Crevice corrosion of nickel superalloy in deaerated chloride/ sulphate solution at 90°C

被引:1
|
作者
Ortiz, M. Rincon [1 ]
Carranza, R. M. [2 ]
Rodriguez, M. A. [2 ]
机构
[1] Univ Ind Santander, Bucaramanga, Colombia
[2] Comis Nacl Energia Atom, Inst Sabato, Buenos Aires, DF, Argentina
关键词
ALLOY-22;
D O I
10.1088/1742-6596/786/1/012034
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Alloy 22 is a nickel base alloy highly resistant to all forms of corrosion. It was designed to resist to most aggressive environments for industrial applications. Electrochemical studies such as Potentiodynamic-Galvanostatic-Potentiostatic (PD-GS-PD) tests and Electrochemical Impedance Spectroscopy (EIS) and Scanning Electron Microscopy (SEM) observations were performed to determine the corrosion behaviour of alloy 22 (N06022). The effect of sulphate ion in chloride containing solutions at 90 degrees C, were studied in this work under aggressive conditions where this material might be susceptible to crevice corrosion. The electrolyte solution, which consisted of 0.1M and 1M NaCl and different sulphate concentrations. It was observed that there were complete inhibitions of crevice corrosion for R-CRIT=[SO4=]/[Cl-]=1 in the 0.1mol/L NaCl solutions and R-CRIT=2 in the 1mol/L NaCl solutions. The corrosion rate obtained was about 0.1 mu m/year at 24 hours of immersion.
引用
收藏
页数:4
相关论文
共 50 条
  • [41] Influence of interlayer on the corrosion behavior of multilayered WC-Ti1-xAlxN coatings in deaerated 3.5% sodium chloride solution
    Hong, J. H.
    Ahn, S. H.
    Kim, J. G.
    ECO-MATERIALS PROCESSING AND DESIGN VIII, 2007, 544-545 : 359 - +
  • [42] Corrosion resistance of 625 nickel superalloy exposed to isothermal and thermal cycling conditions in a chloride/carbonate salt
    Bell, Stuart
    de Bruyn, Mitchell
    Steinberg, Ted
    Will, Geoffrey
    SOLAR ENERGY, 2023, 249 : 278 - 287
  • [43] Anodic Stress Corrosion Cracking Suspectibility of Nickel and Nickel-Chromium Alloys Containing Molybdenum and Iron in Bicarbonate Plus Chloride Solutions at 90°C
    Zadorozne, N. S.
    Giordano, C. M.
    Rebak, R. B.
    Ares, A. E.
    Carranza, R. M.
    CORROSION, 2015, 71 (04) : 420 - 432
  • [44] Chemical Equilibria of Nickel Chloride in HCl Solution at 25°C
    Lee, Man Seung
    Nam, Sang-Ho
    BULLETIN OF THE KOREAN CHEMICAL SOCIETY, 2009, 30 (10): : 2203 - 2207
  • [45] Effects of applied potential and solution temperature on the pitting corrosion of pure aluminium in sulphate ion-containing chloride solution
    Suk-Soo Kim
    Woo-Jin Lee
    Su-Il Pyun
    Dai-Ryong Kim
    Metals and Materials, 1999, 5 : 583 - 588
  • [46] Effects of applied potential and solution temperature on the fitting corrosion of pure aluminium in sulphate ion-containing chloride solution
    Kim, SS
    Lee, WJ
    Pyun, SI
    Kim, DR
    METALS AND MATERIALS-KOREA, 1999, 5 (06): : 583 - 588
  • [47] The Role of Micro Pits in the Initiation Process of Crevice Corrosion of SUS304 Stainless Steel in an Aqueous Chloride Solution
    Nagaoka, Akira
    Nose, Kiyomi
    Nokami, Kana
    Kajimura, Haruhiko
    MATERIALS TRANSACTIONS, 2022, 63 (03) : 335 - 342
  • [48] The role of micro pit in the initiaion process of crevice corrosion of SUS304 stainless steel in aqueous chloride solution
    Nagaoka, Akira
    Nose, Kiyomi
    Nokami, Kana
    Kajimura, Haruhiko
    Zairyo to Kankyo/ Corrosion Engineering, 2021, 70 (02): : 32 - 39
  • [49] The effect of molybdenum on corrosion of low-temperature nitrided stainless steels in sulphate-chloride solution
    Flis, J.
    Kuczynska-Wydorska, M.
    Flis-Kabulska, I.
    JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2006, 10 (09) : 689 - 695
  • [50] INFLUENCE OF S2O32-, NO3-, AND AMMONIA IONS ON PITTING AND CREVICE CORROSION OF TITANIUM IN CHLORIDE SOLUTION AT 160-DEGREES-C
    KURNOSIKOVA, VN
    GORBACHEV, AK
    PROTECTION OF METALS, 1985, 21 (03): : 322 - 325