Crystallization of sputtered NiTi films

被引:0
|
作者
Vestel, MJ [1 ]
Grummon, DS [1 ]
Pisano, AP [1 ]
机构
[1] Univ Calif Berkeley, Lawrence Berkeley Lab, LUSTER, Berkeley, CA 94720 USA
关键词
D O I
暂无
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Sputtered, crystalline thin films of nickel-titanium (NiTi) can display both superelastic properties and the shape memory effect, either of which may be used in films for MEMS sensors and actuators. However, direct deposition of crystalline NiTi films requires high deposition temperature and cooldown can lead to catastrophic delamination from extrinsic residual stress. To avoid delamination, especially for thick films (>5 micrometers) the amorphous form of NiTi can be sputter deposited at a low temperature, patterned and etched, released, and then crystallized to develop the proper microstructure. Here we report some results from a study of the crystallization process using differential scanning calorimetry (DSC) and transmission electron microscopy (TEM). The minimum temperature for complete crystallization in a reasonable length of time was found to be about 400degreesC. Crystalline grains always nucleated first at the surface, rapidly grew laterally until impingement, and then continued to grow inward to form columnar grains as the parent amorphous phase was consumed. Surface roughness delayed the onset of surface nucleation. For very smooth surfaces, crystallization nucleated quickly, but after lateral impingement, growth inward was apparently more sluggish. Multiple DSC exotherms observed in some cases suggest that additional nucleation events may have occurred in the interior of the films.
引用
收藏
页码:7 / 13
页数:7
相关论文
共 50 条
  • [31] Crystallization kinetics of amorphous NiTi shape memory alloy thin films
    Wang, X
    Vlassak, JJ
    SCRIPTA MATERIALIA, 2006, 54 (05) : 925 - 930
  • [32] Composition analysis of NiTi thin films sputtered from a mosaic target: synthesis and simulation
    Abhilash, V
    Sumesh, MA
    Mohan, S
    SMART MATERIALS AND STRUCTURES, 2005, 14 (05) : S323 - S328
  • [33] Surface morphology of sputtered NiTi-based shape memory alloy thin films
    Huang, X
    Liu, Y
    SURFACE & COATINGS TECHNOLOGY, 2005, 190 (2-3): : 400 - 405
  • [34] PLASTIC DEFORMATION OF SPUTTERED NITI THIN FILMS ON POLYIMIDE SUBSTRATES BY CO-ROLLING
    Foltz, John
    Grummon, D. S.
    Zhang, Yijun
    SMST 2006: PROCEEDINGS OF THE INTERNATIONAL CONFERENCE ON SHAPE MEMORY AND SUPERELASTIC TECHNOLOGIES, 2008, : 323 - 330
  • [35] OBSERVATIONS OF PROPAGATION IN SHOCK-CRYSTALLIZATION OF SPUTTERED AMORPHOUS GERMANIUM FILMS
    MINEO, A
    MATSUDA, A
    KUROSU, T
    KIKUCHI, M
    SOLID STATE COMMUNICATIONS, 1973, 13 (09) : 1307 - 1310
  • [36] Thickness effect on the crystallization characteristic of RF sputtered Sb thin films
    Yufeng Huang
    Weihua Wu
    Shengqing Xu
    Xiaoqin Zhu
    Sannian Song
    Zhitang Song
    Journal of Materials Science: Materials in Electronics, 2021, 32 : 24240 - 24247
  • [37] Analysis of crystallization kinetics of sputtered SmCo based permanent magnetic films
    Peng, Long
    Li, Lezhong
    Yang, Dingyu
    Zhu, Xinghua
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2012, 324 (08) : 1539 - 1542
  • [38] Laser induced crystallization of sputtered MoS2 thin films
    Tonon, Alessandro
    Di Russo, Enrico
    Sgarbossa, Francesco
    Bacci, Luca
    Argiolas, Nicola
    Scian, Carlo
    Ivanov, Yurii P.
    Divitini, Giorgio
    Sheehan, Brendan
    De Salvador, Davide
    Gasparotto, Andrea
    Morandi, Vittorio
    Duffy, Ray
    Napolitani, Enrico
    MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2023, 164
  • [39] Thickness effect on the crystallization characteristic of RF sputtered Sb thin films
    Huang, Yufeng
    Wu, Weihua
    Xu, Shengqing
    Zhu, Xiaoqin
    Song, Sannian
    Song, Zhitang
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2021, 32 (19) : 24240 - 24247
  • [40] EXPLOSIVE CRYSTALLIZATION OF RF-SPUTTERED AMORPHOUS CDTE-FILMS
    KRISHNASWAMY, SV
    MESSIER, R
    SWAB, P
    TONGSON, LL
    VEDAM, K
    JOURNAL OF ELECTRONIC MATERIALS, 1981, 10 (03) : 433 - 443