Production of hydrogen by methane catalytic decomposition over Ni-Cu-Fe/Al2O3 catalyst

被引:92
|
作者
Chesnokov, Vladimir V. [1 ]
Chichkan, Alexandra S. [1 ]
机构
[1] RAS, Boreskov Inst Catalysis SB, Novosibirsk, Russia
关键词
Hydrogen production; Methane decomposition; Natural gas; Ni-Cu-Fe/Al2O3; catalyst; FILAMENTOUS CARBON; ACTIVATED CARBONS; NANOFIBERS; CRACKING; NI/SIO2;
D O I
10.1016/j.ijhydene.2009.01.074
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Catalysts with high nickel concentrations 75%Ni-12%Cu/Al2O3, 70%Ni-10%Cu-10%Fe/Al2O3 were prepared by mechanochemical activation and their catalytic properties were studied in methane decomposition. It was shown that modification of the 75%Ni-12%Cu/Al2O3 catalyst with iron made it possible to increase optimal operating temperatures to 700-750 degrees C while maintaining excellent catalyst stability. The formation of finely dispersed Ni-Cu-Fe alloy particles makes the catalysts stable and capable of operating at 700-750 degrees C in methane decomposition to hydrogen and carbon nanofibers. The yield of carbon nanofibers on the modified 70%Ni-10%Cu-10%Fe/Al2O3 catalyst at 700-750 degrees C was 150-160 g/g. The developed hydrogen production method is also efficient when natural gas is used as the feedstock. An installation with a rotating reactor was developed for production of hydrogen and carbon nanofibers from natural gas. It was shown that the 70%Ni-10%Cu-10%Fe/Al2O3 catalyst could operate in this installation for a prolonged period of time. The hydrogen concentration at the reactor outlet exceeded 70 mol%. (C) 2009 International Association for Hydrogen Energy. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:2979 / 2985
页数:7
相关论文
共 50 条
  • [41] Growth of carbon nanotubes by the catalytic decomposition of methane over Fe-Mo/Al2O3 catalyst: effect of temperature on tube structure
    Song Jin-ling
    Wang Li
    Feng Shou-ai
    Zhao Jiang-hong
    Zhu Zhen-ping
    [J]. NEW CARBON MATERIALS, 2009, 24 (04) : 307 - 313
  • [42] The effect of hydrogen on thiophene catalytic removal over Ni/Al2O3
    Zhao, Jinchong
    Chai, Yongming
    Liu, Bin
    Liu, Yaqing
    Liu, Yunqi
    Liu, Chenguang
    [J]. CATALYSIS COMMUNICATIONS, 2019, 119 : 6 - 10
  • [43] Microkinetic modelling of methane dry reforming over Ni/Al2O3 catalyst
    Dehimi, Leila
    Benguerba, Yacine
    Virginie, Mirella
    Hijazi, Houssam
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (30) : 18930 - 18940
  • [44] Pulse study on the partial oxidation of methane over Ni/θ-Al2O3 catalyst
    Liu, ZW
    Jun, KW
    Roh, HS
    Baek, SC
    Park, SE
    [J]. JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 2002, 189 (02) : 283 - 293
  • [45] Thermocatalytic decomposition of methane over mesoporous Ni/xMgO•Al2O3 nanocatalysts
    Rastegarpanah, Ali
    Rezaei, Mehran
    Meshkani, Fereshteh
    Dai, Hongxing
    Arandiyan, Hamidreza
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2018, 43 (32) : 15112 - 15123
  • [46] Hydrogen production by catalytic decomposition of methane over Ni-Cu-Co alloy particles
    Lua, Aik Chong
    Wang, Hong Yan
    [J]. APPLIED CATALYSIS B-ENVIRONMENTAL, 2014, 156 : 84 - 93
  • [47] REACTIONS OF ADSORBED HYDROGEN WITH OXYGEN ON FE/AL2O3, NI/AL2O3 AND FE-NI/AL2O3 CATALYSTS
    LESNIEWSKA, E
    RYNKOWSKI, J
    PARYJCZAK, T
    [J]. PRZEMYSL CHEMICZNY, 1995, 74 (01): : 21 - 22
  • [48] Catalytic hydrolysis of gaseous HCN over Cu-Ni/γ-Al2O3 catalyst: parameters and conditions
    Yan, Linxia
    Tian, Senlin
    Zhou, Jian
    Yuan, Xin
    [J]. FRONTIERS OF ENVIRONMENTAL SCIENCE & ENGINEERING, 2016, 10 (06)
  • [49] Catalytic combustion of methane over Ni modified Pd/Al2O3 catalysts
    Todorova, Silviya
    Naydenov, Anton
    Velinova, Ralitsa
    Kolev, Hristo
    Larin, Alexander
    Karashanova, D.
    [J]. MATERIALS TODAY-PROCEEDINGS, 2022, 61 : 1212 - 1216
  • [50] Hydrogen from wood vinegar via catalytic reforming over Ni/Ce/γ-Al2O3 catalyst
    Xu Xiwei
    Jiang Enchen
    [J]. JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2014, 107 : 1 - 8