Structure and thermal stability of melt spun and mechanically alloyed Cu47Ti34Zr11Ni8 and Cu47Ti34Sn11Ni8 alloys

被引:3
|
作者
Oleszak, D. [1 ]
Wierzbicki, L. [1 ]
Kulik, T. [1 ]
机构
[1] Warsaw Univ Technol, Fac Mat Sci & Engn, PL-02507 Warsaw, Poland
关键词
BULK METALLIC GLASSES;
D O I
10.1088/1742-6596/144/1/012023
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Two applied samples preparation techniques (rapid quenching from the melt and mechanical alloying) resulted in the formation of fully amorphous Cu47Ti34Zr11Ni8 and Cu47Ti34Sn11Ni8 alloys. However, a significant differences in thermal stability and crystallization behaviour have been found, depending not only on the alloy composition, but on the fabrication method as well. MA powders of both alloys studied revealed one dominating DSC exothermic effect. Zr-containing ribbon showed four exothermic effects, while Sn-containing one - only two overlapping peaks. In the case of ribbons it was found that replacing Zr by Sn did not influenced the crystallization temperature or supercooled liquid region, however, the activation energy of crystallization increased significantly, from 190 to 223 kJmol(-1). Opposite behaviour was observed for MA powders. Introducing Sn into the alloy instead of Zr resulted in a considerably increase of the crystallization temperature (from 783 to 826 K), simultaneously the activation energy for crystallization remained the same.
引用
收藏
页数:4
相关论文
共 50 条
  • [31] Wear and corrosion properties of laser cladded Cu47Ti34Zr11Ni8/SiC amorphous composite coatings on AZ91D magnesium alloy
    Huang Kai-jin
    Yan Li
    Wang Cun-shan
    Xie Chang-sheng
    Zhou Chang-rong
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (07) : 1351 - 1355
  • [32] 在水冷铜坩埚中用吸铸法制备Cu47Ti34Zr11Ni8块状非晶合金
    寇生中
    岳武
    丁雨田
    许广济
    [J]. 科学技术与工程, 2006, (03) : 302 - 303
  • [33] On the fragility of Cu47Ti33Zr11Ni8Si1 metallic glass
    Venkataraman, S.
    Biswas, K.
    Wei, B. C.
    Sordelet, D. J.
    Eckert, J.
    [J]. JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2006, 39 (12) : 2600 - 2608
  • [34] Improvement of the glass-forming ability of Zr55Cu30Al10Ni5 and Cu47Ti34Zr11Ni83Ni8 alloys by electro-deoxidation of the melts
    Castellero, A.
    Bossuyt, S.
    Stoica, M.
    Deledda, S.
    Eckert, J.
    Chen, G. Z.
    Fray, D. J.
    Greer, A. L.
    [J]. SCRIPTA MATERIALIA, 2006, 55 (01) : 87 - 90
  • [35] Cu/Ti base multicomponent amorphous Cu47Ti33Zr11Ni8Si1 and nanocrystalline silver composites
    Dutkiewicz, Jan
    Litynska-Dobrzynska, Lidia
    Rogal, Lukasz
    Maziarz, Wojciech
    Czeppe, Tomasz
    [J]. PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2010, 207 (05): : 1109 - 1113
  • [36] Effect of adding elements on glass-forming ability of (Cu47Ti34Zr11Ni8)99M (M = Al, Be, Si, Nb, Fe and Co) bulk amorphous alloys
    Kong, Jian
    Xiong, Dangsheng
    Ma, Xuan
    Li, Jianliang
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 2010, 356 (20-22) : 952 - 957
  • [37] In situ synthesis of TiC reinforcedCu47Ti34Zr11Ni8 bulk metallic glass composites
    Sun, YF
    Zhang, GS
    Wei, BC
    Li, WH
    Wang, YR
    [J]. CHINESE SCIENCE BULLETIN, 2004, 49 (06): : 542 - 546
  • [38] Metallic glass formation in the Cu47Ti33Zr11Ni8Si1 alloy
    Venkataraman, S.
    Bartusch, B.
    Mickel, C.
    Kim, K. B.
    Das, J.
    Scudino, S.
    Stoica, M.
    Sordelet, D. J.
    Eckert, J.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 444 (1-2): : 257 - 264
  • [39] Glass formation and crystallization of CU47Ti33Zr11Ni8X1 (X = Fe, Si, Sn, Pb) alloys
    Calin, M
    Stoica, M
    Eckert, J
    Yavari, AR
    Schultz, L
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 392 (1-2): : 169 - 178
  • [40] Phase formation, thermal stability and crystallization behavior of Cu47Ti33Zr11Ni8X1, (X = Fe, Si, Sn, Pb) bulk glassy alloys
    Calin, M
    Stoica, M
    Eckert, J
    Yavari, AR
    Schultz, L
    [J]. ZEITSCHRIFT FUR METALLKUNDE, 2004, 95 (11): : 970 - 977