Fracture and toughening mechanisms in SiC nanofiber reinforced SiC matrix nanocomposites with amorphous carbon coatings

被引:8
|
作者
Li, Lili [1 ]
Niu, Jianbing [2 ]
Yang, Yanqing [4 ]
Xia, Zhenhai [2 ,3 ]
机构
[1] Fujian Univ Technol, Sch Mat Sci & Engn, Fuzhou 350108, Peoples R China
[2] Univ N Texas, Dept Mat Sci & Engn, Denton, TX 76203 USA
[3] Univ N Texas, Dept Chem, Denton, TX 76203 USA
[4] Northwestern Polytech Univ, Sch Mat Sci & Engn, Xian 710072, Peoples R China
基金
美国国家科学基金会;
关键词
Molecular dynamic simulation; Mechanical properties; Coatings; Interface/interphase; Nanocomposites; HIGH-STRENGTH; COMPOSITES; DESIGN; POTENTIALS; SIMULATION; TOUGHNESS;
D O I
10.1016/j.commatsci.2013.11.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fracture behavior of SiC matrix nanocomposites reinforced by SiC nanofiber coated with amorphous carbon (a-C) coatings is studied via molecular dynamics simulations. The a-C coating plays a significant role in the tensile strength, and fracture energy of the nanocomposites. With increasing thickness of the a-C coating, the failure behavior of nanocomposites transitions from brittle fracture to a non-catastrophic mode of ductile performance while the tensile strength increases. An introduction of appropriate functionally-graded a-C coating can significantly enhance nanofiber pullout and thus pullout energy by an order of magnitude. Our results suggest that material design directions - coating thickness and the functionally-graded coating - are all efficient approaches for engineering nanoscale SiC/SiC composites for high strength and toughness. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:255 / 260
页数:6
相关论文
共 50 条
  • [1] Toughening Mechanisms in Carbon Nanotube-Reinforced Amorphous Carbon Matrix Composites
    Niu, J. B.
    Li, L. L.
    Xu, Q.
    Xia, Z. H.
    CMC-COMPUTERS MATERIALS & CONTINUA, 2013, 38 (01): : 31 - 41
  • [2] Mullite-bonded SiC-whisker-reinforced SiC matrix composites: Preparation, characterization, and toughening mechanisms
    Luo, Yang
    Zheng, Shi-li
    Ma, Shu-hua
    Liu, Chun-li
    Wang, Xiao-hui
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (16) : 5282 - 5293
  • [3] FRACTURE MECHANISMS OF A 2124 ALUMINUM MATRIX COMPOSITE REINFORCED WITH SIC WHISKERS
    KIM, YH
    LEE, SH
    KIM, NJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1992, 23 (09): : 2589 - 2596
  • [4] FATIGUE FRACTURE MECHANISMS FOR SIC WHISKERS AND SIC PARTICULATES REINFORCED ALUMINUM COMPOSITES
    MASUDA, C
    TANAKA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1989, 75 (09): : 1753 - 1760
  • [5] Toughening mechanisms and properties of mullite matrix composites reinforced by the addition of SiC particles and Y-TZP
    Hong, JS
    Huang, XX
    Guo, JK
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (18) : 4847 - 4852
  • [6] Study on the fracture behavior and toughening mechanism of Si3N4/SiC(n)/SiC(w) nanocomposites
    Dong, LM
    Wang, C
    Tian, JM
    RARE METAL MATERIALS AND ENGINEERING, 2003, 32 : 196 - 198
  • [7] AMORPHOUS SIC PVD COATINGS
    KNOTEK, O
    LOFFLER, F
    WOLKERS, L
    DIAMOND AND RELATED MATERIALS, 1993, 2 (2-4) : 528 - 530
  • [8] Analysis on Toughening Mechanisms of Different SiC Particle Reinforced Thermal Protective Ceramics
    Liang Jun
    Wang Chao
    Luan Xu
    Wang Baolai
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 : 894 - 897
  • [9] Damage and toughening mechanisms of carbon fibers reinforced carbon matrix composites
    Aly-Hassan, MS
    Hatta, H
    Wakayama, S
    Miyagawa, K
    DE SIGN, MANUFACTURING AND APPLICATIONS OF COMPOSITES, 2003, : 444 - 451
  • [10] Epoxy nanocomposites - fracture and toughening mechanisms
    Wetzel, Bernd
    Rosso, Patrick
    Haupert, Frank
    Friedrich, Klaus
    ENGINEERING FRACTURE MECHANICS, 2006, 73 (16) : 2375 - 2398