Possible scenarios for the causes of accelerated fireside corrosion of superheater tubes in coal-fired boilers

被引:8
|
作者
Wright, Ian G. [1 ]
Kung, Steve C. [2 ]
机构
[1] WrightHT Inc, Denver, CO 80211 USA
[2] Elect Power Res Inst, Charlotte, NC USA
关键词
Coal-fired boilers; superheaters and reheaters; fireside corrosion and Mechanisms; HOT CORROSION;
D O I
10.1080/09603409.2017.1334351
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Recent experience of rapid corrosion of superheater tubes in coal-fired boilers has led to the application of weld-overlay coatings, which have proved effective but are expensive and can degrade mechanical tube life. Lack of understanding of how such corrosion differs from the established mechanism involving low-melting, complex, alkali-iron trisulphates is a major obstacle to devising alternative protective measures. Suggested scenarios for such accelerated corrosion are considered, including (1) increased tube surface temperatures allowing other sulphate mixtures to melt, analogous to Hot Corrosion mechanisms in gas turbines; (2) changes in the corrosivity of tube deposits from carryover of reduced species; and (3) increased release of corrosive species from the coal under substoichiometric combustion conditions. The potential for such scenarios to change the corrosive environment is assessed on the basis of current mechanistic understanding, though the general lack of phase diagrams for relevant ternary and quaternary sulphate systems is a major drawback to specifying the processes involved.
引用
收藏
页码:316 / 326
页数:11
相关论文
共 50 条
  • [31] Study on Corrosion of Superheater in the Biomass-fired Boilers
    Song Yun-jing
    Shi Wen-hua
    VACUUM TECHNOLOGY AND SURFACE ENGINEERING - PROCEEDINGS OF THE 9TH VACUUM METALLURGY AND SURFACE ENGINEERING CONFERENCE, 2009, : 35 - 38
  • [32] Reducing superheater corrosion in wood-fired boilers
    Henderson, P
    Szakálos, P
    Pettersson, R
    Andersson, C
    Högberg, J
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2006, 57 (02): : 128 - 134
  • [33] STOP TUBE CORROSION AND WEAR IN COAL-FIRED POWER BOILERS.
    Meringolo, Vince
    1600, (125):
  • [34] EXTERNAL CORROSION IN COAL-FIRED BOILERS - ASSESSMENT FROM LABORATORY DATA
    CUTLER, AJB
    RAASK, E
    CORROSION SCIENCE, 1981, 21 (11) : 789 - 800
  • [35] MODULAR COAL-FIRED PACKAGED BOILERS
    不详
    CME-CHARTERED MECHANICAL ENGINEER, 1985, 32 (12): : 14 - 14
  • [36] PARTICULATE CONTROL FOR COAL-FIRED BOILERS
    ARDELL, M
    CHEMICAL ENGINEERING PROGRESS, 1979, 75 (08) : 78 - 82
  • [37] FABRIC FILTRATION COAL-FIRED FOR BOILERS
    DENNIS, R
    CHEMICAL ENGINEER-LONDON, 1978, (333): : 480 - 484
  • [38] A numerical study on the superheater tubes bundle of a 660 MW coal-fired supercritical boiler
    Nawaz, Muhammad
    Hamzaoui, Mondher
    Bukhari, Muhammad Dawood
    Mustafa, Ghulam
    Khan, Sami Ullah
    Aydi, Abdelkarim
    Kolsi, Lioua
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2024, 38 (17):
  • [39] EQUILIBRIUM SO3 PRESSURES OF INNER LAYERS OF FIRESIDE DEPOSITS FROM COAL-FIRED BOILERS
    ANDERSON, CH
    GODDARD, CW
    JOURNAL OF THE INSTITUTE OF FUEL, 1968, 41 (332): : 357 - &
  • [40] HIGH-TEMPERATURE CORROSION OF ALLOYS AND COATINGS IN OIL-FIRED AND COAL-FIRED BOILERS
    MEADOWCROFT, DB
    MATERIALS SCIENCE AND ENGINEERING, 1987, 88 : 313 - 320