Fracture and toughening mechanisms in SiC nanofiber reinforced SiC matrix nanocomposites with amorphous carbon coatings

被引:8
|
作者
Li, Lili [1 ]
Niu, Jianbing [2 ]
Yang, Yanqing [4 ]
Xia, Zhenhai [2 ,3 ]
机构
[1] Fujian Univ Technol, Sch Mat Sci & Engn, Fuzhou 350108, Peoples R China
[2] Univ N Texas, Dept Mat Sci & Engn, Denton, TX 76203 USA
[3] Univ N Texas, Dept Chem, Denton, TX 76203 USA
[4] Northwestern Polytech Univ, Sch Mat Sci & Engn, Xian 710072, Peoples R China
基金
美国国家科学基金会;
关键词
Molecular dynamic simulation; Mechanical properties; Coatings; Interface/interphase; Nanocomposites; HIGH-STRENGTH; COMPOSITES; DESIGN; POTENTIALS; SIMULATION; TOUGHNESS;
D O I
10.1016/j.commatsci.2013.11.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fracture behavior of SiC matrix nanocomposites reinforced by SiC nanofiber coated with amorphous carbon (a-C) coatings is studied via molecular dynamics simulations. The a-C coating plays a significant role in the tensile strength, and fracture energy of the nanocomposites. With increasing thickness of the a-C coating, the failure behavior of nanocomposites transitions from brittle fracture to a non-catastrophic mode of ductile performance while the tensile strength increases. An introduction of appropriate functionally-graded a-C coating can significantly enhance nanofiber pullout and thus pullout energy by an order of magnitude. Our results suggest that material design directions - coating thickness and the functionally-graded coating - are all efficient approaches for engineering nanoscale SiC/SiC composites for high strength and toughness. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:255 / 260
页数:6
相关论文
共 50 条
  • [41] THE ROLE OF THE MATRIX IN SiC REINFORCED COMPOSITES
    Madej, Marcin
    Leszczynska-Madej, Beata
    Wasik, Anna
    Kopec-Surzyn, Anna
    COMPOSITES THEORY AND PRACTICE, 2023, 23 (01): : 30 - 36
  • [42] Evaluation of interface fracture toughness in SiC fiber reinforced titanium matrix composite
    Yuan Mei-ni
    Yang Yan-qing
    Huang Bin
    Li Jian-kang
    Chen Yan
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2008, 18 (04) : 925 - 929
  • [43] Fracture behaviour of SiC fibre-reinforced nitrogen glass matrix composites
    Zhang, E
    Thompson, DP
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (24) : 6423 - 6429
  • [44] THE FRACTURE-BEHAVIOR OF SIC REINFORCED SIALYON CERAMIC-MATRIX COMPOSITES
    KASPRZAK, E
    BARBAUX, Y
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C7): : 1923 - 1926
  • [45] Evaluation of interface fracture toughness in SiC fiber reinforced titanium matrix composite
    原梅妮
    杨延清
    黄斌
    李健康
    陈彦
    Transactions of Nonferrous Metals Society of China, 2008, (04) : 925 - 929
  • [46] Interfacial microstructure and fracture behavior of SiC whisker reinforced magnesium matrix composites
    Zheng, MY
    Wu, K
    Yao, CK
    Kamado, S
    Kojima, Y
    MAGNESIUM ALLOYS 2003, PTS 1 AND 2, 2003, 419-4 : 795 - 800
  • [47] Interfacial optimization of SiC nanocomposites reinforced by SiC nanowires with high volume fraction
    Ruan, Jing
    Yang, Jinshan
    Dong, Shaoming
    Yan, Jingyi
    Zhang, Xiangyu
    Ding, Yusheng
    Zhou, Haijun
    Hu, Jianbao
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2019, 102 (09) : 5033 - 5037
  • [48] FRACTURE-TOUGHNESS OF SIC FIBER-REINFORCED LAS MATRIX COMPOSITES
    KAGAWA, Y
    KISHI, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (12) : 1470 - 1478
  • [49] Amorphous SiC coatings for WC cutting tools
    Costa, AK
    Camargo, SS
    SURFACE & COATINGS TECHNOLOGY, 2003, 163 : 176 - 180
  • [50] Preparation of Carbon Fiber Reinforced SiC Matrix Composites By PIP Process
    Zhang, Quanqing
    Zeng, Tao
    Cheng, Su
    ADVANCED MATERIALS AND ENGINEERING MATERIALS II, 2013, 683 : 124 - +