The impact of the growth of thermally grown oxide layer on the propagation of surface cracks within thermal barrier coatings

被引:21
|
作者
Lv, JunNan [1 ]
Fan, XueLing [1 ]
Li, Qun [1 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Strength & Vibrat Mech Struct, Sch Aerosp, Xian 710049, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Thermal barrier coating; Thermally grown oxide; Surface crack; Material configurational forces; J(k)-integral; FAILURE MECHANISMS; ELEVATED-TEMPERATURES; INTERFACIAL FRACTURE; COMPOSITE-MATERIALS; TBC SYSTEMS; BOND COATS; OXIDATION; STRESS; BEHAVIOR; TGO;
D O I
10.1016/j.surfcoat.2016.10.039
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Failure mechanisms of thermal barrier coating system (TBCs) are complicated, wherein spalling of ceramic top coat (TC) caused by the interfacial oxidation is the most important factor. The present paper focuses on clarifying the impact of continuous formation of thermally grown oxide (TGO) on the shielding/anti-shielding and deflection of surface cracks within the TC. The growth stress in the TC due to the expansion of TGO layer is taken into account by introducing a new three-layered model in TBCs where the initial residual stress in TC is also presented. The theory of material configurational force is innovatively used to analyze the influence of the growth of TGO layer on the crack-tip driving force, i.e., the J(k)-integral. A fracture criterion is employed to predict the deflection of lengthways propagation of the surface crack via the maximum energy release rate associated with J(k)-integral. The influences of the key factors such as the initial crack length, the initial crack inclination angle, the magnitude of growth eigenstrain of TGO, the dwelling time of TGO at elevated temperature on the propagation of surface cracks are analyzed. Numerical results verify that the growth of TGO layer significantly impacts the failure of TBCs, particularly the lateral growth behavior of TGO layer is the key factor influencing the initiation and propagation of surface crack at elevated temperature. The lateral expansion growth of TGO layer induced additional tensile stress in TC can accelerate the initiation of surface cracks. Furthermore, the TGO growth can partly suppress/enhance the deflection of surface crack depending on the inclination angle and the suppression/enhancement effect becomes stronger as the dwelling (oxidation) time increases. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:1033 / 1044
页数:12
相关论文
共 50 条
  • [31] Analysis of Thermally Grown Oxide Developed by Thermal Barrier Coatings with the Aid of Selective Deep Etching
    Tawancy H.M.
    Tawancy, H. M. (tawancy@kfupm.edu.sa), 2013, Springer Science and Business Media, LLC (02) : 88 - 95
  • [32] Optimizing thermally grown oxide for thermal barrier coatings on TiAl components via fluorine treatment
    A. Donchev
    R. Braun
    M. Schütze
    JOM, 2010, 62 : 70 - 74
  • [33] TEM study on microstructure of thermally grown oxide in EB-PVD thermal barrier coatings
    Hu, MH
    Guo, SQ
    Tomimatsu, T
    Ikuhara, Y
    Kagawa, Y
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (20-21): : 6130 - 6136
  • [34] The effect of morphology of thermally grown oxide on the stress field in a turbine blade with thermal barrier coatings
    Zhu, W.
    Cai, M.
    Yang, L.
    Guo, J. W.
    Zhou, Y. C.
    Lu, C.
    SURFACE & COATINGS TECHNOLOGY, 2015, 276 : 160 - 167
  • [35] Effect of Thermal Spraying Method, Time and Temperature on the Thickness of Thermally Grown Oxide and Lifetime of Thermal Barrier Coatings
    Rahimi, Javad
    Poursaeidi, Esmaeil
    Montakhabi, Farzam
    Sigaroodi, Mohammad Rasoul Javadi
    Jamalabad, Yousef Yousefi
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2023, 32 (08) : 2580 - 2602
  • [36] Effect of Thermal Spraying Method, Time and Temperature on the Thickness of Thermally Grown Oxide and Lifetime of Thermal Barrier Coatings
    Javad Rahimi
    Esmaeil Poursaeidi
    Farzam Montakhabi
    Mohammad Rasoul Javadi Sigaroodi
    Yousef Yousefi Jamalabad
    Journal of Thermal Spray Technology, 2023, 32 : 2580 - 2602
  • [37] Microstructural evolution and growth kinetics of thermally grown oxides in plasma sprayed thermal barrier coatings
    Xiaoju Liu
    Teng Wang
    Caicai Li
    Zhenhuan Zheng
    Qiang Li
    ProgressinNaturalScience:MaterialsInternational, 2016, 26 (01) : 103 - 111
  • [38] Microstructural evolution and growth kinetics of thermally grown oxides in plasma sprayed thermal barrier coatings
    Liu, Xiaoju
    Wang, Teng
    Li, Caicai
    Zheng, Zhenhuan
    Li, Qiang
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2016, 26 (01) : 103 - 111
  • [39] Experimental study of a thin thermally grown oxide layer in thermal barrier coatings based on the SWT-BP algorithm and terahertz technology
    Luo, Manting
    Zhong, Shuncong
    Huang, Yi
    Zhang, Zhenghao
    Nsengiyumva, Walter
    Tu, Wanli
    APPLIED OPTICS, 2024, 63 (13) : 3430 - 3437
  • [40] Analysis of the Cr3+ luminescence spectra from thermally grown oxide in thermal barrier coatings
    Selcuk, A
    Atkinson, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 335 (1-2): : 147 - 156