Effect of prolonged application of single-step self-etching primer and hydrofluoric acid on the surface roughness and shear bond strength of CAD/CAM materials

被引:16
|
作者
Donmez, Mustafa B. [1 ]
Okutan, Yener [2 ]
Yucel, Munir T. [3 ]
机构
[1] Biruni Univ, Fac Dent, Dept Prosthodont, 10 Yil St 45, Istanbul, Turkey
[2] Adnan Menderes Univ, Fac Dent, Dept Prosthodont, Aydin, Turkey
[3] Selcuk Univ, Fac Dent, Dept Prosthodont, Konya, Turkey
关键词
CAD; CAM ceramic; ceramic primer; hydrofluoric acid; shear bond strength; surface roughness; MECHANICAL-PROPERTIES; LITHIUM DISILICATE; RESIN COMPOSITE; CERAMIC PRIMER; CEMENTS; ADHESION; TIME;
D O I
10.1111/eos.12747
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
This in vitro study aimed to assess the influence of different concentrations and durations of hydrofluoric acid (HF) and Monobond Etch & Prime (MEP) etching on the surface roughness (R-a) of different CAD/CAM materials and on the shear bond strength (SBS) of a self-adhesive resin bonded to the materials. Seventy specimens of hybrid ceramic, leucite-based glass-ceramic, lithium disilicate glass-ceramic, and zirconia-reinforced lithium silicate glass-ceramic were prepared and divided into seven groups according to the surface treatments: Control (C); MEP etching for 60 (MEP60) and 120 (MEP120) s; 5% HF etching for 60 (HF-5%(60)) and 120 (HF-5%(120)) s; 9.5% HF etching for 60 (HF-9.5%(60)) and 120 (HF-9.5%(120)) s. The R-a was measured using a 3D profilometer. All groups were treated with a universal primer except for the C, MEP60, and MEP120 groups. A self-adhesive resin cement was bonded to all specimens, and the bond strengths were measured using a universal testing machine. All surface treatments increased both R-a and SBS values compared to the control in each material. Neither the duration of surface treatments nor the HF acid concentrations had a statistically significant effect on SBS. Within the limitations of this experimental study, it can be concluded that Monobond Etch & Prime may be a preferable method to achieve high bond strength values.
引用
下载
收藏
页码:542 / 549
页数:8
相关论文
共 50 条
  • [31] Effect of a single-component ceramic conditioner on shear bond strength of precoated brackets to different CAD/CAM materials
    Gonzalez-Serrano, Carlos
    Phark, Jin-Ho
    Fuentes, Maria Victoria
    Albaladejo, Alberto
    Sanchez-Monescillo, Andres
    Duarte, Sillas, Jr.
    Ceballos, Laura
    CLINICAL ORAL INVESTIGATIONS, 2021, 25 (04) : 1953 - 1965
  • [32] The effect of different parameters on the wear, surface properties, and shear bond strength of monolithic zirconia CAD/CAM restorative materials
    Alper, Seval Baspinar
    Tekce, Neslihan
    Yildirim, Elif Sevilay
    Sancak, Elif Ilgi
    Fidan, Sinan
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2023, 37 (23) : 3379 - 3392
  • [33] Effect of a single-component ceramic conditioner on shear bond strength of precoated brackets to different CAD/CAM materials
    Carlos González-Serrano
    Jin-Ho Phark
    María Victoria Fuentes
    Alberto Albaladejo
    Andrés Sánchez-Monescillo
    Sillas Duarte
    Laura Ceballos
    Clinical Oral Investigations, 2021, 25 : 1953 - 1965
  • [34] Shear Bond Strength of Self-etching Adhesives to Cavities Prepared by Diamond Bur or Er, Cr:YSGG Laser and Effect of Prior Acid Etching
    Jhingan, Pulkit
    Sachdev, Vinod
    Sandhu, Meera
    Sharma, Karan
    JOURNAL OF ADHESIVE DENTISTRY, 2015, 17 (06): : 505 - 512
  • [35] Effect of surface treatment of CAD/CAM resin composites on the shear bond strength of self-adhesive resin cement
    Nagasawa, Yuko
    Hibino, Yasushi
    Eda, Yoshikazu
    Nakajima, Hiroshi
    DENTAL MATERIALS JOURNAL, 2021, 40 (02) : 364 - 378
  • [36] Effect of milling, fitting adjustments, and hydrofluoric acid etching on the strength and roughness of CAD-CAM glass-ceramics: A systematic review and meta-analysis
    May, Michele Mirian
    Fraga, Sara
    May, Liliana Gressler
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 128 (06): : 1190 - 1200
  • [37] Surface pH and bond strength of a self-etching primer/adhesive system to intracoronal dentin after application of hydrogen peroxide bleach with sodium perborate
    Elkhatib, H
    Nakajima, M
    Hiraishi, N
    Kitasako, Y
    Tagami, J
    Nomura, S
    OPERATIVE DENTISTRY, 2003, 28 (05) : 591 - 597
  • [38] Effect of 9% Hydrofluoric Acid Gel Hot-Etching Surface Treatment on Shear Bond Strength of Resin Cements to Zirconia Ceramics
    Kim, So-Hyun
    Cho, Sung-Chan
    Lee, Myung-Hyun
    Kim, Hyo-Jung
    Oh, Nam-Sik
    MEDICINA-LITHUANIA, 2022, 58 (10):
  • [39] Effect of thermal cycling on shear bond strength with different types of self-etching primer for bonding orthodontic brackets using a MMA-based resin
    Meguro, D
    Hayakawa, T
    Saito, K
    Kawasaki, M
    Kasai, K
    DENTAL MATERIALS JOURNAL, 2005, 24 (01) : 30 - 35
  • [40] Effect of surface treatments on shear bond strength of resin composite bonded to CAD/CAM resin-ceramic hybrid materials
    Gungor, Merve Bankoglu
    Nemli, Secil Karakoca
    Bal, Bilge Turhan
    Unver, Senem
    Dogan, Aylin
    JOURNAL OF ADVANCED PROSTHODONTICS, 2016, 8 (04): : 259 - 266