摘要
Ladle refining is a popular secondary metallurgy process and plays a vital role in achieving the desired chemistry and temperature during steelmaking. The slag produced after ladle refining mostly contains dicalcium silicate (C2S). The presence of high C2S in slag leads to the disintegration of slag into fine powder during cooling due to phase transformation of C2S. The adverse impact is that the dust is easily aerated and carried by wind creating environmental pollution and makes the working area unsafe. In this paper, an attempt was made to study the effect of the addition of different additives on the disintegration of slag. Initial laboratory experiments were conducted with different additives such as Colemanite (boron-based mineral), silica-rich synthetic slag, and a siliceous natural occurring mineral perlite. Analysis of slag samples was carried out before and after treatment with additives. Based on the optimized conditions, industrial trials were conducted with different additives, and its success was measured in terms of lumpy slag formation. It was successfully studied that the addition of 10% of perlite during ladle furnace treatment process helped in preventing the slag disintegration by 90%.
引用
收藏
页码:115 / 125
页数:11
相关论文
共 50 条
  • [21] Use of Solid Slag Mixtures in a Ladle Furnace Unit
    Zolin, A. N.
    Dobromilov, A. A.
    Esil'baev, R. D.
    Shafigulin, R. K.
    Gulyakov, V. S.
    Vusikhis, A. S.
    METALLURGIST, 2022, 66 (5-6) : 698 - 703
  • [22] EFFECTIVE UTILIZATION OF BOF SLAG FOR LADLE REFINING FURNACE
    FURUNO, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (12): : 1101 - 1101
  • [23] A way to reduce environmental impact of ladle furnace slag
    Branca, T. A.
    Colla, V.
    Valentini, R.
    IRONMAKING & STEELMAKING, 2009, 36 (08) : 597 - 602
  • [24] Effect of additives on viscosity of LATS refining ladle slag
    Wang, HM
    Li, GR
    Dai, QX
    Lei, YC
    Zhao, YT
    Li, B
    Shi, GM
    Ren, ZM
    ISIJ INTERNATIONAL, 2006, 46 (05) : 637 - 640
  • [25] Ladle Furnace Slag in the Construction of Embankments: Expansive Behavior
    Montenegro, J. M.
    Celemin-Matachana, M.
    Canizal, J.
    Setien, J.
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2013, 25 (08) : 972 - 979
  • [26] Effect of additives on viscosity of LATS refining ladle slag
    Wang, Hong-Ming
    Li, Gui-Rong
    Xu, Ming-Xi
    Li, Bo
    Zhang, Xue-Jun
    Shi, Guo-Min
    Guocheng Gongcheng Xuebao/The Chinese Journal of Process Engineering, 2006, 6 (02): : 227 - 230
  • [27] Optimization of ladle furnace slag for use as a supplementary cementing material
    Papayianni, I.
    Anastasiou, E.
    MEASURING, MONITORING AND MODELING CONCRETE PROPERTIES, 2006, : 411 - +
  • [28] A Review on Stabilization of Ladle Furnace Slag-Powdering Issue
    Abinash Dash
    Prasenjit Chanda
    P. K. Tripathy
    Nikhil Kumar
    Journal of Sustainable Metallurgy, 2022, 8 : 1435 - 1449
  • [29] Unit Ladle-Furnace: Slag Forming Conditions and Stabilization
    Sheshukov, O. Yu
    Nerkasov, I., V
    Mikheenkov, M. A.
    Egiazaryan, D. K.
    Sivtsov, A., V
    Chencov, V. P.
    Gertsberg, G. E.
    INTERNATIONAL CONFERENCE WITH ELEMENTS OF SCHOOL FOR YOUNG SCIENTISTS ON RECYCLING AND UTILIZATION OF TECHNOGENIC FORMATIONS (TECHNOGEN-2017), 2017, : 70 - 75
  • [30] Characterization of ladle furnace basic slag for use as a construction material
    Setien, J.
    Hernandez, D.
    Gonzalez, J. J.
    CONSTRUCTION AND BUILDING MATERIALS, 2009, 23 (05) : 1788 - 1794