Cryorolling effect on microstructure and mechanical properties of Fe-25Cr-20Ni austenitic stainless steel

被引:44
|
作者
Xiong, Yi [1 ,2 ]
He, Tiantian [3 ]
Wang, Junbei [1 ]
Lu, Yan [1 ]
Chen, Lufei [1 ]
Ren, Fengzhang [1 ,2 ]
Liu, Yuliang [1 ]
Volinsky, Alex A. [4 ]
机构
[1] Henan Univ Sci & Technol, Sch Mat Sci & Engn, Luoyang 471023, Peoples R China
[2] Collaborat Innovat Ctr Nonferrous Met, Luoyang 471023, Peoples R China
[3] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
[4] Univ S Florida, Dept Mech Engn, Tampa, FL 33620 USA
基金
中国国家自然科学基金;
关键词
Austenitic stainless steel; Cryorolling; Microstructure; Mechanical properties; STACKING-FAULT ENERGY; GRAIN-REFINEMENT; TENSILE BEHAVIOR; COLD WORK; DEFORMATION; DUCTILITY; NANOSTRUCTURES; TEMPERATURE; STRENGTH; ALLOYS;
D O I
10.1016/j.matdes.2015.09.029
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructure and mechanical properties of the Fe-25Cr-20Ni austenitic stainless steel after cryorolling with different reductions were investigated by means of optical, scanning and transmission electron microscopy, X-ray diffraction and mini-tensile testing. High density tangled dislocations and a small amount of deformation twins formed after 30% deformation. After 50% strain, a large amount of deformation twins was generated. Meanwhile, interactions between the twins and dislocations started to happen. As the strain increased to 70%, many deformation twins were produced and the interactions between the twins and dislocations were significantly enhanced. When the cryorolling was 90%, the grain size was refined to the nanometer scale. XRD analysis indicated that the diffraction peaks of the samples became broader with the strain increase. The yield strength and the ultimate strength increased from 305 MPa and 645 MPa (before deformation) to 1502 MPa and 1560 MPa (after 90% deformation), respectively. However, the corresponding elongation decreased from 40.8% to 6.4%. The tensile fracture morphology changed from typical dimple rupture to a mixture of quasi-cleavage and ductile fracture. After 90% deformation, the microhardness was 520 HV, which increased by 100% compared with the original un-deformed sample. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:398 / 405
页数:8
相关论文
共 50 条
  • [21] High Temperature Deformation Behavior of a Fe-25Ni-20Cr (Wt Pct) Austenitic Stainless Steel
    Alomari, Abdullah S.
    Kumar, N.
    Hawary, Mahmoud
    Murty, K. L.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2022, 53 (08): : 3194 - 3203
  • [22] Understanding Creep-Fatigue Interaction in Fe-25Ni-20Cr (wt%) Austenitic Stainless Steel
    Kumar, N.
    Alomari, A.
    Murty, K. L.
    CHALLENGES IN MECHANICS OF TIME-DEPENDENT MATERIALS (2018), VOL 2, 2019, : 33 - 38
  • [23] CORROSION OF FE-25CR-20NI ALLOY IN MOLTEN ALKALI CARBONATES
    HSU, HS
    HOWELL, M
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1987, 134 (03) : C110 - C110
  • [24] Influence of pre-oxidation on the corrosion and mechanical strength of Fe-25Cr and Fe-25Cr-20Ni alloys at 973 K
    Sohn, Il Ryoung
    Narita, Toshio
    OXIDATION OF METALS, 2006, 65 (3-4): : 181 - 194
  • [25] Effect of Microstructure on Mechanical Properties of 316 LN Austenitic Stainless Steel
    Fang, Kewei
    Luo, Kunjie
    Wang, Li
    COATINGS, 2022, 12 (10)
  • [26] The effect of aging on the microstructure and mechanical behavior of the alumina-forming austenitic stainless steel Fe-20Cr-30Ni-2Nb-5Al
    Trotter, Geneva
    Baker, Ian
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 627 : 270 - 276
  • [27] Effect of Cu addition on microstructure and properties of Fe-20Ni-14Cr alumina-forming austenitic steel
    Gao, Qiuzhi
    Lu, Bingyi
    Ma, Qingshuang
    Zhang, Hailian
    Li, Huijun
    Liu, Ziyun
    INTERMETALLICS, 2021, 138
  • [28] Microstructure and mechanical properties of Ni-Cr stabilised austenitic cast steel
    Garbiak, M
    Piekarski, B
    Proceedings of the 2nd International Conference of DAAAM National Estonia, 2000, : 244 - 247
  • [29] The Effect of Cold Rolling on Microstructure and Mechanical Properties of a New Cr–Mn Austenitic Stainless Steel in Comparison with AISI 316 Stainless Steel
    Mehdi Mahmoudiniya
    Shahram Kheirandish
    Mohsen Asadiasadabad
    Transactions of the Indian Institute of Metals, 2017, 70 : 1251 - 1259
  • [30] Effect of Cryorolling–Annealing and Bake-Hardening on the Microstructure and Mechanical Properties of AISI 301LN Grade Austenitic Stainless Steel
    Debasish Chatterjee
    Metallography, Microstructure, and Analysis, 2020, 9 : 695 - 708