Notched Tensile Strength and Fatigue Crack Growth Behavior of Ti-6Al-6V-2Sn Laser Welds

被引:15
|
作者
Tsay, Leu-Wen [1 ]
Lee, Chun-Xian [1 ]
Chen, Chun [2 ]
机构
[1] Natl Taiwan Ocean Univ, Inst Mat Engn, Chilung 202, Taiwan
[2] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 106, Taiwan
关键词
notched tensile strength; fatigue crack growth rate; Ti-6Al-6V-2Sn; laser welding; post-weld heat treatment; ALPHA+BETA TITANIUM-ALLOYS; POSTWELD HEAT-TREATMENT; FRACTURE-TOUGHNESS; MECHANICAL-PROPERTIES; TI-6AL-4V ALLOY; MICROSTRUCTURE; PROPAGATION; RESISTANCE; SHEET;
D O I
10.2320/matertrans.M2009001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Notched tensile and fatigue crack growth tests were performed on Ti-6Al-6V-2Sn laser welds which were subjected to post-weld heat treatments (PWHTs) at various temperatures. In comparison with the mill-annealed base metal (13M), Ti-6Al-6V-2Sn laser welds showed notch brittleness at different degrees. Generally, the weld metal (WM) had a lower fatigue crack growth rates (FCGRs) than the BM. Fine acicular a distributed uniformly in the beta matrix could account for the high hardness of the as-welded WM relative to the BM. With the PWHTS at higher temperatures, the coarsened microstructures of the welds reduced not only the hardness but also the sensitivity to notch brittleness. The fatigue fracture morphology of the WM was much tougher and irregular than that of the BM. A tortuous crack path in the WM as compared to the relatively straight path in the BM resulted in reduced FCGRs in the WM, particularly for the welds subjected to PWHTs at 704 degrees C or higher. [doi: 10.2320/matertrans.M2009001]
引用
收藏
页码:1785 / 1791
页数:7
相关论文
共 50 条
  • [1] The influence of aging treatments on the notched tensile strength of Ti-6Al-6V-2Sn laser welds
    Tsay, L. W.
    Lee, C. X.
    Chung, W. C.
    Chen, C.
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES, PTS 1 AND 2, 2008, 47-50 : 185 - +
  • [2] The Effect of Preheating on Notched Tensile Strength and Impact Toughness of Ti-6Al-6V-2Sn Laser Welds
    Tsay, Leu-Wen
    Jiang, Yun-Chen
    Chen, Chun
    MATERIALS TRANSACTIONS, 2011, 52 (03) : 406 - 411
  • [3] Notched Tensile Fracture of Ti-6Al-6V-2Sn Welds at Elevated Temperature
    Tsay, L. W.
    Hsu, C. L.
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES II, PTS 1 AND 2, 2009, 79-82 : 1137 - 1140
  • [4] The Influence of Microstructures on the Notched Tensile Fracture of Ti-6Al-6V-2Sn Welds at Elevated Temperatures
    Tsay, Leu-Wen
    Hsu, Chung-Liang
    Chen, Chun
    ISIJ INTERNATIONAL, 2010, 50 (01) : 128 - 132
  • [5] FATIGUE AND CRACK-PROPAGATION BEHAVIOR IN TI-6AL-6V-2SN
    AMATEAU, MF
    KENDALL, EG
    METALS ENGINEERING QUARTERLY, 1974, 14 (03): : 59 - 61
  • [6] The effect of post-weld heat treatment on the notched tensile fracture of Ti-6Al-4V to Ti-6Al-6V-2Sn dissimilar laser welds
    Hsieh, C. T.
    Chu, C. Y.
    Shiue, R. K.
    Tsay, L. W.
    MATERIALS & DESIGN, 2014, 59 : 227 - 232
  • [7] ENHANCEMENT OF FATIGUE-CRACK GROWTH AND FRACTURE RESISTANCE IN TI-6AL-4V AND TI-6AL-6V-2SN
    YODER, GR
    COOLEY, LA
    CROOKER, TW
    ASTRONAUTICS & AERONAUTICS, 1977, 15 (10): : B22 - B22
  • [8] FATIGUE CRACK GROWTH-BEHAVIOR OF TI-6AL-6V-2SN IN METHANOL AND METHANOL-WATER SOLUTIONS
    DAWSON, DB
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (05): : 791 - 800
  • [9] SUMMARY OF FATIGUE CRACK GROWTH-RATE CHARACTERISTICS OF TI-6AL-6V-2SN ALLOYS
    YODER, GR
    COOLEY, LA
    CROOKER, TW
    REPORT OF NRL PROGRESS, 1976, (SEP): : 6 - 8
  • [10] ENHANCEMENT OF FATIGUE CRACK GROWTH AND FRACTURE RESISTANCE IN TI-6AL-4V AND TI-6AL-6V-2SN THROUGH MICROSTRUCTURAL MODIFICATION
    YODER, GR
    COOLEY, LA
    CROOKER, TW
    REPORT OF NRL PROGRESS, 1976, (NOV): : 19 - 19