Cracking tendency and drying skrinkage of silica fume concrete for bridge deck applications

被引:0
|
作者
Whiting, DA [1 ]
Detwiler, RJ
Lagergren, ES
机构
[1] Construct Technol Labs Inc, Skokie, IL 60077 USA
[2] Nabisco Inc, Parsippany, NJ 07054 USA
关键词
bridge decks; concretes; cracking; shrinkage; silica fume;
D O I
暂无
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper presents the results of a study of the cracking tendency and drying shrinkage of silica fume concretes designed for full-depth and overlay placements of highway bridge decks. Mixtures for each application were prepared over a range of silica fume silica fume contents and water-cementitious material ratios (w/cm). Concrete laboratory specimens were prepared for testing of unrestrained drying shrinkage and tendency to crack using a restrained ring geometry. Regression analyses were performed on data developed from the laboratory testing and response surface models, and analyses of variance were carried out. The results demonstrated that the tendency of concrete to crack is influenced by the addition of silica fume only when the concrete is improperly cured. When concrete is cured for 7 days under continuously moist conditions, there is no statistically significant effect of silica fume on the tendency of the concrete to exhibit early-age cracking Silica fume has little effect on the ultimate (long-term) shrinkage of concrete; concretes containing silica fume do not shrink more than otherwise identical concretes without silica fume. At early ages, however, silica fume concrete mixtures show somewhat higher shrinkages than their conventional counterparts. Concrete containing silica fume is more sensitive to changes in w/cm than conventional concrete in terms of the shrinkage that develops at early ages It is recommended that specifications for silica fume concretes in bridge deck construction include a provision for 7-day continuous moist curing of exposed surfaces.
引用
收藏
页码:71 / 77
页数:7
相关论文
共 44 条
  • [21] Silica fume effect on fracture parameters and cracking pattern maps of recycled aggregate concrete
    Cakir, Ozgur
    Dilbas, Hasan
    [J]. JOURNAL OF THE FACULTY OF ENGINEERING AND ARCHITECTURE OF GAZI UNIVERSITY, 2019, 34 (01): : 137 - 154
  • [22] Effect of drying on the deicer salt scaling resistance of concrete mixtures with and without silica fume
    Marchand, J
    Boisvert, L
    Pigeon, M
    Houdusse, O
    Hornain, H
    [J]. MATERIALS AND STRUCTURES, 1997, 30 (198) : 217 - 224
  • [23] SILICA FUME CONCRETE FOR HIGH-STRENGTH PRECAST PRESTRESSED HIGHWAY BRIDGE GIRDERS
    JOHNSTON, CD
    [J]. FLY ASH, SILICA FUME, SLAG, AND NATURAL POZZOLANS IN CONCRETE, VOL 1-2, 1989, 114 : 1077 - 1100
  • [24] Use of Longitudinal Expansion Joints in Wide-Bridge Applications to Reduce Deck Cracking
    Liu, Zhengyu
    Phares, Brent M.
    Greimann, Lowell F.
    [J]. JOURNAL OF BRIDGE ENGINEERING, 2016, 21 (10)
  • [25] Mechanical performance of concrete pavement reinforced by CFRP grids for bridge deck applications
    Fang, Hai
    Zou, Fang
    Liu, Weiqing
    Wu, Chao
    Bai, Yu
    Hui, David
    [J]. COMPOSITES PART B-ENGINEERING, 2017, 110 : 315 - 335
  • [26] Drying Shrinkage and Cracking Tendency of Concrete Pavement Mixtures with Variable Packing Densities of Aggregates and Paste Contents
    Olek, Jan
    Rudy, Adam
    [J]. SCIENTIFIC-TECHNICAL CONFERENCE: E-MOBILITY, SUSTAINABLE MATERIALS AND TECHNOLOGIES (MATBUD'2020), 2020, 322
  • [27] The Study on the Early Age Cracking due to the Addition of Silica Fume into Concrete and the Trouble-shooting Strategy
    Hwang, Chao Lung
    Chen, Chun Tsun
    Bui, Le Anh Tuan
    Kurniawan, Fondly Reymont
    [J]. MANUFACTURING SCIENCE AND TECHNOLOGY, PTS 1-3, 2011, 295-297 : 824 - 829
  • [28] Autogenous shrinkage of high-strength concrete containing silica fume under drying at early ages
    Yang, Y
    Sato, R
    Kawai, K
    [J]. CEMENT AND CONCRETE RESEARCH, 2005, 35 (03) : 449 - 456
  • [29] Study on the anti-cracking of GFRP bars asphalt concrete bridge deck pavement under the vehicle load
    Feng, Xiaoxin
    He, Xiongjun
    Yang, Zhuhua
    [J]. ADVANCED CONSTRUCTION TECHNOLOGIES, 2014, 919-921 : 1173 - +
  • [30] Causes and controls of cracking at bridge deck overlay with very-early strength latex-modified concrete
    Yun, Kyong-Ku
    Choi, Pangil
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2014, 56 : 53 - 62