Effects of cerium and manganese on corrosion of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO2 and Ar-20CO2-20H2O gases at 650 °C

被引:48
|
作者
Nguyen, Thuan Dinh [1 ]
Zhang, Jianqiang [1 ]
Young, David J. [1 ]
机构
[1] Univ New S Wales, Sch Mat Sci & Engn, Sydney, NSW 2052, Australia
基金
澳大利亚研究理事会;
关键词
Rare earth elements; Stainless steel; Carburisation; High temperature corrosion; DIFFUSION-COEFFICIENT; INTERNAL OXIDATION; HYDROGEN ATTACK; CHROMIA SCALES; CARBURIZATION; STEELS; IRON; RELEVANT; BEHAVIOR; KINETICS;
D O I
10.1016/j.corsci.2015.08.012
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Model alloys Fe-9Cr, Fe-20Cr and Fe-20Cr-20Ni (wt.%) with 0.1% Ce or 2% Mn were exposed to Ar-20CO(2) and Ar-20CO(2)-20H(2)O gas mixtures at 650 degrees C. Ferritic alloys underwent breakaway oxidation in both gases. Manganese additions significantly improved the oxidation resistance of Fe-20Cr in dry but not wet CO2. Water vapour accelerated internal oxidation of Fe-(9, 20)Cr. Austenitic alloys were more protective during corrosion in wet CO2. Cerium/manganese improved Fe-20Cr-20Ni performance in dry but not wet CO2. Most alloys carburised beneath their scales in both gases. Breakaway resistance is discussed in terms of Wagner's criteria for selective chromia scaling. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:448 / 465
页数:18
相关论文
共 50 条
  • [41] Effect of 0.3 at. % Ce on the corrosion resistance of Fe40Ni20Co20Cr20 40 Ni 20 Co 20 Cr 20 high-entropy alloy in 3.5 wt% NaCl solution
    Guo, Qiang
    Liu, Bin
    Li, Qiang
    Xie, Jiuqi
    MATERIALS LETTERS, 2024, 364
  • [42] SULFIDATION BEHAVIOR OF FE-25CR-20NI-3SI IN H2/H2O/H2S/AR AT 700-DEGREES-C
    SRINIVASAN, V
    PADGETT, RA
    CHOUDHURY, A
    CORROSION, 1991, 47 (09) : 703 - 712
  • [43] Mechanical properties of nano grained Ni20Cr20Fe5Nb1Y2O3 composite and Ni20Cr20Fe5Nb2Al alloy
    Kim, IH
    Kim, YH
    Kim, CS
    ADVANCES IN FRACTURE AND STRENGTH, PTS 1- 4, 2005, 297-300 : 250 - 256
  • [44] HIGH-TEMPERATURE OXIDATION OF FE-CR ALLOYS IN AR-10-PERCENT-H2O ATMOSPHERE
    KUSABIRAKI, K
    TOKI, H
    ASAMI, K
    ISHIGURO, T
    OOKA, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1988, 74 (05): : 863 - 870
  • [45] Precipitation strengthening of ductile Cr15Fe20Co35Ni20Mo10 alloys
    Ming, Kaisheng
    Bi, Xiaofang
    Wang, Jian
    SCRIPTA MATERIALIA, 2017, 137 : 88 - 93
  • [46] INFLUENCE OF A LITTLE AMOUNT OF H2S ON CO2 CORROSION OF FE-CR BINARY-ALLOYS
    UEDA, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 (05): : S685 - S685
  • [47] Microstructure and Phase Transformation in Fe20Co20Ni20Cr20B201xSix Alloys Prepared by Mechanical Alloying
    Zhang, Yicheng
    Ishimaru, Manabu
    Tokunaga, Tatsuya
    Era, Hidenori
    MATERIALS TRANSACTIONS, 2023, 64 (11) : 2568 - 2574
  • [48] Corrosion behavior of Fe-Cr alloys in Li2CO3-K2CO3 molten carbonate
    Takeuchi, K
    Nishijima, A
    Ui, K
    Koura, N
    Loong, CK
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (09) : B364 - B368
  • [49] MIXED OXIDATION OF FE-CR, FE-AL, AND FE-CR-AL ALLOYS IN AR-CL2-O2 ENVIRONMENTS BETWEEN 900 AND 1200 K
    KIM, AS
    MCNALLAN, MJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1987, 134 (03) : C110 - C110
  • [50] Water vapour effects on corrosion of Ni-Cr alloys in CO2 gas at 650 °C
    Xie, Yun
    Zhang, Jianqiang
    Young, David J.
    CORROSION SCIENCE, 2018, 136 : 311 - 325