Effect of water vapor on the oxidation behavior of fe-0.5 and 5 mass%Ni alloys in air at 1273 K

被引:3
|
作者
Fukumoto, M
Hayashi, S
Maeda, S
Narita, T
机构
[1] Hokkaido Univ, Grad Sch Engn, Res Grp Interface Control Engn, Sapporo, Hokkaido 0608628, Japan
[2] Nippon Steel Corp Ltd, Steel Res Labs, Futtsu 2930011, Japan
关键词
iron-nickel alloy; high temperature oxidation; effect of water vapor; oxidation kinetics; inner layer; dissociation;
D O I
10.2320/jinstmet1952.66.5_513
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Oxidation behavior of Fe-0.5 and 5 mass%Ni alloys(0.5Ni, 5Ni) as well as Fe for comparison, was investigated at 1273 K for up to 7.2 ks in air and air containing 10.5 vol%H2O (air-10.5H(2)O) . In the air-10.5H(2)O, the 0.5Ni and 5Ni were oxidized faster than in air. The scale was composed of a duplex structure, an outer Fe-oxides layer and an inner FeO + Ni layer containing voids. Marker experiments with a small Pt wire were carried out for the 5Ni oxidized in air and the Pt-marker was located between the inner and outer layers, suggesting that the inner layer grows due to inward migration of oxygen and the outer layer clue to outward iron diffusion. A similar scale structure was observed for the 5Ni oxidized in air but the inner layer thickness of the 5Ni oxidized in air-10.5H(2)O was thicker than in air. Oxygen in the inner FeO + Ni layer formed in air was supplied by the dissociation of outer Fe-oxides, leaving voids there, probably by the perforating dissociation mechanism. Both oxygen and water molecules could be diffusing species through the void in the atmosphere containing water vapor. Concentration profiles of each element indicated that concentration of Ni was increased at the scale/alloy interface. The Ni-concentration of the 0.5Ni oxidized in air was lower than that in air-10.5H(2)O, but the Ni-concentration of the 5Ni oxidized in air was higher than that in air-10.5H(2)O.
引用
收藏
页码:513 / 520
页数:8
相关论文
共 50 条
  • [31] Effect of Water Vapor on the Oxidation of Pt-modified Ni-22Al Alloys
    S.HAYASHI
    M.AUCHI
    T.NARITA
    B.GLEESON
    中国腐蚀与防护学报, 2009, 29 (04) : 317 - 318
  • [32] Competitive effect of water vapor and oxygen on the oxidation of Fe-5 wt.% Al alloy at 1073 K
    Hayashi, S
    Narita, T
    OXIDATION OF METALS, 2001, 56 (3-4): : 251 - 270
  • [33] Effect of coatings on the creep and oxidation behavior of TiAl alloys at 1173K in air
    Nishimoto, Takumi
    Hayashi, Shigenari
    Narita, Toshio
    HIGH-TEMPERATURE OXIDATION AND CORROSION 2005, 2006, 522-523 : 665 - 672
  • [34] Effect of oxidation resistant coatings on the deformation behavior of TiAl alloys at 1173 K in air
    Nishimoto, Takumi
    Hayashi, Shigenari
    Narita, Toshio
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2007, 71 (01) : 25 - 33
  • [35] Water Vapor Effects on the Oxidation Behavior of Fe-Cr and Ni-Cr Alloys in Atmospheres Relevant to Oxy-fuel Combustion
    Mu, N.
    Jung, K. Y.
    Yanar, N. M.
    Meier, G. H.
    Pettit, F. S.
    Holcomb, G. R.
    OXIDATION OF METALS, 2012, 78 (3-4): : 221 - 237
  • [36] Effect of Water Vapor in Air on the Oxidation Behavior of Ferritic Stainless Steels for SOFC Interconnects
    Chung, J. H.
    Huh, J. Y.
    Jun, J. H.
    Kim, D. H.
    Jun, Joong-Hwan
    THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 : 305 - 309
  • [37] Role of nickel in the oxidation of Fe-Cr-Ni alloys in air-water vapour atmospheres
    Pettersson, RFA
    Enecker, J
    Liu, L
    MATERIALS AT HIGH TEMPERATURES, 2005, 22 (3-4) : 269 - 281
  • [38] Oxidation behavior of the single crystal Ni-based superalloy at 900 °C in air and water vapor
    Wu, Ying
    Narita, Toshio
    SURFACE & COATINGS TECHNOLOGY, 2007, 202 (01): : 140 - 145
  • [39] Effect of Grain Size on Oxidation Behavior of Fe-40Ni-15Cr Alloys
    Cao, Z. Q.
    Sun, Y.
    Sun, H. J.
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2012, 31 (01) : 83 - 87
  • [40] The Effects of Al Addition on the Oxidation Behavior of Ni-Fe-Cr-Nb Alloys at 800 °C in Air
    Kuo, Yen-Ling
    Kakehi, Koji
    Nanko, Makoto
    Hayashi, Shigenari
    HIGH TEMPERATURE CORROSION OF MATERIALS, 2024, 101 (04) : 667 - 683