Improving the plasticity of bulk metallic glasses via pre-compression below the yield stress

被引:32
|
作者
Gu, Ji [1 ]
Song, Min [1 ]
Ni, Song [1 ]
Liao, Xiaozhou [2 ]
Guo, Shengfeng [3 ]
机构
[1] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[2] Univ Sydney, Sch Aerosp Mech & Mech Engn, Sydney, NSW 2006, Australia
[3] Southwest Univ, Fac Mat & Energy, Chongqing 400715, Peoples R China
基金
澳大利亚研究理事会; 中国国家自然科学基金;
关键词
Bulk metallic glasses; Pre-compression; Plasticity; Free volume; Nanocrystallite; AMORPHOUS-ALLOYS; MECHANICAL-BEHAVIOR; SHEAR-BAND; ENHANCED PLASTICITY; ROOM-TEMPERATURE; ZRC PARTICLES; FREE-VOLUME; DEFORMATION; DUCTILITY; COMPOSITES;
D O I
10.1016/j.msea.2014.02.065
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The poor plasticity of bulk metallic glasses (BMGs) has severely limited their potential structural applications. In this paper, we reported that uniaxial pre-compression below the yield stress can be used to significantly improve the plasticity of BMGs. An as-cast Cu36Zr48Al8Ag8 BMG was pre-compressed under various pressures (400, 800 and 1600 MPa) and durations (30, 60 and 120 mm). The pre-compression processes led to structural change that increases the free volume and produces nanocrystals in the BMG matrix, which subsequently improved the plasticity of the BMG. Detailed data analysis showed that increasing the applied pressure speeds up the structural relaxation process and nanocrystallization occurs only at high enough pressure. This investigation indicated that appropriate selection of the pressure and duration of a pre-compression process is critical for the improved plasticity of BMGs. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:68 / 76
页数:9
相关论文
共 50 条
  • [21] Effects of Pre-compression on the Microstructure and Corrosion Resistance of Cu50Zr50 Bulk Metallic Glass Matrix Composites
    Zhai, Sicheng
    Wang, Wen
    Wang, Yan
    ADVANCED FUNCTIONAL MATERIALS (CMC 2017), 2018, : 275 - 283
  • [22] Applicability of Pre-Plastic Deformation Method for Improving Mechanical Properties of Bulk Metallic Glasses
    Zhou, Changshan
    Zhang, Hezhi
    Yuan, Xudong
    Song, Kaikai
    Liu, Dan
    MATERIALS, 2022, 15 (21)
  • [23] Enhancement of plasticity in Zr-based bulk metallic glasses
    Wang X.D.
    Yang L.
    Jiang J.Z.
    Saksl K.
    Franz H.
    Fecht H.-J.
    Liu Y.G.
    Xian H.S.
    Journal of Materials Research, 2007, 22 (09) : 2454 - 2459
  • [24] Poisson's ratio and plasticity in CuZrAl bulk metallic glasses
    Yu, Peng
    Bai, H. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 485 (1-2): : 1 - 4
  • [25] Extended plasticity in the supercooled liquid region of bulk metallic glasses
    Nieh, TG
    Wadsworth, J
    Liu, CT
    Ice, GE
    Chung, KS
    MATERIALS TRANSACTIONS, 2001, 42 (04) : 613 - 618
  • [26] Plasticity of bulk metallic glasses improved by controlling the solidification condition
    Zhu Z.W.
    Zheng S.J.
    Zhang H.F.
    Ding B.Z.
    Hu Z.Q.
    Liaw P.K.
    Wang Y.D.
    Ren Y.
    J Mater Res, 2008, 4 (941-948): : 941 - 948
  • [27] Effect of testing conditions on the compressive plasticity of bulk metallic glasses
    Yunpeng Jiang
    Journal of Materials Research, 2016, 31 : 2686 - 2694
  • [28] Plasticity of bulk metallic glasses improved by controlling the solidification condition
    Zhu, Z. W.
    Zheng, S. J.
    Zhang, H. F.
    Ding, B. Z.
    Hu, Z. Q.
    Liaw, P. K.
    Wang, Y. D.
    Ren, Y.
    JOURNAL OF MATERIALS RESEARCH, 2008, 23 (04) : 941 - 948
  • [29] Quaternary magnetic FeNiPC bulk metallic glasses with large plasticity
    Ma, Xiuhua
    Yang, Xiaohui
    Li, Qiang
    Guo, Shengfeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 577 : 345 - 350
  • [30] Effect of testing conditions on the compressive plasticity of bulk metallic glasses
    Jiang, Yunpeng
    JOURNAL OF MATERIALS RESEARCH, 2016, 31 (17) : 2686 - 2694