Delamination-resistant bi-layer electrolyte for anode-supported solid oxide fuel cells

被引:9
|
作者
Park, Mi Young [1 ]
Jung, Yeon-Gil [1 ]
Lim, Hyung-Tae [1 ]
机构
[1] Changwon Natl Univ, Sch Mat Sci & Engn, Chang Won 641773, South Korea
基金
新加坡国家研究基金会;
关键词
Solid oxide fuel cells; Bi-Layer; Cell Imbalance; Delamination; Degradation; OXYGEN; FAILURE; ION;
D O I
10.1016/j.ssi.2014.02.013
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
One of the critical fuel cell degradation phenomena is 'cell imbalance' in a series-connected stack, which can cause abnormal operation under a negative cell voltage and consequently rapid degradation by anode interface delamination. In a previous study, the effect of electrolyte composition on the electrochemical degradation of solid oxide fuel cell (SOFC) was investigated, and it was observed that a small amount of ceria (an electronic conducting material) prevents anode delamination under abnormal (negative voltage) operation. However, the open circuit voltage (OCV) was lowered as a result of reduction of ceria. In the present study, bi-layer, YSZ (8 mol % yttria doped zirconia, a predominantly ionic conductor) at the cathode side and 8CYSZ (8 mol % ceria doped YSZ, a mixed ionic-electronic conductor) at the anode side were fabricated for anode-supported cells with a Pt probe embedded in each layer to estimate the internal oxygen chemical potential and tested under a negative voltage. The results indicated that the OCV was close to the theoretical value (similar to that of a YSZ single layer cell) and no delamination was observed under negative voltage operation (similar to the case of an 8CYSZ single-layer cell). Therefore, the bi-layer-structured electrolyte (with locally increased electronic conduction at the anode side) is effective in preventing anode/electrolyte delamination as well as maintaining open circuit voltage. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:438 / 443
页数:6
相关论文
共 50 条
  • [41] Modelling the leakage current in a solid oxide fuel cell with bi-layer electrolyte
    Krishnamurthy, Balaji
    Ramasubramanian, Hariharan
    JOURNAL OF ELECTROCHEMICAL SCIENCE AND ENGINEERING, 2020, 10 (03): : 293 - 304
  • [42] NiO/YSZ, anode-supported, thin-electrolyte, solid oxide fuel cells fabricated by gel casting
    Zhang, Lan
    Jiang, San Ping
    Wang, Wei
    Zhang, Yujun
    JOURNAL OF POWER SOURCES, 2007, 170 (01) : 55 - 60
  • [43] Reduced-Temperature Firing of Anode-Supported Solid Oxide Fuel Cells
    Gao, Zhan
    Barnett, Scott A.
    ELECTROCHEMICAL SYNTHESIS OF FUELS 2, 2013, 58 (02): : 231 - 242
  • [44] Effects of Reduced Firing Temperature on Anode-Supported Solid Oxide Fuel Cells
    Gao, Zhan
    Barnett, Scott A.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2014, 161 (05) : F600 - F604
  • [45] Evaluation and modeling of the cell resistance in anode-supported solid oxide fuel cells
    Leonide, A.
    Sonn, V.
    Weber, A.
    Ivers-Tiffee, E.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2008, 155 (01) : B36 - B41
  • [46] Performance of anode-supported single-chamber solid oxide fuel cells
    Ai Gang
    Lu Zhe
    Wei Bo
    Huang Xiqiang
    Chen Kongfa
    Su Wenhui
    CHINESE JOURNAL OF CATALYSIS, 2006, 27 (10) : 885 - 889
  • [47] Operation of anode-supported solid oxide fuel cells on methane and natural gas
    Liu, JA
    Barnett, SA
    SOLID STATE IONICS, 2003, 158 (1-2) : 11 - 16
  • [48] Anode-supported Solid Oxide Fuel Cells Prepared by Spin-coating
    Yu, Ji Haeng
    Lee, Hee Lak
    Woo, Sang Kuk
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2007, 44 (12) : 733 - 739
  • [49] Low-temperature constrained sintering of YSZ electrolyte with Bi2O3 sintering sacrificial layer for anode-supported solid oxide fuel cells
    Lim, Yonghyun
    Lee, Hojae
    Park, Junghum
    Kim, Young-Beom
    CERAMICS INTERNATIONAL, 2022, 48 (07) : 9673 - 9680
  • [50] Ni-GDC anode-supported ceria electrolyte film and its application in solid oxide fuel cells
    Lin, H.
    Ding, C.
    Kumada, K.
    Sato, K.
    Tsutai, Y.
    Wada, C.
    Hashida, T.
    WATER DYNAMICS, 2008, 987 : 54 - +