Toughening of reaction-bonded silicon nitride ceramics through microstructural design

被引:0
|
作者
Appiagyei, KA [1 ]
机构
[1] Kwame Nkrumah Univ Sci & Technol, Inst Min & Mineral Engn, Kumasi, Ghana
来源
关键词
reaction-bonded silicon nitride; beta-Si3N4; seed; fracture toughness; microstructure;
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The mechanical properties of silicon nitride ceramics (Si3N4) depend significantly on their microstructures. In this work, nitridation of silicon compacts (with 20 vol% SiC added as a second phase), containing 0, 1, 3, and 5 vol% respectively of an in-house prepared beta-Si3N4 seed particles of varying morphologies, was carried out at 1370degreesC for 20 hours. The nitridation product, a porous reaction-bonded silicon nitride-silicon carbide composite, was post-sintered in a gas pressure sintering furnace. Analysis of the post-sintered samples showed a bi-modal microstructure. The added beta-Si3N4 seed particles served as a nuclei for the epitaxial growth of large and elongated grains whilst another generation of beta-Si3N4 with relatively small grains developed from the alpha-beta transformation of silicon nitride during the liquid phase sintering process. Further microstructural analysis indicated that equiaxed seed particles gave rise to larger equiaxed grains whilst elongated beta-Si3N4 seed particles gave rise to larger elongated grains. In both cases, the grains showed a core- rim structure. Samples containing Si3N4 seed particles with the largest aspect ratio gave the best nitridation results. Evaluation of mechanical properties of post-sintered samples showed that those containing 3 vol% seed material had better properties than those that contained 1 or 5 vol%. Fracture toughness (K-IC) of about 8.5 MPa.m(1/2), an improvement of nearly 35% above the value for the sample without seed material used as the datum level for comparing results, was measured for samples that contained 3 vol% seed material. In the same samples, flexural strength of similar to 1000 MPa was obtained.
引用
收藏
页码:309 / 312
页数:4
相关论文
共 50 条
  • [31] Estimate of the Porous Structure Parameters of Reaction-Bonded Silicon Nitride
    Kryuchkov, Yu. N.
    GLASS AND CERAMICS, 2021, 78 (3-4) : 157 - 160
  • [32] DYNAMIC FRACTURE TOUGHNESSES OF REACTION-BONDED SILICON-NITRIDE
    KOBAYASHI, AS
    EMERY, AF
    LIAW, BM
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1983, 66 (02) : 151 - 155
  • [33] HIGH-STRENGTH REACTION-BONDED SILICON-NITRIDE
    RITTER, JE
    NAIR, SV
    GENNARI, PA
    DUNLAY, WA
    HAGGERTY, JS
    GARVEY, GJ
    ADVANCED CERAMIC MATERIALS, 1988, 3 (04): : 415 - 417
  • [34] STRENGTH OF REACTION-BONDED SILICON-NITRIDE WITH ARTIFICIAL PORES
    HEINRICH, J
    MUNZ, D
    AMERICAN CERAMIC SOCIETY BULLETIN, 1980, 59 (12): : 1221 - 1222
  • [35] OXIDATION PROTECTION OF POROUS REACTION-BONDED SILICON-NITRIDE
    FOX, DS
    JOURNAL OF MATERIALS SCIENCE, 1994, 29 (21) : 5693 - 5698
  • [36] Joining of reaction-bonded silicon carbide ceramics in green state
    Key Laboratory for Silicate Materials Science and Engineering, Wuhan University of Technology, Wuhan 430070, China
    Wuhan Ligong Daxue Xuebao, 2008, 3 (36-39):
  • [37] NONISOTHERMAL MICROWAVE PROCESSING OF REACTION-BONDED SILICON-NITRIDE
    THOMAS, JJ
    CHRISTENSEN, RJ
    JOHNSON, DL
    JENNINGS, HM
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (05) : 1384 - 1386
  • [38] Formation of reaction-bonded silicon nitride using microwave heating
    Thomas, JJ
    Skamser, DJ
    Jennings, HM
    Johnson, DL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (09) : 2458 - 2468
  • [39] FRACTURE SURFACE STUDIES ON REACTION-BONDED SILICON-NITRIDE
    DONLEY, MS
    STOEBE, TG
    AMERICAN CERAMIC SOCIETY BULLETIN, 1984, 63 (08): : 998 - 998
  • [40] VAPOR TRANSPORT OF MAGNESIA INTO REACTION-BONDED SILICON-NITRIDE
    PUGH, MD
    MOULSON, AJ
    JOURNAL OF MATERIALS SCIENCE, 1995, 30 (06) : 1425 - 1428