Microstructure, wetting property of Sn-Ag-Cu-Bi-xCe solder and IMC growth at solder/Cu interface during thermal cycling

被引:21
|
作者
Wang, Yuan [1 ]
Zhao, Xiu-Chen [1 ]
Liu, Ying [1 ]
Wang, Yong [1 ,2 ]
Li, Dong-Mei [2 ]
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, Beijing 100081, Peoples R China
[2] Beijing Microelect Technol Inst, Ctr Packaging & Testing, Beijing 100076, Peoples R China
关键词
Lead-free solder; Rare earth element; Microstructure; Wettability; Intermetallic compound; Thermal cycling;
D O I
10.1007/s12598-015-0526-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of adding small amounts of cerium (Ce) to Sn-3.3Ag-0.2Cu-4.7Bi solder on microstructure, wettability characteristic, interfacial morphology and the growth of interfacial intermetallic compound (IMC) during thermal cycling were investigated by optical microscopy (OM), scanning electron microscopy (SEM) and solderability tester. It is found that the beta-Sn phase, Ag3Sn phase and Cu6Sn5 phase in the solder are refined and the wetting force increases. Ce is an active element; it more easily accumulates at the solder/flux interface in the molten state, which decreases the interfacial surface energy and reduces the driving force for IMC formation on Cu substrate; therefore, the thickness of IMC at the solder/Cu interface decreases when appropriate Ce was added into the solder. Moreover, the Ce-containing solders have lower growth rate of interfacial IMC than solders without Ce during the thermal cycling between -55 and 125 degrees C. When the Ce content is 0.03 wt% in the Sn-3.3Ag-0.2Cu-4.7Bi solder, the solder has the best wettability and the minimum growth rate of interfacial IMC layer.
引用
收藏
页码:714 / 719
页数:6
相关论文
共 50 条
  • [1] Microstructure,wetting property of Sn-Ag-Cu-Bi-xCe solder and IMC growth at solder/Cu interface during thermal cycling
    Yuan Wang
    Xiu-Chen Zhao
    Ying Liu
    Yong Wang
    Dong-Mei Li
    Rare Metals, 2021, 40 (03) : 714 - 719
  • [2] Microstructure, wetting property of Sn–Ag–Cu–Bi–xCe solder and IMC growth at solder/Cu interface during thermal cycling
    Yuan Wang
    Xiu-Chen Zhao
    Ying Liu
    Yong Wang
    Dong-Mei Li
    Rare Metals, 2021, 40 : 714 - 719
  • [3] Thermal cycling aging effects on Sn-Ag-Cu solder joint microstructure, IMC and strength
    Pang, JHL
    Low, TH
    Xiong, BS
    Xu, LH
    Neo, CC
    THIN SOLID FILMS, 2004, 462 : 370 - 375
  • [4] The effect of Bi on the IMC growth in Sn-3Ag-0.5Cu solder interface during aging process
    Qi, L
    Zhao, J
    Wang, XM
    Wang, L
    2004 INTERNATIONAL CONFERENCE ON THE BUSINESS OF ELECTRONIC PRODUCT RELIABILITY AND LIABILITY, PROCEEDINGS, 2004, : 42 - 46
  • [5] Microstructure and mechanical property of Sn–Ag–Cu solder material
    Yi-Gang Kong
    Zhi-Gang Kong
    Feng-Min Shi
    Rare Metals, 2017, 36 : 193 - 197
  • [6] Microstructure and mechanical property of Sn–Ag–Cu solder material
    Yi-Gang Kong
    Zhi-Gang Kong
    Feng-Min Shi
    RareMetals, 2017, 36 (03) : 193 - 197
  • [7] The growth of intermetallic compounds at Sn-Ag-Cu solder/Cu and Sn-Ag-Cu solder/Ni interfaces and the associated evolution of the solder microstructure
    A. Zribi
    A. Clark
    L. Zavalij
    P. Borgesen
    E. J. Cotts
    Journal of Electronic Materials, 2001, 30 : 1157 - 1164
  • [8] The growth of intermetallic compounds at Sn-Ag-Cu solder/Cu and Sn-Ag-Cu solder/Ni interfaces and the associated evolution of the solder microstructure
    Zribi, A
    Clark, A
    Zavalij, L
    Borgesen, P
    Cotts, EJ
    JOURNAL OF ELECTRONIC MATERIALS, 2001, 30 (09) : 1157 - 1164
  • [9] Microstructure and Property Changes in Cu/Sn-58Bi/Cu Solder Joints during Thermomigration
    Shen, Yu-An
    Zhou, Shiqi
    Li, Jiahui
    Tu, K. N.
    Nishikawa, Hiroshi
    2019 IEEE 69TH ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE (ECTC), 2019, : 2003 - 2008
  • [10] Microstructure and mechanical property of Sn-Ag-Cu solder material
    Kong, Yi-Gang
    Kong, Zhi-Gang
    Shi, Feng-Min
    RARE METALS, 2017, 36 (03) : 193 - 197