Effect of heat treatment and in vitro aging on the microstructure and mechanical properties of cold isostatic-pressed zirconia ceramics for dental restorations

被引:21
|
作者
Vatali, Anna [1 ]
Kontonasaki, Eleana [1 ]
Kavouras, Panagiotis [2 ,4 ]
Kantiranis, Nikolaos [3 ]
Papadopoulou, Lambrini [3 ]
Paraskevopoulos, Konstantinos K. M. [4 ]
Koidis, Petros [1 ]
机构
[1] Aristotle Univ Thessaloniki, Sch Dent, Dept Fixed Prosthesis & Implant Prosthodont, GR-54124 Thessaloniki, Greece
[2] Technol Educ Inst Thessaloniki, Dept Appl Sci, Sindos, Greece
[3] Aristotle Univ Thessaloniki, Dept Geol, GR-54124 Thessaloniki, Greece
[4] Aristotle Univ Thessaloniki, Dept Phys, GR-54124 Thessaloniki, Greece
关键词
Y-TZP zirconia ceramics; Nano-hardness; Elastic constant; Heat-treatment; Aging; Monoclinic zirconia; XRD; FTIR; SEM; FLEXURAL STRENGTH; FRACTURE-RESISTANCE; GRAIN-SIZE; TRANSFORMATION; TEMPERATURE; SURFACE; DEGRADATION; ZRO2; POLYCRYSTALS; PERFORMANCE;
D O I
10.1016/j.dental.2014.05.017
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The temperature variations during the veneering firing cycles of a zirconia dental ceramic can negatively affect its mechanical properties. A possible synergistic effect of both heat-treatment and aging while exposed to the oral environment could result to catastrophic failure. The aim of the present study was to investigate the effect of heat treatment followed during veneering and in vitro aging on the mechanical and microstructural properties of zirconia dental ceramics. Methods. Three specimens from each of two zirconia blocks (Ivoclar IPS e.max ZirCAD (IV) and Wieland ZENO Zr (WI)) were cut by CAD/CAM technology, fully sintered and polished. Each one was cut in four equal parts. One part was used as control (C), one was heat-treated (H), one was aged (A) (134 degrees C, 2 bar, 10 h) and one was heat-treated and subsequently aged (HA). The mechanical properties (nano-hardness (H) and elastic modulus (0) were investigated by nano-indentation tests while the surface characterization was carried out with XRD, FTIR and SEM. Results. Different treatments on IV and WI samples resulted in a reduction of both H and E* values, however the differences were not statistically significant (p > 0.05). The combination of treatments imposes an overall effect (p <0.001), enhancing the influence on both H and E* values. This reduction in mechanical properties was followed by an increase of monoclinic content. Greater variations in both H and E* values were recorded for WI samples. Signcance. The clinical performance of zirconia dental ceramics may be affected during firing and aging resulting in increased probability of failure. (C) 2014 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:E272 / E282
页数:11
相关论文
共 50 条
  • [21] Effect of the Prior Particle Boundary on the Microstructure and Mechanical Properties of Hot-Isostatic-Pressed IN718 Alloy
    Kuo, Yen-Ling
    Kakehi, Koji
    MATERIALS TRANSACTIONS, 2017, 58 (07) : 1042 - 1048
  • [22] Effect of Chairside Rapid Sintering Process on Microstructure and Mechanical Properties of TZP Zirconia Ceramics
    Han, Yanfeng
    Zheng, Dongxiang
    Wang, Qiuyue
    Si, Wenjie
    JOURNAL OF BIOMATERIALS AND TISSUE ENGINEERING, 2018, 8 (01) : 95 - 102
  • [23] Effect of Solution and Aging Heat Treatment on the Microstructure and Mechanical Properties of Inconel 625 Deposited Metal
    Wang, Yingdi
    Su, Yunhai
    Dai, Zhiyong
    CRYSTALS, 2024, 14 (09)
  • [24] Effect of Heat Treatment on Microstructure and Mechanical Properties of New Cold-Rolled Automotive Steels
    Huang, Fei
    Chen, Jian
    Ge, Zhangqi
    Li, Junliang
    Wang, Yongqiang
    METALS, 2020, 10 (11) : 1 - 9
  • [25] Effects of Hot Isostatic Pressing and Heat Treatment on the Microstructure and Mechanical Properties of Cast TiAl Alloy
    Yu, Wen
    Zhou, Jianxin
    Yin, Yajun
    Feng, Xin
    Nan, Hai
    Lin, Junpin
    Ding, Xianfei
    Duan, Wei
    METALS, 2021, 11 (08)
  • [26] Effect of heat treatment on the microstructure and mechanical properties of SiCf/Ti55531 composite fabricated by hot isostatic pressing
    Li, Guanliang
    Jiang, Xueqi
    Jia, Qiuyue
    Zhang, Yuming
    Li, Mushi
    Yang, Lina
    Gao, Ximan
    Wang, Yifan
    Wang, Yumin
    Yang, Rui
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1016
  • [27] Influence of heat treatment on the microstructure and the physical and mechanical properties of dental highly translucent zirconia (vol 14, pg 96, 2022)
    Dimitriadis, K.
    Sfikas, A. K.
    Kamnis, S.
    Tsolka, P.
    Agathopoulos, S.
    JOURNAL OF ADVANCED PROSTHODONTICS, 2023, 15 (06): : 333 - 333
  • [28] The Effect of Heat Treatment and Feldspathic Glazing on Some Mechanical Properties of Zirconia
    Hjerppe, Jenni
    Froberg, Kaj
    Lassila, Lippo V. J.
    Vallittu, Pekka K.
    SILICON, 2010, 2 (03) : 171 - 178
  • [29] The Effect of Heat Treatment and Feldspathic Glazing on Some Mechanical Properties of Zirconia
    Jenni Hjerppe
    Kaj Fröberg
    Lippo V. J. Lassila
    Pekka K. Vallittu
    Silicon, 2010, 2 : 171 - 178
  • [30] Effect of in vitro aging on the flexural strength and probability to fracture of Y-TZP zirconia ceramics for all-ceramic restorations
    Siarampi, Eleni
    Kontonasaki, Eleana
    Andrikopoulos, Konstantinos S.
    Kantiranis, Nikolaos
    Voyiatzis, George A.
    Zorba, Triantafillia
    Paraskevopoulos, Konstantinos M.
    Koidis, Petros
    DENTAL MATERIALS, 2014, 30 (12) : E306 - E316