The electromigration and thermomigration behaviors Pb-free flip chip Sn-3Ag-0.5Cu solder bumps, with UBM (under bump metals) layers Al (0.3 mu m)/Ni(V) (0.3 mu m)/Cu (0.5 mu m) layers, upon current stressing at 120 degrees C were investigated. The current density applied was 1.18 X 10(4)A/cm(2) for all investigations. To investigate the change morphology and composition in the bulk of solder bumps and the IMC layers at the interface between the UBM and solder, the solder bumps were examined at specified period of current stressing using SEM (Scanning Electron microscope), EDX (Energy Dispersive X-ray Spectroscopy) and WDS (Wave Dispersive X-ray Spectroscopy). There exists a thermal gradient between cathode and anode. The synergism effect electromigration and thermornigration accelerated the growth and propagation of voids at the cathode. Voids formed on the Al trace/solder interface regardless of the direction electron flow. Voids also formed at the interface even though the current flowed along the Al trace. Thermomigration overwhelms electromigration and results in mass diffusion when counter flow of electron and thermal gradient exists. The evidence of mass transfer was further confirmed by the mass analysis throughout the bump and the hillock appeared at the lower portion of the bump. The formation of intermetallic compound at the substrate side (metallized with Cu/Ni-P/Au) was suppressed when the electron flow and thermal gradient were in the opposite direction. The solder mass was forced to migrate to the substrate when the current flowed toward the substrate or along the Al trace. In order to illustrate the importance of heat dissipation, a set of joints were stressed with current at an environmental temperature of -5 degrees C. The comparison between the as produced bump and current stressed bump indicated that no visible defect exists either at the cathode or at the anode even after 600 hours. These observations further emphasized the significance of heat dissipation in reducing the migration defect.
引用
下载
收藏
页码:667 / +
页数:3
相关论文
共 50 条
  • [41] DYNAMIC RECRYSTALLIZATION of Sn3.0Ag0.5Cu Pb-FREE SOLDER ALLOY
    Holdermann, Ken
    Cuddalorepatta, Gayatri
    Dasgupta, Abhijit
    IMECE2008: PROCEEDINGS OF THE INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION - 2008, VOL 6, 2009, : 163 - 169
  • [42] Manufacturing of Cu/electroless nickel/Sn-Pb flip chip solder bumps
    Lin, KL
    Liu, YC
    IEEE TRANSACTIONS ON ADVANCED PACKAGING, 1999, 22 (04): : 575 - 579
  • [43] Electromigration of Composite Sn-Ag-Cu Solder Bumps
    Sharma, Ashutosh
    Xu, Di Erick
    Chow, Jasper
    Mayer, Michael
    Sohn, Heung-Rak
    Jung, Jae Pil
    ELECTRONIC MATERIALS LETTERS, 2015, 11 (06) : 1072 - 1077
  • [44] Electromigration failure mechanism of Sn96.5Ag3.5 flip-chip solder bumps
    Shao, TL
    Chen, IH
    Chen, C
    54TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE, VOLS 1 AND 2, PROCEEDINGS, 2004, : 979 - 982
  • [45] Role of diffusion anisotropy in β-Sn in microstructural evolution of Sn-3.0Ag-0.5Cu flip chip bumps undergoing electromigration
    Huang, M. L.
    Zhao, J. F.
    Zhang, Z. J.
    Zhao, N.
    ACTA MATERIALIA, 2015, 100 : 98 - 106
  • [46] EFFECT OF ELECTROMIGRATION ON INTERFACIAL REACTION IN Ni/Sn3.0Ag0.5Cu/Cu FLIP CHIP SOLDER JOINTS
    Huang Mingliang
    Chen Leida
    Zhou Shaoming
    ACTA METALLURGICA SINICA, 2012, 48 (03) : 321 - 328
  • [47] Electromigration behavior of lead-free solder flip chip bumps on NiP/Cu metallization
    Jang, J. W.
    Ramanathan, L. N.
    Frear, D. R.
    JOURNAL OF APPLIED PHYSICS, 2008, 103 (12)
  • [48] Pb-free solder alloys for flip chip applications
    Kang, SK
    Horkans, J
    Andricacos, PC
    Carruthers, RA
    Cotte, J
    Datta, M
    Gruber, P
    Harper, JME
    Kwietniak, K
    Sambucetti, C
    Shi, L
    Brouillette, G
    Danovitch, D
    49TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE - 1999 PROCEEDINGS, 1999, : 283 - 288
  • [49] Influences of intermetallic compounds morphologies on fracture behaviors of Sn-3Ag-0.5Cu/Cu solder joint
    Yang, L. M.
    Zhang, Z. F.
    2013 14TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY (ICEPT), 2013, : 247 - 249
  • [50] Pb-free solder alloys for flip chip applications
    Kang, S.K.
    Horkans, J.
    Andricacos, P.C.
    Carruthers, R.A.
    Cotte, J.
    Datta, M.
    Gruber, P.
    Harper, J.M.E.
    Kwietniak, K.
    Sambucetti, C.
    Shi, L.
    Brouillette, G.
    Danovitch, D.
    Proceedings - Electronic Components and Technology Conference, 1999, : 283 - 288