共 26 条
- [22] DEVELOPMENT OF HIGH-STRENGTH 12CR-1MO-1W-V-NB STEEL TUBE FOR BOILER .2. MECHANICAL-PROPERTIES AND HOT CORROSION BEHAVIOR OF 12-PERCENT CR HEAT-RESISTANT STEELS FOR BOILER AFTER SERVICE EXPOSURE [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (05): : S665 - S665
- [25] Hot Corrosion Evaluation of Cr3C2/8YSZ-Based Plasma-Sprayed Coatings on SS316 in Na2SO4–V2O5 Molten Salt Environment at 700 °C [J]. Journal of Failure Analysis and Prevention, 2024, 24 : 769 - 778