摘要
Pyrite is an abundant mineral, and its dissolution is important in the formation of acid mine drainage and the extraction of metals. It has also been considered as a candidate material for electrochemical solar cells. We studied the anodic processes on pyrite in hydrochloric acid. The current-voltage curve at steady state has three regions. At potentials below 0.6 V, the current is low, and the Tafel slope is high; between 0.6 and 0.9 V, the current is significant, and the Tafel slope is 0.082 V/decade; at potentials above 0.9 V, the current remains high, but the Tafel slope changes to 0.430 V/decade. From careful measurements of the dissolution of pyrite by chlorine, we show that this third region is due to charge transfer and not ohmic resistance. The shape of the current-voltage curve is unaffected by the type of acid used. The effect of temperature was measured, and the activation energies for the middle and upper region are 46 and 105 kJ/mol, respectively. The steady-state current-voltage curves are not affected by the concentration of HCI, but are affected by the concentration of chloride ions, with an order of reaction of -0.1, indicating that the rate only slightly dependent on chloride ions. Pretreatment tests and XPS analysis of the surface confirm that the change in Tafel slope is not due to the formation of a surface coating or oxidation product. A comprehensive model of the anodic dissolution of pyrite that describes the current-voltage behavior of pyrite over the entire anodic region is proposed. At low potentials, the behavior of pyrite is typical of an n-type semiconductor with some dissolution. However, as the potential is increased, the Fermi level overlaps with an intrinsic surface state. The rate of dissolution of the pyrite in this region is dependent on the occupancy of the surface state. This accounts for previous reports indicating that pyrite is quasi-metallic. The rate-determining step is the transfer of charge across the space-charge layer. As the potential is increased to about 0.9 V, the surface state is unoccupied, and the rate-determining step changes to the transfer of ions across the Helmholtz layer. An expression based on this model fits the experimental data. An important feature of this model is that it also explains two contradictory features of pyrite electrochemistry. On the one hand, n-type and p-type pyrite samples may have similar kinetic parameters, which suggests that the electronic structure of pyrite makes little difference. On the other hand, illuminating the sample with light increases the rate of dissolution, which suggests that the electronic structure is important. The proposed model based on surface states explains these seemingly contradictory observations. (C) 2014 Elsevier B.V. All rights reserved.
引用
下载
收藏
页码:42 / 53
页数:12
相关论文
共 50 条
  • [21] THIN PHOTOACTIVE FES2 (PYRITE) FILMS
    CHATZITHEODOROU, G
    FIECHTER, S
    KONENKAMP, R
    KUNST, M
    JAEGERMANN, W
    TRIBUTSCH, H
    MATERIALS RESEARCH BULLETIN, 1986, 21 (12) : 1481 - 1487
  • [22] REDETERMINED CRYSTAL STRUCTURE OF FES2 (PYRITE)
    BROSTIGEN, G
    KJEKSHUS, A
    ACTA CHEMICA SCANDINAVICA, 1969, 23 (06): : 2186 - +
  • [23] Rotating ring (Pt)-disc (FeS2) electrode behavior in hydrochloric solutions
    Yin, Q
    Kelsall, GH
    Vaughan, DJ
    Welham, NJ
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1999, 210 (02) : 375 - 383
  • [24] ANODIC-DISSOLUTION OF PALLADIUM IN GLYCERINIC HYDROCHLORIC-ACID SOLUTIONS
    YUZIKIS, PA
    PROTECTION OF METALS, 1989, 25 (04): : 537 - 539
  • [25] THE AQUEOUS SURFACE-CHEMISTRY OF PYRITE (FES2) AND MACKINAWITE (FES)
    KORNICKER, WA
    MORSE, JW
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1987, 194 : 36 - ENVR
  • [26] Catalytic behavior of hexaphenyldisiloxane in the synthesis of pyrite FeS2
    Todd, Paul K.
    Martinolich, Andrew J.
    Neilson, James R.
    CHEMICAL COMMUNICATIONS, 2020, 56 (64) : 9186 - 9189
  • [27] Adsorption of organic monolayers on pyrite (FeS2)(100)
    Himmel, HJ
    Kaschke, M
    Harder, P
    Woll, C
    THIN SOLID FILMS, 1996, 284 : 275 - 280
  • [28] Nanoscale FeS2 (Pyrite) as a Sustainable Thermoelectric Material
    Uhlig, Christian
    Guenes, Ekrem
    Schulze, Anne S.
    Elm, Matthias T.
    Klar, Peter J.
    Schlecht, Sabine
    JOURNAL OF ELECTRONIC MATERIALS, 2014, 43 (06) : 2362 - 2370
  • [29] Nanoscale FeS2 (Pyrite) as a Sustainable Thermoelectric Material
    Christian Uhlig
    Ekrem Guenes
    Anne S. Schulze
    Matthias T. Elm
    Peter J. Klar
    Sabine Schlecht
    Journal of Electronic Materials, 2014, 43 : 2362 - 2370
  • [30] Photoacoustic characterization of natural mineral pyrite (FeS2)
    Nikolic, P. M.
    Lukovic, D. T.
    Nikolic, M. V.
    Djuric, S.
    Savic, S. M.
    Milovanovic, A. M.
    Dukic, S. R.
    Stamenovic, B.
    EUROPEAN PHYSICAL JOURNAL-SPECIAL TOPICS, 2008, 153 (1): : 187 - 189