Influence of coke thickness on the on-line SiO2/S coating preparation and its thermal shock property

被引:0
|
作者
Wang Zhiyuan [1 ]
Zhou Jianxin [2 ]
Xu Hong [3 ]
机构
[1] Univ Shanghai Sci & Technol, Sch Energy & Power Engn, Shanghai 200093, Peoples R China
[2] Nanjing Univ Technol, Sch Mech & Power Engn, Nanjing 210009, Jiangsu, Peoples R China
[3] E China Univ Sci & Technol, State Key Lab Chem Engn, Shanghai 200237, Peoples R China
关键词
Coke deposition; HP40; specimen; SiO2/S coating; Coating deposition; Thermal shock; DEPOSITION; RESISTANCE; PARTICLES; BEHAVIOR; ALUMINA; IRON;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
SiO2/S coating was prepared on the surface of HP40 specimen with different thicknesses of coke. The influence of coke on the coating deposition and thermal shock property was studied. Scanning electron microscopy, X-ray diffractometry and X-ray energy dispersive spectroscopy were used for microstructure and microchemical analysis. The morphologies of cokes and SiO2/S coatings were investigated. The results show that the oxide layer of HP40 specimen formed at 850 degrees C for 2 hour is porous and mainly composed of (Cr, Fe)-spinel and a small amount of Fe2O3. The coking rate initially is high, then decreases with increasing cracking time, and finally reaches a stable value after 20 minutes. The diameter of coke changes from 1 mu m to 0.2 mu m, and then is about 0.5 mu m. The thickness of the coke layer changes from 0.56 mu m to 2.58 mu m. The thickness of coke layer has an important influence on the morphology and thermal shock property of the on-line SiO2/S coating. With increasing the thickness of the coke layer, the coating becomes rough and incompact. When the thickness of the coke layer is 0.56 mu m, the coating can bear 13 thermal shock tests. And the coating is out of service when the coke layer is 2.58 mu m. It is suggested that a thorough decoking should be carried out to improve the adhesion between the on-line coating and the inner surface of the cracking tube.
引用
收藏
页码:682 / 688
页数:7
相关论文
共 50 条
  • [21] Thermal shock and tritium resistance of SiO2 coating on the inner wall of 316L stainless steel pipeline
    Liu, Dong-Guang
    Yang, Ting-Ting
    Liu, Yu-Lan
    Luo, Lai-Ma
    Wu, Yu-Cheng
    VACUUM, 2021, 185
  • [22] Influence of SiO2 coating preparation process on the oxidation resistance of 3-D carbon fiber braids
    Gao, PZ
    Wang, HJ
    Jin, ZH
    JOURNAL OF INORGANIC MATERIALS, 2003, 18 (04) : 849 - 854
  • [23] Influence of SiO2 coating preparation process on the oxidation resistance of 3D carbon fiber braids
    Gao, Peng-Zhao
    Wang, Hong-Jie
    Jin, Zhi-Hao
    Wuji Cailiao Xuebao/Journal of Inorganic Materials, 2003, 18 (04): : 849 - 854
  • [24] The preparation of superhydrophobic photocatalytic fluorosilicone/SiO2–TiO2 coating and its self-cleaning performance
    Lijun Zong
    Yaping Wu
    Xingeng Li
    Bo Jiang
    Journal of Coatings Technology and Research, 2021, 18 : 1245 - 1259
  • [25] Preparation of a superhydrophobic coating based on polysiloxane modified SiO2 and study on its anti-icing performance
    Liu, Yang
    Zhao, Zhenbo
    Shao, Yawei
    Wang, Yanqiu
    Liu, Bin
    SURFACE & COATINGS TECHNOLOGY, 2022, 437
  • [26] Preparation and performance study of SiO2 aerogel thermal insulation coating with nanoporous structure for wind turbine blade surface
    He, Jianjun
    Huang, Caiyuan
    Pu, Min
    Shu, Zhonghu
    Duan, Zihao
    Zeng, Zijing
    Li, Jianwei
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2024, 38 (13) : 2425 - 2446
  • [27] Microstructure and mechanical property of Al2O3f/SiO2 composites after thermal shock and fatigue tests
    Cao Jie
    Xiang Yang
    Wang Hua-qiong
    Zhu Cheng-xin
    Wang Yi
    Li Guang-de
    Wen Jin
    Cao Feng
    COMPOSITES COMMUNICATIONS, 2020, 17 : 66 - 71
  • [28] Preparation of SiO2 coated Ce2S3 red pigment with improved thermal stability
    陈观宏
    朱振峰
    刘辉
    武英峰
    朱春奎
    Journal of Rare Earths, 2013, 31 (09) : 891 - 896
  • [29] Preparation of SiO2 coated Ce2S3 red pigment with improved thermal stability
    Chen Guanhong
    Zhu Zhenfeng
    Liu Hui
    Wu Yingfeng
    Zhu Chunkui
    JOURNAL OF RARE EARTHS, 2013, 31 (09) : 891 - 896
  • [30] Anti-coking property of the SiO2/S coating during light naphtha steam cracking in a pilot plant setup
    Zhou Jianxin
    Wang Zhiyuan
    Luan Xiaojian
    Xu Hong
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2011, 90 (01) : 7 - 12