Oxidation protection of carbon/carbon composites with SiC/indialite coating for intermediate temperatures

被引:18
|
作者
Li Ke-Zhi [1 ]
Lan Feng-Tao [1 ]
Li He-Jun [1 ]
Shen Xue-Tao [1 ]
He Yong-Gang [1 ]
机构
[1] Northwestern Polytech Univ, CC Composites Technol Res Ctr, Natl Key Lab Thermostruct Composite Mat, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Sintering; Interfaces; Corrosion; Glass ceramics; Engine components; CARBON-CARBON COMPOSITES;
D O I
10.1016/j.jeurceramsoc.2008.11.003
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to improve the oxidation resistance of carbon/carbon composites at intermediate temperatures, a novel double-layer SiC/indialite coating was prepared by a simple and low-cost method. The internal SiC transition layer was prepared by pack cementation and the external indialite glass-ceramic coating was produced by in situ crystallization of ternary MgO-Al2O3-SiO2 glass. The microstructures and morphologies of coating were determined by scanning electron microscopy (SEM), X-ray diffraction (XRD) and energy dispersive spectroscopy (EDS). Oxidation resistance of the as-coated C/C composites was evaluated in ambient air at temperature from 800 degrees C to 1200 degrees C. Nearly neglectable mass loss was measured after 100 h isothermal oxidation test, indicating that SiC/indialite coating possesses excellent oxidation protection ability. The as-coated samples have a good thermal shock resistance and no obvious damage was found in the coating even after suffered more than 11 thermal cycles between test temperature and room temperature. The oxidation protection mechanism of this coating was also discussed. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1803 / 1807
页数:5
相关论文
共 50 条
  • [11] A C/SiC gradient oxidation protective coating for carbon/carbon composites
    Zhang, Yu-Lei
    Li, He-Jun
    Fu, Qian-Gang
    Li, Ke-Zhi
    Wei, Jian
    Wang, Peng-Yun
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (06): : 3491 - 3495
  • [12] SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites
    Li, HJ
    Fu, QG
    Shi, XH
    Li, KZ
    Hu, ZB
    CARBON, 2006, 44 (03) : 602 - 605
  • [13] Oxidation protection of C/SiC coated carbon/carbon composites with Si-Mo coating at high temperature
    Zhang, Yu-Lei
    Li, He-Jun
    Yao, Xi-Yuan
    Li, Ke-Zhi
    Qiang, Xin-Fa
    CORROSION SCIENCE, 2011, 53 (06) : 2075 - 2079
  • [14] A SiC/ZrB2-SiC/SiC oxidation resistance multilayer coating for carbon/carbon composites
    Yao, Xi-Yuan
    Li, He-Jun
    Zhang, Yu-Lei
    Ren, Jun-Jie
    Yao, Dong-Jia
    Tao, Jun
    CORROSION SCIENCE, 2012, 57 : 148 - 153
  • [15] Simple method of SiC coating on carbon/carbon composites and evaluations of oxidation resistance
    Kogo, Yasuo
    Hatta, Hiroshi
    Okura, Akimitsu
    Goto, Yasuhiro
    Sawada, Yutaka
    Oya-Seimiya, Yoshihiro
    Yarii, Toshio
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 1998, 62 (02): : 197 - 206
  • [16] A MoSi2/SiC oxidation protective coating for carbon/carbon composites
    Huang, Jian-Feng
    Wang, Bo
    Li, He-Jun
    Liu, Miao
    Cao, Li-Yun
    Yao, Chun-Yan
    CORROSION SCIENCE, 2011, 53 (02) : 834 - 839
  • [17] A ZrSiO4/SiC oxidation protective coating for carbon/carbon composites
    Liu, Jia
    Cao, Li-Yun
    Huang, Jian-Feng
    Xin, Yu
    Yang, Wen-Dong
    Fei, Jie
    Yao, Chun-Yan
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (14): : 3270 - 3274
  • [18] Simple method of SiC coating on carbon/carbon composites and evaluations of oxidation resistance
    Kogo, Y
    Hatta, H
    Okura, A
    Goto, Y
    Sawada, Y
    Oya-Seimiya, Y
    Yarii, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1998, 62 (02) : 197 - 206
  • [19] Yttrium silicate oxidation protective coating for SiC coated carbon/carbon composites
    Huang, JF
    Li, HJ
    Zeng, XR
    Li, KZ
    CERAMICS INTERNATIONAL, 2006, 32 (04) : 417 - 421
  • [20] Oxidation behavior of SiC/glaze-precursor coating on carbon/carbon composites
    Jiao, Xingjian
    Li, Tongqi
    Li, Yumei
    Zhang, Zhongwei
    Dai, Fuzhi
    Feng, Zhihai
    CERAMICS INTERNATIONAL, 2017, 43 (11) : 8208 - 8213