Perforation of clamped, woven E-glass/polyester panels

被引:20
|
作者
Fatt, MSH [1 ]
Lin, CF [1 ]
机构
[1] Univ Akron, Dept Mech Engn, Akron, OH 44325 USA
关键词
woven E-glass/polyester laminates;
D O I
10.1016/j.compositesb.2003.04.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Analytical solutions to predict the perforation of fully clamped, woven E-glass/polyester panels subjected to static indentation by a blunt cylinder were derived. Three panel aspect ratios of 12.5, 25 and 50 were considered in order to show how modes of failure vary with panel flexibility. The analytical solutions for the deformation and interlaminar shear stresses compared well to finite element predictions using ABAQUS. It was found that the panel with an aspect ratio of 50 underwent large deformation and deformed in a membrane phase before fracture due to tensile necking. Failure of panels with aspect ratios of 12.5 and 25 was predicted using ply-by-ply failure analysis and the Tsai-Wu failure criterion. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:359 / 378
页数:20
相关论文
共 50 条
  • [41] Four testing and evaluation methods of the spreading effects on E-glass woven fabrics
    Wang, Xi
    Zheng, Tianyong
    Ning, Xiangchun
    [J]. GLASS TECHNOLOGY-EUROPEAN JOURNAL OF GLASS SCIENCE AND TECHNOLOGY PART A, 2021, 62 (06): : 198 - 204
  • [42] Delamination growth behavior of a woven E-glass/bismaleimide composite in seawater environment
    Zhao, Yian
    Liu, Wei
    Seah, Leong Keey
    Chai, Gin Boay
    [J]. COMPOSITES PART B-ENGINEERING, 2016, 106 : 332 - 343
  • [43] The Possibility of E-glass Woven Roving as Reinforcement of GFRP Composite Sheet Roof
    Setyanto, Djoko
    [J]. PROCEEDINGS OF THE 4TH INTERNATIONAL CONFERENCE AND EXHIBITION OF SUSTAINABLE ENERGY AND ADVANCED MATERIALS 2015 (ICE-SEAM 2015), 2016, 1717
  • [44] Quasi-static crush energy absorption capability of E-glass/polyester and hybrid E-glass-basalt/polyester composite structures
    Esnaola, A.
    Ulacia, I.
    Aretxabaleta, L.
    Aurrekoetxea, J.
    Gallego, I.
    [J]. MATERIALS & DESIGN, 2015, 76 : 18 - 25
  • [45] Tensile dynamic behaviour of a quasi-unidirectonal E-glass/polyester composite
    Pardo, S
    Baptiste, D
    Décobert, F
    Fitoussi, J
    Joannic, R
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 2002, 62 (04) : 579 - 584
  • [46] Investigating the creep resistance of E-glass/polyester composite for automotive structural components
    Marye, Sisay Asmare
    Jamir, T. Moansunep
    Desalegn, Yiene Molla
    [J]. DISCOVER APPLIED SCIENCES, 2024, 6 (07)
  • [47] Thermal behavior of E-glass fiber-reinforced unsaturated polyester composites
    Laoubi, K.
    Hamadi, Z.
    Benyahia, A. Ahmed
    Serier, A.
    Azari, Z.
    [J]. COMPOSITES PART B-ENGINEERING, 2014, 56 : 520 - 526
  • [48] THERMAL AGING OF UNSATURATED POLYESTER COMPOSITE REINFORCED WITH E-GLASS NONWOVEN MAT
    Hossain, Md. Milon
    Elahi, A. H. M. Fazle
    Afrin, Shahida
    Mahmud, Md. Iqbal
    Cho, Haeng Muk
    Khan, Mubarak Ahmad
    [J]. AUTEX RESEARCH JOURNAL, 2017, 17 (04) : 313 - 318
  • [49] Thermogravimetric analysis of aluminised E-glass fibre reinforced unsaturated polyester composites
    Ferreira, J. M.
    Errajhi, O. A. Z.
    Richardson, M. O. W.
    [J]. POLYMER TESTING, 2006, 25 (08) : 1091 - 1094
  • [50] LEACHING OF E-GLASS
    ELMER, TH
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1984, 67 (12) : 778 - 782