摘要
We have studied the effects of localized defects in the YBCO coated conductors on the critical current. The artificial defects were introduced into 4, 10 and 12 mm wide tapes as cuts of various lengths made either by laser ablation or mechanical means. Transport measurements were carried out in an external variable magnetic field to obtain the I-V characteristics of the damaged areas. The distribution of the magnetic field in the vicinity of the defects has been mapped as well. The reduction of the critical current by the defects, with and without an external DC magnetic field are discussed and compared with existing theories. A criterion for determining the critical current in the area containing a defect is suggested.
引用
收藏
页码:2921 / 2924
页数:4
相关论文
共 50 条
  • [41] The reversible strain effect on critical current over a wide range of temperatures and magnetic fields for YBCO coated conductors
    Sugano, Michinaka
    Shikimachi, Kouji
    Hirano, Naoki
    Nagaya, Shigeo
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2010, 23 (08):
  • [42] Study on dependence of AC transport current losses in YBCO-coated conductors on distribution of critical current density and n value
    Miyagi, D
    Tsukamoto, O
    ELECTRICAL ENGINEERING IN JAPAN, 2005, 152 (02) : 26 - 38
  • [43] Temperature dependence of critical current and transport current losses of 4 mm YBCO coated conductors manufactured using nonmagnetic substrate
    Kvitkovic, J.
    Hatwar, R.
    Pamidi, S. V.
    Fleshier, S.
    Thieme, C.
    ADVANCES IN CRYOGENIC ENGINEERING - MATERIALS: PROCEEDINGS OF THE INTERNATIONAL CRYOGENIC MATERIALS CONFERENCE (ICMC) 2015, 2015, 102
  • [44] Large enhancement of the in-field critical current density of YBCO coated conductors due to composite pinning landscape
    Kihlstrom, K. J.
    Civale, L.
    Eley, S.
    Miller, D. J.
    Welp, U.
    Kwok, W. K.
    Niraula, P.
    Kayani, A.
    Ghigo, G.
    Laviano, F.
    Fleshler, S.
    Rupich, M.
    Leroux, M.
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2021, 34 (01):
  • [45] Enhancement of critical current in YBCO coated conductors in association with c-axis correlated artificial pinning centers
    Inoue, M.
    Kiss, T.
    Motoyama, K.
    Nakamura, T.
    Fujiwara, T.
    Mitsui, D.
    Awaii, S.
    Watanabe, K.
    Ibi, A.
    Takahashi, K.
    Miyata, S.
    Yamada, Y.
    Shiohara, Y.
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2007, 463 (674-677): : 674 - 677
  • [46] Critical current properties in YBCO coated IBAD tapes
    Inoue, M
    Nishimura, S
    Kuga, T
    Kiuchi, M
    Kiss, T
    Takeo, M
    Matsushita, T
    Iijima, Y
    Kakimoto, K
    Saitoh, T
    Awaji, S
    Watanabe, K
    Shiohara, Y
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2002, 372 : 794 - 797
  • [47] Improving YBCO coated conductors for applications
    Barnes, P. N.
    Harrison, B. C.
    Kell, J. W.
    Levin, G. A.
    Sumption, M. D.
    ADVANCES IN CRYOGENIC ENGINEERING, VOL 52A & 52B, 2006, 824 : 425 - +
  • [48] YBCO Coated Conductors for Fusion Magnets
    Fuger, Rene
    Eisterer, Michael
    Weber, Harald W.
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2009, 19 (03) : 1532 - 1535
  • [49] Stability measurements on YBCO coated conductors
    Armenio, A. Angrisani
    Augieri, A.
    Celentano, G.
    Galluzzi, V.
    Mancini, A.
    Rufoloni, A.
    Vannozzi, A.
    Gambardella, U.
    Saggese, A.
    Sessa, P.
    Pace, S.
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2008, 18 (02) : 1293 - 1296
  • [50] Numerical analysis of YBCO coated conductors
    Jaroszynski, Leszek
    Czerwinski, Dariusz
    PRZEGLAD ELEKTROTECHNICZNY, 2012, 88 (10B): : 160 - 162