La20Mg50Ni30 and within 7.5 h for La25Mg50Ni25. The hydrogen desorption from intensively milled LaMg2NiH7 powder proceeds in two steps. At first, the LaMg2NiH7 decomposes into LaH2-3 and Mg2NiH0.2-0.3 at T-A > 450 degrees C with a decomposition enthalpy of Delta H approximate to 48 kJ/mol and the recombination of LaMg2Ni starts at T-A > 540 degrees C.Above 625 degrees C the LaMg2Ni decomposes by the sublimation of Mg. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:144 / 151
页数:8
相关论文
共 33 条
  • [31] Effect of Rapid Quenching on Microstructures and Electrochemical Performances of La2Mg(Ni0.85Co0.15)9M0.1(M=B, Cr) Hydrogen Storage Alloys
    张羊换
    董小平
    王国清
    冯猛
    任江远
    王新林
    Journal of Rare Earths, 2005, (04) : 460 - 465
  • [33] Effect of rapid quenching on the microstructure and electrochemical characteristics of La0 6Ce0 4Ni3 6Co0 65Mn0 4Al0 2Ti0 05(FeB)0 1 hydrogen storage alloy
    Zhang Peilong
    Song Xiping
    Wang Xiuli
    Pei Pei
    Luo Guiping
    Tu Jiangping
    Chen Guoliang
    RARE METALS, 2010, 29 (06) : 593 - 596