Texture Optimization for Intermediate Si-Containing Non-oriented Electrical Steel

被引:8
|
作者
Xie, Li [1 ]
Yang, Ping [1 ]
Zhang, Ning [1 ]
Mao, Weimin [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
heat treatment; magnetic; steel; SILICON STEEL; GRAIN-GROWTH; CRYSTALLOGRAPHIC TEXTURE; MAGNETIC-PROPERTIES; SHEETS; IRON; DECARBURIZATION; OXIDATION; MANGANESE; EVOLUTION;
D O I
10.1007/s11665-014-1201-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Columnar grains can be obtained by decarburization annealing in the two-phase region of Si-containing non-oriented electrical steel under wet-mixed atmosphere. However, iron oxidation or oxidation of alloying elements on the surface hinders the decarburization process and, consequently, the preferred microstructure and texture evolution. This study aims to optimize the texture and obtain excellent magnetic properties in intermediate Si-containing non-oriented electrical steel by process adjustments, such as final annealing under pure hydrogen atmosphere and coarsening initial microstructure by hot-band annealing. First, pure hydrogen atmosphere is used to weaken the surface oxidation layer and to promote the effect of anisotropic strain energy. Driven by anisotropic strain energy during phase transformation, a number of {100}-nearly oriented columnar grains are obtained. Second, high amounts of non-gamma fiber-oriented recrystallized grains, which strongly influence the final transformation texture, are observed during the rapid heating process in the final annealing because of the coarse initial microstructure. Non-gamma fiber-oriented grains grow from the surface into the center layer along the normal direction and form poor columnar grains by carbon diffusion during slow austenite to ferrite (gamma -> alpha) transformation in final annealing under pure hydrogen atmosphere. A notable increase in magnetic properties is observed, with magnetic induction at 5000/Am (B-50) above 1.76 T and core loss at 1.5 T by 50 Hz (P-15/50) below 2.6 W/kg.
引用
收藏
页码:3849 / 3858
页数:10
相关论文
共 50 条
  • [1] Texture Optimization for Intermediate Si-Containing Non-oriented Electrical Steel
    Li Xie
    Ping Yang
    Ning Zhang
    Weimin Mao
    [J]. Journal of Materials Engineering and Performance, 2014, 23 : 3849 - 3858
  • [2] Evolution of Recrystallization Texture in Non-Oriented Electrical Steel Containing Copper
    Nan Di
    Zeng Yan-ping
    Hu Guan-qiao
    Zhou Zi-yu
    [J]. PROGRESS IN NEW MATERIALS AND MECHANICS RESEARCH, 2012, 502 : 243 - 246
  • [3] Evolution of Texture in a 2.8% Si Non-Oriented Electrical Steel Annealed at 1100°C
    Li, Na
    Ma, Liang
    Xiang, Li
    Qiu, Shengtao
    Zhao, Pei
    [J]. MATERIALS TRANSACTIONS, 2014, 55 (02) : 387 - 390
  • [4] Microstructure and Texture of 0.75%Si Non-oriented Electrical Steel Fabricated by Strip Casting Process
    Chen A.-H.
    Li H.-L.
    [J]. Metallography, Microstructure, and Analysis, 2016, 5 (5) : 428 - 434
  • [5] Texture and magnetic properties improvement of a 3% Si non-oriented electrical steel by Sb addition
    Rodrigues, Marcio Ferreira
    da Cunha, Marco Antonio
    Paolinelli, Sebastiao da Costa
    Cota, Andre Barros
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2013, 331 : 24 - 27
  • [6] Texture Evolution of a 2.8 Wt Pct Si Non-oriented Electrical Steel and the Elimination of the ⟨111⟩//ND Texture
    Mehdi, Mehdi
    He, Youliang
    Hilinski, Erik J.
    Edrisy, Afsaneh
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2019, 50A (07): : 3343 - 3357
  • [7] Effect of heating rate on properties of non-oriented electrical steel containing 0.4% Si
    Bae, BK
    Woo, JS
    Kim, JK
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2003, 254 : 373 - 375
  • [8] Texture Evolution of a 2.8 Wt Pct Si Non-oriented Electrical Steel and the Elimination of the 〈111〉//ND Texture
    Mehdi Mehdi
    Youliang He
    Erik J. Hilinski
    Afsaneh Edrisy
    [J]. Metallurgical and Materials Transactions A, 2019, 50 : 3343 - 3357
  • [9] Texture optimization in non-oriented electrical steels: The role of the Goss texture component
    Landgraf, FJG
    Paolinelli, SC
    Cunha, MA
    de Campos, MF
    [J]. ICOTOM 14: TEXTURES OF MATERIALS, PTS 1AND 2, 2005, 495-497 : 543 - 552
  • [10] Effect of texture and grain size on magnetic flux density and core loss in non-oriented electrical steel containing 3.15% Si
    Lee, K. M.
    Park, S. Y.
    Huh, M. Y.
    Kim, J. S.
    Engler, O.
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2014, 354 : 324 - 332