Microstructure, wetting property of Sn-Ag-Cu-Bi-xCe solder and IMC growth at solder/Cu interface during thermal cycling

被引:21
|
作者
Wang, Yuan [1 ]
Zhao, Xiu-Chen [1 ]
Liu, Ying [1 ]
Wang, Yong [1 ,2 ]
Li, Dong-Mei [2 ]
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, Beijing 100081, Peoples R China
[2] Beijing Microelect Technol Inst, Ctr Packaging & Testing, Beijing 100076, Peoples R China
关键词
Lead-free solder; Rare earth element; Microstructure; Wettability; Intermetallic compound; Thermal cycling;
D O I
10.1007/s12598-015-0526-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of adding small amounts of cerium (Ce) to Sn-3.3Ag-0.2Cu-4.7Bi solder on microstructure, wettability characteristic, interfacial morphology and the growth of interfacial intermetallic compound (IMC) during thermal cycling were investigated by optical microscopy (OM), scanning electron microscopy (SEM) and solderability tester. It is found that the beta-Sn phase, Ag3Sn phase and Cu6Sn5 phase in the solder are refined and the wetting force increases. Ce is an active element; it more easily accumulates at the solder/flux interface in the molten state, which decreases the interfacial surface energy and reduces the driving force for IMC formation on Cu substrate; therefore, the thickness of IMC at the solder/Cu interface decreases when appropriate Ce was added into the solder. Moreover, the Ce-containing solders have lower growth rate of interfacial IMC than solders without Ce during the thermal cycling between -55 and 125 degrees C. When the Ce content is 0.03 wt% in the Sn-3.3Ag-0.2Cu-4.7Bi solder, the solder has the best wettability and the minimum growth rate of interfacial IMC layer.
引用
收藏
页码:714 / 719
页数:6
相关论文
共 50 条
  • [21] Microstructure and strength of interface between Sn-Ag eutectic solder and Cu
    Suganuma, Katsuaki
    Nakamura, Yoshikazu
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 1995, 59 (12): : 1299 - 1305
  • [22] Effect of bi on the microstructure evolution of Sn-3Ag-0.5Cu/Cu solder joint
    Lin, Q
    Jie, Z
    Lai, W
    Shuangqi, H
    FIFTH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY, PROCEEDINGS, 2003, : 265 - 269
  • [23] Wetting and reaction of Sn-2.8Ag-0.5Cu-1.0Bi solder with Cu and Ni substrates
    Rizvi, MJ
    Chan, YC
    Bailey, C
    Lu, H
    Islam, MN
    Wu, BY
    JOURNAL OF ELECTRONIC MATERIALS, 2005, 34 (08) : 1115 - 1122
  • [24] Wetting and reaction of Sn-2.8Ag-0.5Cu-1.0Bi solder with Cu and Ni substrates
    M. J. Rizvi
    Y. C. Chan
    C. Bailey
    H. Lu
    M. N. Islam
    B. Y. Wu
    Journal of Electronic Materials, 2005, 34 : 1115 - 1122
  • [25] Intermetallic growth study at Sn-3.0Ag-0.5Cu/Cu solder joint interface during different thermal conditions
    Li, Shuai
    Yan, Yan-fu
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2015, 26 (12) : 9470 - 9477
  • [26] Microstructural evolutions of Sn-3.0Ag-0.5Cu solder joints during thermal cycling
    Libot, J. B.
    Alexis, J.
    Dalverny, O.
    Arnaud, L.
    Milesi, P.
    Dulondel, F.
    MICROELECTRONICS RELIABILITY, 2018, 83 : 64 - 76
  • [27] IMC Growth and Mechanical Properties of Cu/In-48Sn/Cu Solder Joints
    Zheng Liu
    Li Yang
    Kai Jian Lu
    Yao Cheng Zhang
    Yu Hang Xu
    Feng Xu
    Hui Ming Gao
    Journal of Electronic Materials, 2021, 50 : 3326 - 3333
  • [28] Effect of Thermal Cycling on Interface and Properties of Sn58Bi (nano Ti)/Cu Solder Joints
    Jiang Nan
    Zhang Liang
    Sun Lei
    Wang Fengjiang
    Long Weimin
    Zhong Sujuan
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (01) : 327 - 332
  • [29] Effect of Thermal Cycling on Interface and Properties of Sn58Bi (nano Ti)/Cu Solder Joints
    Jiang, Nan
    Zhang, Liang
    Sun, Lei
    Wang, Fengjiang
    Long, Weimin
    Zhong, Sujuan
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (01): : 327 - 332
  • [30] IMC Growth and Mechanical Properties of Cu/In-48Sn/Cu Solder Joints
    Liu, Zheng
    Yang, Li
    Lu, Kai Jian
    Zhang, Yao Cheng
    Xu, Yu Hang
    Xu, Feng
    Gao, Hui Ming
    JOURNAL OF ELECTRONIC MATERIALS, 2021, 50 (06) : 3326 - 3333