Low temperature formation of SiO2 thin films by nitric acid oxidation of Si (NAOS) and application to thin film transistor (TFT)

被引:9
|
作者
Matsumoto, T. [1 ]
Asuha [1 ,3 ]
Kim, W. -B. [1 ]
Yamada, M. [1 ]
Imai, S. [2 ]
Terakawa, S. [1 ]
Kobayashi, H. [1 ]
机构
[1] Osaka Univ, Japan Sci & Technol Agcy, CREST, ISIR, Osaka 5670047, Japan
[2] Sharp Co Ltd, Display Technol Dev Grp, Nara 6328567, Japan
[3] Inner Mongolia Normal Univ, Chem & Environm Sci Coll, Zhaowudalu 010022, Hohhot, Peoples R China
关键词
MOS; Nitric acid oxidation; Silicon oxide; Thin film transistor; Low temperature oxidation; Gate oxide;
D O I
10.1016/j.mee.2009.03.080
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Nitric acid oxidation of Si (NAOS) can form 1.3-20 nm SiO2 films on Si(100) and poly-crystalline silicon (poly-Si) surfaces at low temperatures below 120 degrees C. The 1.3 nm SiO2 layer formed by immersion in 68 wt% HNO3 possesses a low leakage current density and it can be made lower by post-metallization annealing (PMA) in hydrogen than that for thermal oxide with the same thickness. A thicker SiO2 layer can be formed by immersion in 40 wt% HNO3 followed by 68 wt% HNO3, and its leakage current density becomes nearly the same after PMA as that of thermal oxide. The low leakage current density results from elimination of the interface states by hydrogen and the high atomic density of the NAOS-SiO2 layer as estimated from the vibrational frequencies of transverse and longitudinal optical phonons of the Si-O-Si asymmetric stretching mode. The thickness of the NAOS-SiO2 layer is uniform even on the rough poly-Si surfaces. The dispersion of the thickness of the NAOS-SiO2 layer is also found to be less than +/- 5% on the 32 cm x 40 cm poly-Si substrates. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:1939 / 1941
页数:3
相关论文
共 50 条
  • [1] Nitric acid oxidation of Si (NAOS) method for low temperature fabrication of SiO2/Si and SiO2/SiC structures
    Kobayashi, H.
    Imamura, K.
    Kim, W. -B.
    Im, S. -S.
    Asuha
    APPLIED SURFACE SCIENCE, 2010, 256 (19) : 5744 - 5756
  • [2] High-quality SiO2/Si interface formation and its application to fabrication of low-temperature-processed polycrystalline Si thin-film transistor
    Higashi, S
    Abe, D
    Hiroshima, Y
    Miyashita, K
    Kawamura, T
    Inoue, S
    Shimoda, T
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2002, 41 (6A): : 3646 - 3650
  • [3] High-quality SiO2/Si interface formation and its application to fabrication of low-temperature-processed polycrystalline Si thin-film transistor
    Higashi, Seiichiro
    Abe, Daisuke
    Hiroshima, Yasushi
    Miyashita, Kazuyuki
    Kawamura, Takahiro
    Inoue, Satoshi
    Shimoda, Tatsuya
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 2002, 41 (6 A): : 3646 - 3650
  • [4] Low temperature formation of SiO2/Si structure by nitric acid vapor
    Imamura, Kentarou
    Maida, Osamu
    Hattori, Kensaku
    Takahashi, Masao
    Kobayashi, Hikaru
    JOURNAL OF APPLIED PHYSICS, 2006, 100 (11)
  • [5] Low temperature fabrication of 5-10 nm SiO2/Si structure using advanced nitric acid oxidation of silicon (NAOS) method
    Fukaya, Yousuke
    Yanase, Takashi
    Kubota, Yasushi
    Imai, Shigeki
    Matsumoto, Taketoshi
    Kobayashi, Hikaru
    APPLIED SURFACE SCIENCE, 2010, 256 (18) : 5610 - 5613
  • [6] Thin Ag film formation onto Si/SiO2 substrate
    Iida, S
    Okui, T
    Tai, T
    Akao, S
    APPLIED SURFACE SCIENCE, 2000, 166 (1-4) : 160 - 164
  • [7] Low temperature sound velocity of thin SiO2 films
    Gaganidze, E
    Konig, R
    Esquinazi, P
    Zimmer, K
    Burin, A
    PHYSICAL REVIEW LETTERS, 1997, 79 (25) : 5038 - 5041
  • [8] GISAXS study of Si nanocrystals formation in SiO2 thin films
    Pivac, B.
    Kovacevic, I.
    Dubcek, P.
    Radic, N.
    Bernstoff, S.
    THIN SOLID FILMS, 2006, 515 (02) : 756 - 758
  • [9] Stability and oxidation behavior of Ir thin film electrodes on Si and SiO2
    Saenger, KL
    Grill, A
    Shaw, TM
    Neumayer, DA
    Lin, CT
    Wang, YY
    FERROELECTRIC THIN FILMS VII, 1999, 541 : 119 - 127
  • [10] Stability and oxidation behavior of Ir thin film electrodes on Si and SiO2
    Saenger, K.L.
    Grill, A.
    Shaw, T.M.
    Neumayer, D.A.
    Lin, Chenting
    Wang, Y.Y.
    Materials Research Society Symposium - Proceedings, 1999, 541 : 119 - 127