Indentation Deformation of a Cu47.5Zr19Hf28.5Al5 Bulk-Metallic Glass-Matrix Nanocomposite

被引:0
|
作者
Sun, Yuan [1 ,2 ]
Zhang, Dong [1 ]
Xin, Shaojie [1 ]
Yang, Fuqian [2 ]
机构
[1] Shanghai Dianji Univ, Sch Mech Engn, Shanghai 201306, Peoples R China
[2] Univ Kentucky, Mat Program, Dept Chem & Mat Engn, Lexington, KY 40506 USA
关键词
Metallic Glass; Plastic Flow; Indentation; STRUCTURAL RELAXATION; MECHANICAL-PROPERTIES; AMORPHOUS-ALLOYS; PLASTIC-FLOW; NANOINDENTATION; BEHAVIOR; NI; CRYSTALLIZATION; DECOMPOSITION; KINETICS;
D O I
10.1166/jnn.2020.16954
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
In this work, we study the indentation deformation of a Cu47.5Zr19Hf28.5Al5 bulk-metallic glass-matrix composite and characterize the effects of the indentation-loading rate and the holding time at the peak-indentation load. For the same peak-indentation load, increasing the holding time and/or decreasing the indentation-loading rate cause the increase of the indentation depth. There exists the "bulge" of the unloading curve at the onset of the unloading for small indentation-loading rates. The Vickers hardness is a monotonically increasing function of the indentation-loading rate for the same peak-indentation load. For the indentations with the same loading and unloading time of 30 s and without an intermediate stage at the peak-indentation load, the Vickers hardness of the Cu47.5Zr19Hf28.5Al5 bulk-metallic glass-matrix composite decreases with the increase of the indentation load. The strain energy dissipated through plastic deformation during the indentation is a power-law function of the indentation load with a power index of 3/2, and the energy ratio (total energy/plastic energy) linearly increases with the depth ratio (residual indentation depth/maximum indentation depth).
引用
收藏
页码:1530 / 1539
页数:10
相关论文
共 50 条
  • [21] Deformation behavior of thermally rejuvenated Zr-Cu-Al-(Ti) bulk metallic glass
    Ghodki, Nandita
    Jha, Shristy
    Alla, Siva Shankar
    Yang, Yu-Chia
    Pharr, George M.
    Mukherjee, Sundeep
    SCIENTIFIC REPORTS, 2024, 14 (01):
  • [22] Fabrication of Metastable Crystalline Nanocomposites by Flash Annealing of Cu47.5Zr47.5Al5 Metallic Glass Using Joule Heating
    Okulov, Ilya
    Soldatov, Ivan
    Kaban, Ivan
    Sarac, Baran
    Spieckermann, Florian
    Eckert, Juergen
    NANOMATERIALS, 2020, 10 (01)
  • [23] Work hardening ability of ductile Ti45Cu40Ni7.5Zr5Sn2.5 and Cu47.5Zr47.5Al5 bulk metallic glasses
    Kim, K. B.
    Das, J.
    Venkataraman, S.
    Yi, S.
    Eckert, J.
    APPLIED PHYSICS LETTERS, 2006, 89 (07)
  • [24] Effects of pre-compression on the microstructure, mechanical properties and corrosion resistance of Cu47.5Zr47.5Al5 bulk metallic glasses
    Zhai, Sicheng
    Axinte, Eugen
    Wang, Shouren
    Wang, Wen
    Xing, Qi
    Wang, Yan
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 481 : 383 - 390
  • [25] Study of micro indentation assisted deformation on HPT processed Zr62Cu22Al10Fe5Dy1 bulk metallic glass
    Jain, Abhilasha
    Prabhu, Yogesh
    Gunderov, Dmitry
    Ubyivovk, E. V.
    Bhatt, Jatin
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2021, 566
  • [26] Deformation behavior of a Zr55Al10Ni5Cu30 bulk metallic glass at high temperatures
    Shin, HS
    Jung, YJ
    Kim, KH
    Ahn, JH
    Kato, H
    Inoue, A
    Metastable, Mechanically Alloyed and Nanocrystalline Materials, 2005, 24-25 : 359 - 362
  • [27] Plastic deformation of bulk metallic glass Zr55Al10Ni5Cu30 during nanoindentation
    Yang, Fei
    Deng, Yufu
    Yang, Jianlin
    Zhang, Wei
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2007, 36 (04): : 578 - 582
  • [28] Plastic deformation of bulk metallic glass Zr55Al10Ni5Cu30 during nanoindentation
    Yang Fei
    Deng You
    Yang Jianlin
    Zhang Wei
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 (04) : 578 - 582
  • [29] Effect of Ta on glass formation, thermal stability and mechanical properties of a Zr52.25Cu28.5Ni4.75Al9.5Ta5 bulk metallic glass
    He, G
    Zhang, ZF
    Löser, W
    Eckert, J
    Schultz, L
    ACTA MATERIALIA, 2003, 51 (08) : 2383 - 2395
  • [30] Hydrogen-enhanced plastic deformation during indentation for bulk metallic glass of Zr65Al7.5Ni10Cu17.5
    Shan, G. B.
    Li, J. X.
    Yang, Y. Z.
    Qiao, L. J.
    Chu, W. Y.
    MATERIALS LETTERS, 2007, 61 (8-9) : 1625 - 1628