Corrosion of SiC/SiC composite in Na2SO4 vapor environments from 1000 to 1500 °C

被引:23
|
作者
Wu, Shoujun [1 ]
Cheng, Laifei [1 ]
Zhang, Litong [1 ]
Xu, Yongdong [1 ]
Luan, Xingang [1 ]
Mei, Hui [1 ]
机构
[1] Northwestern Polytech Univ, Natl Key Lab Thermostruct Composite Mat, Xian 710072, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
3D SiC/SiC composite; corrosion; Na2SO4;
D O I
10.1016/j.compositesa.2005.07.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Corrosion of a three-dimensional SiC/SiC composite with a CVD Sic coating was investigated in environments containing Na2SO4 vapor, oxygen and water vapor at temperatures from 1000 to 1500 degrees C. The corrosion behavior was greatly related to temperature. Below 1200 degrees C, the composite exhibited excellent resistance to corrosion, and then the residual flexural strength nearly kept the same value as the as-received strength. From 1200 to 1300 degrees C, the interaction of oxidation and corrosion led to a rapid weight gain. Above 1300 degrees C, weight loss due to volatilization and sublimation of Si(OH)(4) and Na2O center dot xSiO(2) on the surface increased continuously. At the same time, the gas release resulted in the formation of bubbles/corrosion pits and the maximum diameters of them increased with an increasing temperature. Additionally, above 1200 degrees C, with an increasing temperature, the residual flexural strength of the composite decreased greatly. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1396 / 1401
页数:6
相关论文
共 50 条
  • [21] Stressed oxidation behaviour of 3D C/SiC in water/oxygen/Na2SO4 coupled environment
    Luan, Xingang
    Yi, Runlin
    Zhang, Mingshuo
    Cheng, Laifei
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (13) : 7531 - 7539
  • [22] The conversion from Na2SO4
    Janecke, E
    ZEITSCHRIFT FUR PHYSIKALISCHE CHEMIE--STOCHIOMETRIE UND VERWANDTSCHAFTSLEHRE, 1916, 91 (05): : 548 - 570
  • [23] Hot corrosion behavior of CM 247 LC alloy in Na2SO4 and NaCl environments
    Gurrappa, I
    OXIDATION OF METALS, 1999, 51 (5-6): : 353 - 382
  • [24] Hot Corrosion Behavior of CM 247 LC Alloy in Na2SO4 and NaCl Environments
    I. Gurrappa
    Oxidation of Metals, 1999, 51 : 353 - 382
  • [25] A method for investigation of hot corrosion by gaseous Na2SO4
    Knutsson, Pavleta
    Lai, Haiping
    Stiller, Krystyna
    CORROSION SCIENCE, 2013, 73 : 230 - 236
  • [26] Interaction of low-expansion NZP ceramics with Na2SO4 at 1000 degrees C
    Lee, WY
    Stinton, DP
    Joslin, DL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (02) : 484 - 486
  • [27] Gaseous corrosion mechanisms of silicon carbides in Na2SO4 and V2O5 environments
    Say, WC
    Liu, SC
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (11) : 3003 - 3008
  • [28] MECHANISM OF NA2SO4 INDUCED CORROSION AT 600-DEGREES-C-900-DEGREES-C
    LUTHRA, KL
    SHORES, DA
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (10) : 2202 - 2210
  • [29] Packing and properties of composite phase change energy storage materials based on SiC nanowires and Na2SO4·10H2O
    Jian Tie
    Xin Liu
    Shengnian Tie
    Jiqing Zhang
    Siyuan Jiang
    Ruixin Tao
    Xiaobin Huang
    Journal of Thermal Analysis and Calorimetry, 2020, 139 : 855 - 862
  • [30] Packing and properties of composite phase change energy storage materials based on SiC nanowires and Na2SO4•10H2O
    Tie, Jian
    Liu, Xin
    Tie, Shengnian
    Zhang, Jiqing
    Jiang, Siyuan
    Tao, Ruixin
    Huang, Xiaobin
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2020, 139 (02) : 855 - 862