Microstructure and hydrogen absorption/desorption properties of Mg24Y3M (M = Ni, Co, Cu, Al) alloys

被引:27
|
作者
Yang, Tai [1 ,2 ,3 ]
Li, Qiang [1 ,2 ]
Liang, Chunyong [1 ,2 ]
Wang, Xinghua [1 ,2 ]
Xia, Chaoqun [1 ,2 ]
Wang, Hongshui [1 ,2 ]
Yin, Fuxing [1 ,2 ]
Zhang, Yanghuan [3 ]
机构
[1] Hebei Univ Technol, Sch Mat Sci & Engn, Res Inst Energy Equipment Mat, Tianjin 300130, Peoples R China
[2] Hebei Univ Technol, Tianjin Key Lab Laminating Fabricat & Interface C, Tianjin 300130, Peoples R China
[3] Cent Iron & Steel Res Inst, Dept Funct Mat Res, Beijing 100081, Peoples R China
关键词
Hydrogen storage; Mg-based alloy; Multiphase structure; Kinetics; Thermodynamics; STACKING ORDERED STRUCTURE; STORAGE PROPERTIES; INDUCED AMORPHIZATION; DESORPTION-KINETICS; HYDRIDING PROPERTIES; METAL-HYDRIDES; LAVES PHASES; MELT-SPUN; COMPOSITE; TRANSITION;
D O I
10.1016/j.ijhydene.2018.02.199
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ternary alloys with the nominal composition of Mg24Y3M (M = Ni, Co, Cu, Al) have been fabricated by using vacuum induction melting method. Their microstructure and phase composition are characterized by using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The isothermal hydrogen absorption and desorption kinetics are measured by a Sievert's-type apparatus. The dehydrogenation behaviors of the full hydrogenated alloys are also analyzed by differential scanning calorimetry (DSC) method. Results show that each and every alloy has a distinct multiphase structure containing the main phase Mg24Y5 and some amount of Mg. Intermetallic compounds of YCo2 and Al2Y are detected in the M = Co and M = Al alloy, while long-period stacking ordered (LPSO) phase can be also observed in M = Ni and M = Cu alloy. The hydrogen absorption and desorption kinetics shows a decreased trend in the following order: (M = Ni) > (M = Al) > (M = Co) > (M = Cu). The M = Ni alloy has the best hydrogen storage performance among the investigated alloys. The dehydrogenation activation energy (E-a) of the M = Ni alloy decreases to 66 kJ/mol, and its decomposition peak temperature is also reduced to 313 degrees C. Moreover, the p-c-T (pressure-composition isotherms) curves of the studied alloys are also discussed. (C) 2018 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:8877 / 8887
页数:11
相关论文
共 50 条
  • [21] Hydrogen absorption and desorption in rapidly solidified Mg-Al alloys
    Urgnani, J.
    Di Chio, M.
    Palumbo, M.
    Feuerbacher, M.
    Fernandez, J. F.
    Leardini, F.
    Baricco, M.
    13TH INTERNATIONAL CONFERENCE ON RAPIDLY QUENCHED AND METASTABLE MATERIALS, 2009, 144
  • [22] Hydrogen storage properties of LaNi3.8Al1.0M0.2 (M = Ni, Cu, Fe, Al, Cr, Mn) alloys
    Li, S. L.
    Wang, P.
    Chen, W.
    Luo, G.
    Chen, D. M.
    Yang, K.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 485 (1-2) : 867 - 871
  • [23] Advanced interpretation of hydrogen absorption process in LaMgNi3.6M0.4 (M = Ni, Mn, Al, Co, Cu) alloys using statistical physics treatment
    Bouaziz, Nadia
    Aouaini, Fatma
    Ben Torkia, Yosra
    Altowyan, Abeer S.
    Ben Lamine, Abdelmottaleb
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (17) : 10389 - 10395
  • [24] Viscosity of molten Cu-M alloys (M = Ni, Al)
    Takeda, Osamu
    Ouchi, Noritaka
    Takagi, Kounosuke
    Sato, Yuzuru
    Zhu, Hongmin
    HIGH TEMPERATURES-HIGH PRESSURES, 2023, 52 (3-4) : 211 - 227
  • [25] Catalytic Decomposition of Methane Over M–Co–Al Catalysts (M = Mg, Ni, Zn, Cu)
    Natanael A. Hermes
    Marla A. Lansarin
    Oscar W. Perez-Lopez
    Catalysis Letters, 2011, 141 : 1018 - 1025
  • [26] Hydrogen storage properties of Mg1.7M0.3Ni(M=Mg, La, Ce, Nd) hydrogen storage alloys
    Li, Yunlong
    Li, Ping
    Zhai, Fuqiang
    Zhang, Weina
    Qu, Xuanhui
    RENEWABLE AND SUSTAINABLE ENERGY II, PTS 1-4, 2012, 512-515 : 1503 - 1508
  • [27] Hydrogen absorption/desorption characteristics of Mg-V-Ni hydrogen storage alloys
    Sakamoto, Tomoya
    Atsumi, Hisao
    FUSION ENGINEERING AND DESIGN, 2019, 138 : 6 - 9
  • [28] Improved physical and electrochemical hydrogen storage kinetics of the as-spun Mg2Ni-type alloys by substituting Ni with M (M=Co, Cu)
    Zhang, Yang-huan
    Li, Bao-wei
    Ren, Hui-ping
    Pang, Zai-guang
    Hou, Zhong-hui
    Zhao, Dong-liang
    FRONTIERS OF ADVANCED MATERIALS AND ENGINEERING TECHNOLOGY, PTS 1-3, 2012, 430-432 : 423 - +
  • [29] Ameliorated microstructure and hydrogen absorption/desorption properties of novel Mg-Ni-La alloy doped with MWCNTs and Co nanoparticles
    Guo, Fenghai
    Zhang, Tiebang
    Shi, Limin
    Chen, Yu
    Song, Lin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (41) : 18044 - 18057
  • [30] Hydrogen Absorption Properties of Zr-V-M(M=Fe, Ga, Y) Getter Alloys
    Park, Je-Shin
    Suh, Chang-Youl
    Kim, Won-Baek
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2005, 15 (06): : 388 - 392