Oxidation and Adhesion of Decorative Nickel-Chromium Plating on Ferritic Stainless Steel

被引:0
|
作者
Wongpinij, Thipusa [1 ]
Wongpanya, Pornwasa [1 ]
机构
[1] Suranaree Univ Technol, Inst Engn, Sch Met Engn, Nakhon Ratchasima 30000, Thailand
关键词
Oxidation; Adhesion; Ferritic stainless steel; Decorative Ni-Cr plating; Carbon Dioxide;
D O I
10.4028/www.scientific.net/AMR.785-786.852
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Decorative Ni-Cr plating on ferritic stainless steel was exposed to pure carbon dioxide (CO2) at 200 and 300 degrees C for 180 hours under continuous and cyclic oxidation tests. After oxidation test, weight changes of samples exposed to CO2 were found to be less than that of samples exposed to air. However, weight changes were dependent on temperature and oxidation conditions. Heat-quench test was operated at temperature of 200-500 degrees C for determining adhesion behavior of decorative Ni-Cr plating. From the heat-quench test, it revealed that adhesion ability between Ni-Cr plating layer and substrate increased with thickness of Ni pre-plating layer at temperature of 200 and 300 degrees C. But, at temperature above 300 degrees C, the adhesion ability increased with surface roughness of substrate before coating. In order to achieve important properties of decorative Ni-Cr plating, i.e., oxidation resistance, beautiful appearance and good adhesion, surface of substrate was necessarily prepared under medium roughness and then it was pre-plated with the thickest Ni layer before Cr coating was applied.
引用
收藏
页码:852 / 857
页数:6
相关论文
共 50 条