The Influence of Microstructures on the Notched Tensile Fracture of Ti-6Al-6V-2Sn Welds at Elevated Temperatures

被引:10
|
作者
Tsay, Leu-Wen [1 ]
Hsu, Chung-Liang [1 ]
Chen, Chun [2 ]
机构
[1] Natl Taiwan Ocean Univ, Inst Mat Engn, Chilung 202, Taiwan
[2] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 106, Taiwan
关键词
notched tensile test; Ti-6Al-6V-2Sn; post-weld heat treatment; CRACK GROWTH-BEHAVIOR; STRENGTH;
D O I
10.2355/isijinternational.50.128
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Notched tensile tests of Ti-6Al-6V-2Sn welds, which were subjected to distinct post-weld heat treatments (PWHTs), were carried out in air at 150, 300 and 450 degrees C. The results were compared with those of mill-annealed base metal (MB) specimens tested at same temperatures. The notched tensile strength (NTS) of the MB specimens decreased significantly with increasing temperature. Moreover, the welds with high hardness showed notch brittleness at room temperature but had a higher NTS than the MB specimen. The presence of grain boundary alpha layer promoted grain boundary shear, therefore, reduced its notch brittleness at room temperature for the weld with the PWHT at 704 degrees C (the W-704 specimen). A lack of deformation compatibility at the interfaces between the alpha and beta phases caused interfacial separations in the MB specimen as well as void formation in the W-704 specimen, leading to the low NTS of these specimens at elevated temperatures.
引用
收藏
页码:128 / 132
页数:5
相关论文
共 50 条
  • [1] Notched Tensile Fracture of Ti-6Al-6V-2Sn Welds at Elevated Temperature
    Tsay, L. W.
    Hsu, C. L.
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES II, PTS 1 AND 2, 2009, 79-82 : 1137 - 1140
  • [2] The influence of aging treatments on the notched tensile strength of Ti-6Al-6V-2Sn laser welds
    Tsay, L. W.
    Lee, C. X.
    Chung, W. C.
    Chen, C.
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES, PTS 1 AND 2, 2008, 47-50 : 185 - +
  • [3] Notched Tensile Fracture of Ti-6Al-4V Laser Welds at Elevated Temperatures
    Lu, M. Y.
    Tsay, L. W.
    Chen, C.
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL III, 2012, : 1860 - 1863
  • [4] Notched Tensile Fracture of Ti-6Al-4V Laser Welds at Elevated Temperatures
    Lu, M. Y.
    Tsay, L. W.
    Chen, C.
    MATERIALS TRANSACTIONS, 2012, 53 (06) : 1042 - 1047
  • [5] The Effect of Preheating on Notched Tensile Strength and Impact Toughness of Ti-6Al-6V-2Sn Laser Welds
    Tsay, Leu-Wen
    Jiang, Yun-Chen
    Chen, Chun
    MATERIALS TRANSACTIONS, 2011, 52 (03) : 406 - 411
  • [6] Notched Tensile Strength and Fatigue Crack Growth Behavior of Ti-6Al-6V-2Sn Laser Welds
    Tsay, Leu-Wen
    Lee, Chun-Xian
    Chen, Chun
    MATERIALS TRANSACTIONS, 2009, 50 (07) : 1785 - 1791
  • [7] The effect of post-weld heat treatment on the notched tensile fracture of Ti-6Al-4V to Ti-6Al-6V-2Sn dissimilar laser welds
    Hsieh, C. T.
    Chu, C. Y.
    Shiue, R. K.
    Tsay, L. W.
    MATERIALS & DESIGN, 2014, 59 : 227 - 232
  • [8] Effects of microstructures on the notch tensile fracture feature of heat-treated Ti-6Al-6V-2Sn alloy
    Huang, Rong-Tan
    Huang, Wen-Liang
    Huang, Rong-Hsin
    Tsay, Leu-Wen
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 595 : 297 - 305
  • [9] Notched tensile fracture of Ti-4.5Al-3V-2Fe-2Mo welds at elevated temperatures
    Tsay, L. W.
    Hsu, C. L.
    Chen, C.
    MATERIALS CHEMISTRY AND PHYSICS, 2010, 120 (2-3) : 715 - 721
  • [10] Diffusion bonding superplastic forming of Ti-6Al-6V-2Sn/SUS 304 stainless steel Ti-6Al-6V-2Sn
    Shyu, JS
    Chuang, TH
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1996, 5 (01) : 84 - 88