Research on the Performance of Diamond-Like Carbon Coatings on Cutting Aluminum Alloy: Cutting Experiments and First-Principles Calculations

被引:3
|
作者
Huang, Biao [1 ]
Zhang, Er-geng [1 ]
Zhou, Qiong [1 ]
Lin, Rong-chuan [2 ]
Du, Hao-ming [3 ]
机构
[1] Shanghai Inst Technol, Shanghai Engn Res Ctr Phys Vapor Deposit PVD Supe, Shanghai 201418, Peoples R China
[2] Jimei Univ, Sch Mech & Energy Engn, Xiamen 361021, Peoples R China
[3] Shanghai Dianji Univ, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
基金
上海市自然科学基金;
关键词
amorphous carbon; hydrogenated amorphous carbon; coating; first-principles molecular dynamics; machinability; aluminum alloy; MINIMUM QUANTITY LUBRICATION; TRIBOLOGICAL BEHAVIOR; POPULATION ANALYSIS; WEAR-RESISTANCE; DLC; TEMPERATURE; FRICTION; STRAIN; FILMS; MICROSTRUCTURE;
D O I
10.3390/coatings11010063
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The purpose of this study is to investigate the cutting performance of amorphous carbon (a-C) coatings and hydrogenated amorphous carbon (a-C:H) coatings on machining 2A50 aluminum alloy. First-principles molecular dynamics simulation was applied to investigate the effect of hydrogen on the interaction between coatings and workpiece. The cross-section topography and internal structure of a-C and a-C:H films were characterized by field emission scanning electron microscopy and Raman spectroscopy. The surface roughness of the deposited films and processed workpiece were measured using a white light interferometer. The results show that the a-C-coated tool had the highest service life of 121 m and the best workpiece surface quality (S-q parameter of 0.23 mu m) while the workpiece surface roughness S-q parameter was 0.35 and 0.52 mu m when machined by the a-C:H-coated and the uncoated tool, respectively. Meanwhile, the build-up edge was observed on the a-C:H-coated tool and a layer of aluminum alloy was observed to have adhered to the surface of the uncoated tool at its stable stage. An interface model that examined the interactions between H-terminated diamond (111)/Al(111) surfaces revealed that H atoms would move laterally with the action of cutting heat (549 K) and increase the interaction between a-C:H and Al surfaces; therefore, Al was prone to adhere to the a-C:H-coated tool surface. The a-C coating shows better performance on cutting aluminum alloy than the a-C:H coating.
引用
收藏
页码:1 / 11
页数:11
相关论文
共 50 条
  • [21] Understanding the friction behavior of sulfur-terminated diamond-like carbon films under high vacuum by first-principles calculations
    Zhang, Renhui
    Zhao, Juan
    Yang, Yingchang
    Shi, Wei
    Lu, Zhibin
    Wang, Junjun
    CURRENT APPLIED PHYSICS, 2018, 18 (03) : 317 - 323
  • [22] Deposition of Protective Nanostructured Diamond-Like Carbon Coatings on Aluminum Alloys
    V. K. Goncharov
    G. A. Gusakov
    M. V. Puzyrev
    Journal of Engineering Physics and Thermophysics, 2022, 95 : 693 - 699
  • [23] DEPOSITION OF PROTECTIVE NANOSTRUCTURED DIAMOND-LIKE CARBON COATINGS ON ALUMINUM ALLOYS
    Goncharov, V. K.
    Gusakov, G. A.
    Puzyrev, M. V.
    JOURNAL OF ENGINEERING PHYSICS AND THERMOPHYSICS, 2022, 95 (03) : 693 - 699
  • [24] Carbon adsorption on doped cementite surfaces for effective catalytic growth of diamond-like carbon: a first-principles study
    Yang, Yang
    Cui, Juan
    Li, Lei
    Lu, Hao
    Li, D. Y.
    Yan, M. F.
    PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2017, 19 (48) : 32341 - 32348
  • [25] Can the cutting performance of trephines still be improved? Application of nanotechnology for manufacturing trephines with diamond-like cutting edges
    Lingenfelder, C
    Kupferschmid, S
    Grabowy, U
    Kleinen, L
    Spraul, CW
    KLINISCHE MONATSBLATTER FUR AUGENHEILKUNDE, 2005, 222 (09) : 709 - 716
  • [26] Diamond-like carbon coating for aluminum 390 alloy - automotive applications
    Malaczynski, GW
    Hamdi, AH
    Elmoursi, AA
    Qiu, XH
    SURFACE & COATINGS TECHNOLOGY, 1997, 93 (2-3): : 280 - 286
  • [27] Frictional Coefficients between Aluminum–Silicon Alloy and Cutting Inserts with MPCVD Diamond Coatings
    Ashkinazi E.E.
    Ral’chenko V.G.
    Konov V.I.
    Vinogradov D.V.
    Tsygankov P.A.
    Dryzhak E.A.
    Khomich A.V.
    Russian Engineering Research, 2018, 38 (06) : 457 - 461
  • [28] Wear of Carbide Plates with Diamond-like and Micro-Nano Polycrystalline Diamond Coatings during Interrupted Cutting of Composite Alloy Al/SiC
    Ashkinazi, Evgeny E.
    Fedorov, Sergey V.
    Martyanov, Artem K.
    Sedov, Vadim S.
    Khmelnitsky, Roman A.
    Ralchenko, Victor G.
    Ryzhkov, Stanislav G.
    Khomich, Andrey A.
    Mosyanov, Mikhail A.
    Grigoriev, Sergey N.
    Konov, Vitaly I.
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2023, 7 (06):
  • [29] Friction and wear performance of diamond-like carbon and Cr-doped diamond-like carbon coatings in contact with steel surfaces
    Renondeau, H.
    Taylor, R. I.
    Smith, G. C.
    Torrance, A. A.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2008, 222 (J3) : 231 - 240
  • [30] Microscopic damage in eutectic SnPb alloy: First-principles calculations and experiments
    Wang, Changwei
    Jiang, Wen
    Han, Kangning
    Liu, Xin
    Zhu, Yaxin
    Xing, Ruisi
    Hou, Chuantao
    ENGINEERING FAILURE ANALYSIS, 2024, 164