Challenges and Improvement Strategies Progress of Lithium Metal Anode

被引:50
|
作者
Liu, Fanfan [1 ]
Zhang, Zhiwen [1 ]
Ye, Shufen [1 ]
Yao, Yu [1 ]
Yu, Yan [1 ,2 ]
机构
[1] Univ Sci & Technol China, Dept Mat Sci & Engn, Hefei Natl Lab Phys Sci Microscale, CAS Key Lab Mat Energy Convers, Hefei 230026, Peoples R China
[2] Chinese Acad Sci, Dalian Natl Lab Clean Energy DNL, Dalian 116023, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
Li metal anode; 3D matrix; Electrolyte; Additive; Artificial SEI; Li metal battery; ELECTROLYTE INTERPHASE LAYER; POROUS CURRENT COLLECTOR; IN-SITU FORMATION; SOLID-ELECTROLYTE; PROTECTIVE LAYER; DOPED GRAPHENE; ION BATTERIES; CU FOAM; ELECTROCHEMICAL PERFORMANCE; FLUOROETHYLENE CARBONATE;
D O I
10.3866/PKU.WHXB202006021
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The Li metal anode is considered the most promising anode for next-generation high energy density batteries owing to its high theoretical capacity and low electrode potential. The development of batteries with high energy density is essential to meet the growing demand for energy storage devices in the modern world. However, the Li metal anode has operational problems. The high activity of Li causes dendritic growth during the cycling process, which leads to the cracking of the SEI (solid-electrolyte interphase), increased side reactions, and formation of dead Li. Furthermore, if the growth of Li dendrites is left uncontrolled, it can penetrate the separator and create a short-circuit accompanied by thermal runaway. Additionally, the complete utilization of active Li is challenged by the infinite volume expansion of the Li anode. To improve the application scope of Li metal batteries, it is imperative to develop advanced strategies for inhibiting Li dendritic growth, enhancing the stability of the SEI, reducing the accumulation of dead Li, and buffering the volume expansion. Understanding the mechanisms and models of Li nucleation and growth provides insight into solving these problems. This review summarizes some of the important models of Li nucleation and growth such as the surface nucleating model, charge-induced model, SEI model, and deposition/dissolution model. These models aid comprehension of the Li nucleation and growth process under various conditions. This review also discusses the strategies explored in the literature for improving the electrodes (such as three-dimensional (3D) matrix), electrolyte, SEI, and separator to realize uniform deposition of Li and improved utilization of Li. The 3D matrix strategy for improving the electrode design explores various matrices including graphene-based, carbon fiber-based, porous metal-based, and powder-based for buffering the volume expansion and reducing the local current density. To improve the electrolyte, concentrated lithium salts and functional additives are employed to stabilize the SEI and inhibit dendritic growth by regulating the chemical composition of SEI and inducing the deposition of Li. With respect to improving the design of the SEI, strategies for the construction of inorganic or organic components with high ionic conductivity and stable structure are explored for even distribution of Li ions and to avoid SEI rupture. This can reduce electrolyte consumption and dead Li formation. The modification of the separator by functional nanocarbon layer can control the direction of dendritic growth, thereby preventing the penetration of dendrites into the separator and achieving a uniform Li deposition layer. Finally, all solid state Li metal batteries (ASSLMBs) are discussed that utilize ceramic and polymer electrolytes owing to high safety of the solid state electrolyte. Therefore, reducing the interfacial resistance and suppressing dendritic growth between the Li anode and the electrolyte is key for the practical applications of ASSLMBs. Overall, this review provides a summary and outlook for promoting the practical applications of Li metal batteries.
引用
收藏
页码:1 / 26
页数:26
相关论文
共 237 条
  • [1] Towards high performance Li metal batteries: Nanoscale surface modification of 3D metal hosts for pre-stored Li metal anodes
    Adair, Keegan R.
    Iqbal, Muhammad
    Wang, Changhong
    Zhao, Yang
    Banis, Mohammad Norouzi
    Li, Ruying
    Zhang, Li
    Yang, Rong
    Lu, Shigang
    Sun, Xueliang
    [J]. NANO ENERGY, 2018, 54 : 375 - 382
  • [2] Long term stability of Li-S batteries using high concentration lithium nitrate electrolytes
    Adams, Brian D.
    Carino, Emily V.
    Connell, Justin G.
    Han, Kee Sung
    Cao, Ruiguo
    Chen, Junzheng
    Zheng, Jianming
    Li, Qiuyan
    Mueller, Karl T.
    Henderson, Wesley A.
    Zhang, Ji-Guang
    [J]. NANO ENERGY, 2017, 40 : 607 - 617
  • [3] Vacuum distillation derived 3D porous current collector for stable lithium-metal batteries
    An, Yongling
    Fei, Huifang
    Zeng, Guifang
    Xu, Xiaoyan
    Ci, Lijie
    Xi, Baojuan
    Xiong, Shenglin
    Feng, Jinkui
    Qian, Yitai
    [J]. NANO ENERGY, 2018, 47 : 503 - 511
  • [4] [Anonymous], 2018, ADV MATER, DOI DOI 10.1002/ADMA.201870122
  • [5] Building better batteries
    Armand, M.
    Tarascon, J. -M.
    [J]. NATURE, 2008, 451 (7179) : 652 - 657
  • [6] Review of selected electrode-solution interactions which determine the performance of Li and Li ion batteries
    Aurbach, D
    [J]. JOURNAL OF POWER SOURCES, 2000, 89 (02) : 206 - 218
  • [7] HISTORICAL DEVELOPMENT OF SECONDARY LITHIUM BATTERIES
    BRANDT, K
    [J]. SOLID STATE IONICS, 1994, 69 (3-4) : 173 - 183
  • [8] Dendritic growth mechanisms in lithium/polymer cells
    Brissot, C
    Rosso, M
    Chazalviel, JN
    Lascaud, S
    [J]. JOURNAL OF POWER SOURCES, 1999, 81 : 925 - 929
  • [9] Bruce PG, 2012, NAT MATER, V11, P19, DOI [10.1038/NMAT3191, 10.1038/nmat3191]
  • [10] The electronic properties of graphene
    Castro Neto, A. H.
    Guinea, F.
    Peres, N. M. R.
    Novoselov, K. S.
    Geim, A. K.
    [J]. REVIEWS OF MODERN PHYSICS, 2009, 81 (01) : 109 - 162