Kinetic study on the effect of adding P2O5 to the LMAS glass-ceramic

被引:6
|
作者
Ariane, Khalissa [1 ]
Tamayo, Aitana [2 ]
Chorfa, Abdellah [1 ,3 ]
Rubio, Fausto [2 ]
Rubio, Juan [2 ]
机构
[1] Ferhat Abbas Univ Setif 1, Inst Opt & Precis Mech, Setif, Algeria
[2] CSIC, Inst Ceram & Vidrio, Madrid, Spain
[3] Ferhat Abbas Univ Setif 1, Lab Appl Opt, IOMP, Setif, Algeria
关键词
LMAS glass-ceramic; Glass stability; Crystallization mechanism; A/L ratio; P2O5; effect; DIFFERENTIAL THERMAL-ANALYSIS; FORMING ABILITY; CRYSTALLIZATION KINETICS; OPTICAL-PROPERTIES; NUCLEATION; CORDIERITE; MICROSTRUCTURE; STABILITY; TEMPERATURE; RELAXATION;
D O I
10.1016/j.bsecv.2019.11.003
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Glasses in the LMAS (Li2O, MgO, Al2O3, SiO2) system containing F, CaO, ZrO2, and TiO2 were subjected to crystallization by incorporating P2O5. The glass stability, glass forming ability, and crystallization kinetics have been determined. Crystals of Lithium Aluminum Silicate (LixAlxSi1-xO2), Enstatite (MgSi2O6) and B-spodumene (LiAlSi2O6) were detected in the samples containing F, but B-spodumene was not observed in the glass-ceramic in its absence. Glasses containing F show a dependence of the activation with the addition of P2O5 with energy values ranging from 426 kJ mol(-1) to 483 kJ mol(-1), being this maximum found for P2O5 amounts up to 3 mol%. High concentrations of P2O5 and Al2O3 improve the glass stability and increase the crystallization temperature. The most common crystallization mechanism is of bulk type with a constant number of nuclei. Two- and three-dimensional growth of crystals was observed in glasses containing F but in its absence and at high Al2O3 concentration bulk crystallization with twoand one-dimensional growth is observed. (C) 2019 SECV. Published by Elsevier Espana, S.L.U.
引用
收藏
页码:239 / 250
页数:12
相关论文
共 50 条
  • [41] A SHORT STUDY ON THE EXPERIMENTAL GLASS-IONOMER CEMENT CONTAINING P2O5
    Mirghaderi, Fatemeh
    Monshi, Ahmad
    Kasiri, Masoud
    Doostmohammadi, Ali
    Khaghani, Masoomeh
    PHOSPHORUS SULFUR AND SILICON AND THE RELATED ELEMENTS, 2014, 189 (01) : 74 - 80
  • [42] ANOMALOUS SCATTERING AND EXAFS STUDY OF GEO2 - P2O5 GLASS SYSTEM
    SHIMIZUGAWA, Y
    MARUMO, F
    NUKUI, A
    OHSUMI, K
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1994, 176 (01) : 76 - 84
  • [43] Incorporation of P2O5 in a Na2O-rich aluminoborosilicate glass
    Achigar, Sophie
    Caurant, Daniel
    Regnier, Elise
    Majerus, Odile
    Charpentier, Thibault
    MATERIALS LETTERS, 2024, 377
  • [44] Effect of Al2O3 on monazite glass-ceramic wasteform
    Liao, Qi-Long
    Liao, Chun-Juan
    Xiang, Guang-Hua
    Pan, She-Qi
    Mu, Tao
    Yuanzineng Kexue Jishu/Atomic Energy Science and Technology, 2014, 48 (01): : 23 - 27
  • [45] EFFECT OF Li2O ON STRUCTURE AND PROPERTIES OF GLASS-CERAMIC BONDS
    Guo, Zichen
    He, Feng
    Li, Zuhao
    Yan, Dongyang
    Zhang, Bing
    Xie, Junlin
    CERAMICS-SILIKATY, 2021, 65 (02) : 198 - 205
  • [46] Effect of Al2O3 on Crystallization Behavior and Microstructure of Na2O-CaO-P2O5-SiO2 Glass-ceramic System
    Mirhadi, Bahman
    Mehdikhani, Behzad
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2012, 49 (02) : 146 - 150
  • [47] Gamma-irradiation effect on kinetic parameters of glass-ceramic materials
    Selçuk, AB
    Yavuz, H
    MATERIALS LETTERS, 2003, 57 (28) : 4382 - 4387
  • [48] Microwave dielectric properties of BaO–ZnO–B2O3–P2O5 glass–ceramic for LTCC application
    B. B. Lu
    J. Huang
    D. H. Jiang
    J. J. Chen
    J. Xu
    J. Xi
    G. H. Chen
    F. Shang
    J. W. Xu
    C. L. Yuan
    C. R. Zhou
    Journal of Materials Science: Materials in Electronics, 2019, 30 : 18599 - 18605
  • [49] Structural study of xK2O·(100 − x)[P2O5·CaO] glass system
    Adriana N. Regos
    R. Ciceo Lucacel
    I. Ardelean
    Journal of Materials Science, 2011, 46 : 7313 - 7318
  • [50] Electrical transport in Li2SO4-Li2O-P2O5 ionic glasses and glass-ceramic composites: A comparative study
    Rathore, Munesh
    Dalvi, Anshuman
    SOLID STATE IONICS, 2013, 239 : 50 - 55