Tensile fracture behavior of continuous SiC fiber-reinforced SiC matrix composites at elevated temperatures and correlation to in situ constituent properties

被引:58
|
作者
Guo, SQ [1 ]
Kagawa, Y [1 ]
机构
[1] Univ Tokyo, Inst Ind Sci, Minato Ku, Tokyo 1068558, Japan
基金
日本学术振兴会;
关键词
composites; fiber strength; interface shear stress; mechanical properties; polymer infiltration pyrolysis; SiC/SiC;
D O I
10.1016/S0955-2219(02)00028-6
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The tensile fracture behavior and tensile mechanical properties of polymer infiltration pyrolysis (PIP)-processed two-dimensional plain-woven fabric carbon-coated Nicalon(TM) SiC fiber and BN-coated Hi-Nicalon(TM) SiC fiber-reinforced SiC matrix composites have been investigated. Tensile testing of the composites was carried out in air between 298 and 1400 K. In situ fiber strength and interface shear stress were determined by fracture mirror size and pulled-out fiber length measurements. For the Nicalon/C/SiC, tensile strength remained nearly constant up to 800 K, and while the strength dropped from 140 MPa at 800 K to 41 MPa at 1200 K, with weakest link failure mode. For the Hi-Nicalon/BN/SiC, the tensile strength increased slightly with increase in test temperature up to 1200 K; however, a large decrease in the strength was observed at 1400 K. In the case of the Hi-Nicalon/BN/SiC, the fracture was governed by fiber bundle strength. The temperature dependence of tensile strength and fracture behavior of both composites was attributed to change of the in situ constituent properties with temperature. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2349 / 2356
页数:8
相关论文
共 50 条
  • [11] Effect of Interface Properties on Tensile and Fatigue Behavior of 2D Woven SiC/SiC Fiber-Reinforced Ceramic-Matrix Composites
    Li, Longbiao
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2020, 2020
  • [12] Oxidation of SiC Fiber-reinforced SiC Matrix Composites with a BN Interphase
    Opila, Elizabeth J.
    Boyd, Meredith K.
    HIGH-TEMPERATURE OXIDATION AND CORROSION 2010, 2011, 696 : 342 - +
  • [13] Compressive creep behavior of SiC fiber-reinforced mullite matrix composites
    Deng, ZY
    Kobayashi, T
    22ND ANNUAL CONFERENCE ON COMPOSITES, ADVANCED CERAMICS, MATERIALS, AND STRUCTURES: A, 1998, 19 (03): : 129 - 136
  • [14] Comparison of prior exposure tensile damage and fracture of two-dimensional C/SiC and SiC/SiC fiber-reinforced ceramic-matrix composites
    Li, Longbiao
    TEXTILE RESEARCH JOURNAL, 2020, 90 (23-24) : 2782 - 2794
  • [15] Tensile Behavior of SiC Fiber-Reinforced γ-TiAl Composites Prepared by Suction Casting
    Yingying Shen
    Qing Jia
    Xu Zhang
    Ronghua Liu
    Yumin Wang
    Yuyou Cui
    Rui Yang
    Acta Metallurgica Sinica (English Letters), 2021, 34 : 932 - 942
  • [16] Tensile Behavior of SiC Fiber-Reinforced γ-TiAl Composites Prepared by Suction Casting
    Yingying Shen
    Qing Jia
    Xu Zhang
    Ronghua Liu
    Yumin Wang
    Yuyou Cui
    Rui Yang
    ActaMetallurgicaSinica(EnglishLetters), 2021, 34 (07) : 932 - 942
  • [17] Tensile Behavior of SiC Fiber-Reinforced γ-TiAl Composites Prepared by Suction Casting
    Shen, Yingying
    Jia, Qing
    Zhang, Xu
    Liu, Ronghua
    Wang, Yumin
    Cui, Yuyou
    Yang, Rui
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2021, 34 (07) : 932 - 942
  • [18] Preparation of SiC fiber-reinforced SiC composites
    He, XB
    Yang, H
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 159 (01) : 135 - 138
  • [19] Effect of residual stress on matrix cracking in continuous fiber-reinforced SiC matrix composites
    Itoh, Yoshiyasu
    Suyama, Shoko
    Kameda, Tsuneji
    Nishida, Katsutoshi
    Zairyo/Journal of the Society of Materials Science, Japan, 2000, 49 (01) : 66 - 71
  • [20] Temperature dependence of in situ constituent properties of polymer-infiltration-pyrolysis-processed Nicalon™ SiC fiber-reinforced SiC matrix composite
    Shuqi Guo
    Yutaka Kagawa
    Journal of Materials Research, 2000, 15 : 951 - 960