EFFECT OF HEATING TEMPERATURE ON DEUTERIUM RETENTION BEHAVIOR FOR HELIUM/CARBON IMPLANTED TUNGSTEN

被引:8
|
作者
Sato, Misaki [1 ]
Yuyama, Kenta [1 ]
Li, Xiao-Chun [1 ]
Ashikawa, Naoko [2 ]
Sagara, Akio [2 ]
Yoshida, Naoaki [3 ]
Chikada, Takumi [1 ]
Oya, Yasuhisa [1 ]
机构
[1] Shizuoka Univ, Grad Sch Sci, Suruga Ku, Shizuoka 4228529, Japan
[2] Natl Inst Nat Sci, Natl Inst Fus Sci, Toki, Gifu 5095292, Japan
[3] Kyushu Univ, Appl Mech Res Inst, Kasuga, Fukuoka 8168580, Japan
关键词
IRRADIATION;
D O I
10.13182/FST14-971
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
The effect of heating temperature on deuterium (D) retention behavior for helium (He+) / carbon (C+) implanted tungsten (W) was studied. It was found that D retention behavior for He+ implanted W was not limited by the size of the He bubbles. The microstructure observation showed that the large helium bubbles were formed near the surface for He+ implanted W at 1173 K, suggesting that the D retention was reduced by the growth of the helium bubbles. In addition, to evaluate the effect of implantation ion species at high temperature, D retention behavior for He+ implanted W at 1173 K was compared with that for C+ implanted W at 673 K It is concluded that the D retention depends on ion species, which makes different kinds of damages like He bubbles for He+ implantation and vacancy-ion complex (voids) for C+ implantation.
引用
收藏
页码:531 / 534
页数:4
相关论文
共 50 条
  • [21] Helium effects on tungsten surface morphology and deuterium retention
    Ueda, Y.
    Peng, H. Y.
    Lee, H. T.
    Ohno, N.
    Kajita, S.
    Yoshida, N.
    Doerner, R.
    De Temmerman, G.
    Alimov, V.
    Wright, G.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 442 (1-3) : S267 - S272
  • [22] Retention of ion-implanted deuterium in tungsten pre-irradiated with carbon ions
    Alimov, VK
    Ertl, K
    Roth, J
    Schmid, K
    JOURNAL OF NUCLEAR MATERIALS, 2000, 282 (2-3) : 125 - 130
  • [23] Effect of carbon pre-implantation on deuterium retention in tungsten
    Poon, M
    Davis, JW
    Haasz, AA
    JOURNAL OF NUCLEAR MATERIALS, 2000, 283 : 1062 - 1067
  • [24] Effects of helium bombardment on the deuterium behavior in tungsten
    Iwakiri, H
    Morishita, K
    Yoshida, N
    JOURNAL OF NUCLEAR MATERIALS, 2002, 307 (1 SUPPL.) : 135 - 138
  • [25] Dependence of implantation temperature on chemical behavior of energetic deuterium implanted into tungsten carbide
    Igarashi, E.
    Nishikawa, Y.
    Nakahata, T.
    Yoshikawa, A.
    Oyaidzu, M.
    Oya, Y.
    Okuno, K.
    JOURNAL OF NUCLEAR MATERIALS, 2007, 363 : 910 - 914
  • [26] Role of grain boundaries and carbon deposition in deuterium retention behavior of deuterium plasma exposed tungsten
    Komarov, DA
    Markin, AV
    Rybakov, SY
    Zakharov, AP
    JOURNAL OF NUCLEAR MATERIALS, 2001, 290 : 433 - 436
  • [27] Retention and re-emission of deuterium implanted into tungsten monocarbide
    Horikawa, T
    Tsuchiya, B
    Morita, K
    JOURNAL OF NUCLEAR MATERIALS, 1998, 258 : 1087 - 1091
  • [28] Influence of tungsten-carbon mixed layer and irradiation defects on deuterium retention behavior in tungsten
    Miura, Ryo
    Fujishima, Tetsuo
    Uchimura, Hiromichi
    Toda, Kensuke
    Kobayashi, Makoto
    Ashikawa, Naoko
    Sagara, Akio
    Yoshida, Naoaki
    Hatano, Yuji
    Oya, Yasuhisa
    Okuno, Kenji
    FUSION ENGINEERING AND DESIGN, 2013, 88 (9-10) : 1827 - 1830
  • [29] Deuterium retention in tungsten mixed carbon dust
    Yoshida, H
    Hino, T
    Akiba, M
    Suzuki, S
    Nakamura, K
    Yamauchi, Y
    Hirohata, Y
    MATERIALS TRANSACTIONS, 2005, 46 (03) : 557 - 560
  • [30] Effect of initial exposure temperature on the deuterium retention and surface blistering in tungsten
    Wang, Ting
    Ren, Mengchong
    Zhu, Xiu-Li
    Ma, Xiaolei
    Yuan, Yue
    Cheng, Long
    Lu, Guang-Hong
    NUCLEAR MATERIALS AND ENERGY, 2022, 33