摘要
Ceramic matrix composites are developmental high temperature materials. We focus on composites with SiC matrices, SiC fibers, and BN fiber coatings. High temperature oxidation/corrosion reactions are discussed for each of these constituents. SiC forms a highly protective SiO2 scale in pure oxygen, but problems arise in complex gas mixtures. These include: SiO(g) formation, Si-O-H(g) formation, impurity enhanced SiO2 formation, and fluxing of SiO2 in molten salts and slags. Refractory oxide coatings may minimize these effects. The major issue with these composites is oxidation of the BN fiber coating. The key reactions here are borosilicate glass formation, potential gettering of oxygen by SiC, and volatilization. We conclude with an oxidation study of an actual composite, which illustrates some of these effects.
引用
下载
收藏
页码:770 / 780
页数:11
相关论文
共 50 条
  • [21] Interfacial coatings on inorganic fibers for high temperature ceramic matrix composites
    Baklanova, Natalia
    Zima, Tatyana
    Titov, Anatoly
    Zaitsev, Boris
    HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 : 1392 - +
  • [22] High temperature brazing for SiC and SiCF/SiC ceramic matrix composites
    Riccardi, B
    Nannetti, CA
    Woltersdorf, J
    Pippel, E
    Petrisor, T
    ADVANCED SIC/SIC CERAMIC COMPOSITES: DEVELOPMENTS AND APPLICATIONS IN ENERGY SYSTEMS, 2002, 144 : 311 - 322
  • [23] Ceramic fibers for matrix composites in high-temperature engine applications
    Baldus, P
    Jansen, M
    Sporn, D
    SCIENCE, 1999, 285 (5428) : 699 - 703
  • [24] Study on the preparation of ceramic/graphite composites and their oxidation resistance at high temperature
    Wei Tong
    Fan Zhuangjun
    Liu Lang
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 : 823 - 825
  • [25] Effects of temperature and of oxidation on the interfacial smear stress between fibres and matrix in ceramic-matrix composites
    Reynaud, P
    Rouby, D
    Fantozzi, G
    ACTA MATERIALIA, 1998, 46 (07) : 2461 - 2469
  • [26] Synergistic Effects of Temperature and Oxidation on Matrix Cracking in Fiber-Reinforced Ceramic-Matrix Composites
    Li Longbiao
    Applied Composite Materials, 2017, 24 : 691 - 715
  • [27] Synergistic Effects of Temperature and Oxidation on Matrix Cracking in Fiber-Reinforced Ceramic-Matrix Composites
    Li Longbiao
    APPLIED COMPOSITE MATERIALS, 2017, 24 (03) : 691 - 715
  • [28] Effects of temperature and of oxidation on the interfacial shear stress between fibres and matrix in ceramic-matrix composites
    UMR CNRS, Villeurbanne, France
    Acta Mater, 7 (2461-2469):
  • [29] Effects of temperature and duration on oxidation of ceramic composites with silicon carbide matrix and carbon nanoparticles
    Lu, Youjun
    Wang, Yanmin
    Shen, Hongfang
    Pan, Zhidong
    Huang, Zhenkun
    Wu, Laner
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 590 : 368 - 373
  • [30] Low-temperature oxidation embrittlement of SiC (Nicalon™)/CAS ceramic matrix composites
    Plucknett, Kevin P.
    Lin, Hua-Tay
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (12) : 4050 - 4054