Damage Formation in Sn Film Anodes of Na-Ion Batteries

被引:14
|
作者
Li, Tao [1 ,2 ]
Gulzar, Umair [1 ,2 ]
Zaccaria, Remo Proietti [1 ,3 ]
Capiglia, Claudio [1 ]
Hackney, S. A. [4 ]
Aifantis, K. E. [5 ]
机构
[1] Ist Italiano Tecnol, Via Morego 30, I-16163 Genoa, Italy
[2] Univ Genoa, DIBRIS, Via Opera Pia 13, I-16145 Genoa, Italy
[3] Chinese Acad Sci, Ningbo Inst Mat Technol & Engn, Cixi Inst Biomed Engn, Ningbo 315201, Zhejiang, Peoples R China
[4] Michigan Technol Univ, Mat Sci & Engn, Houghton, MI 49931 USA
[5] Univ Florida, Mech & Aerosp Engn, Gainesville, FL 32611 USA
来源
JOURNAL OF PHYSICAL CHEMISTRY C | 2019年 / 123卷 / 24期
基金
美国国家科学基金会;
关键词
HIGH-PERFORMANCE ANODE; NANOCOMPOSITE ANODES; PORE FORMATION; TIN ANODES; SODIUM; LITHIUM; CARBON; ELECTRODES; MECHANISM; NANOPARTICLES;
D O I
10.1021/acs.jpcc.9b02004
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Sn anodes for Na-ion batteries exhibit a promising initial capacity of 847 mAh g(-)1, which however, cannot be retained throughout continuous cycling due to the 420% volume changes that Sn experiences during sodiation. Previous experimental studies suggest that fracture does not occur in the submicron Sn particles during the formation of Na-Sn alloys; however, such colossal volume changes must result in microstructural damage. In the present work, the damage mechanisms during sodiation are isolated and accentuated by employing a Sn thick film of 0.5 mm as the anode. This simplified planar geometry allows to dispense with the influence of the binder and carbon additives that are required in porous electrodes. Post-mortem electron microscopy revealed new deformation mechanisms for anode materials, as multiple whiskers nucleated on the surface of the Sn, whereas pores formed within the Sn (over the Na-ion penetration distance) after electrochemical cycling. These mechanisms were in addition to the dry lake-bed fracture that was also observed. A comparative study on a Sn thin-film anode of 0.06 mm revealed the formation of fracture and pores after cycling, but no whiskers. The whiskers and pores observed in the thick Sn film anode may be more subtle at the nanoscale, and therefore have not been reported for submicron Sn particles in porous electrodes during sodiation.
引用
收藏
页码:15244 / 15250
页数:7
相关论文
共 50 条
  • [31] A DFT study on graphene, SiC, BN, and AlN nanosheets as anodes in Na-ion batteries
    A. Hosseinian
    E. Saedi Khosroshahi
    K. Nejati
    E. Edjlali
    E. Vessally
    [J]. Journal of Molecular Modeling, 2017, 23
  • [32] New Paradigms on the Nature of Solid Electrolyte Interphase Formation and Capacity Fading of Hard Carbon Anodes in Na-Ion Batteries
    Bommier, Clement
    Leonard, Daniel
    Jian, Zelang
    Stickle, William F.
    Greaney, P. Alex
    Ji, Xiulei
    [J]. ADVANCED MATERIALS INTERFACES, 2016, 3 (19):
  • [33] Negative electrodes for Na-ion batteries
    Dahbi, Mouad
    Yabuuchi, Naoaki
    Kubota, Kei
    Tokiwa, Kazuyasu
    Komaba, Shinichi
    [J]. PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2014, 16 (29) : 15007 - 15028
  • [34] Na-ion dynamics in tetragonal and cubic Na3PS4, a Na-ion conductor for solid state Na-ion batteries
    Yu, Chuang
    Ganapathy, Swapna
    de Klerk, Niek J. J.
    van Eck, Ernst R. H.
    Wagemaker, Marnix
    [J]. JOURNAL OF MATERIALS CHEMISTRY A, 2016, 4 (39) : 15095 - 15105
  • [35] Nitrogen doped porous carbon as excellent dual anodes for Li-and Na-ion batteries
    Zhanheng Yan
    Qin-Wen Yang
    Qinghong Wang
    Jianmin Ma
    [J]. Chinese Chemical Letters, 2020, 31 (02) : 583 - 588
  • [36] Structure and ionic conductivity of the solid electrolyte interphase layer on tin anodes in Na-ion batteries
    Kuo, Liang-Yin
    Moradabadi, Ashkan
    Huang, Hsin-Fu
    Hwang, Bing-Joe
    Kaghazchi, Payamn
    [J]. JOURNAL OF POWER SOURCES, 2017, 341 : 107 - 113
  • [37] Nitrogen doped porous carbon as excellent dual anodes for Li- and Na-ion batteries
    Yan, Zhanheng
    Yang, Qin-Wen
    Wang, Qinghong
    Ma, Jianmin
    [J]. CHINESE CHEMICAL LETTERS, 2020, 31 (02) : 583 - 588
  • [38] On the Road to Sustainable Energy Storage Technologies: Synthesis of Anodes for Na-Ion Batteries from Biowaste
    Nieto, Nekane
    Noya, Olatz
    Iturrondobeitia, Amaia
    Sanchez-Fontecoba, Paula
    Perez-Lopez, Usue
    Palomares, Veronica
    Lopez-Urionabarrenechea, Alexander
    Rojo, Teofilo
    [J]. BATTERIES-BASEL, 2022, 8 (04):
  • [39] Porous carbon-free SnSb anodes for high-performance Na-ion batteries
    Choi, Jeong-Hee
    Ha, Choong-Wan
    Choi, Hae-Young
    Seong, Jae-Wook
    Park, Cheol-Min
    Lee, Sang -Min
    [J]. JOURNAL OF POWER SOURCES, 2018, 386 : 34 - 39
  • [40] Hierarchical carbon nanocages as high-rate anodes for Li- and Na-ion batteries
    Zhiyang Lyu
    Lijun Yang
    Dan Xu
    Jin Zhao
    Hongwei Lai
    Yufei Jiang
    Qiang Wu
    Yi Li
    Xizhang Wang
    Zheng Hu
    [J]. Nano Research, 2015, 8 : 3535 - 3543