Indentation crack length anisotropy in silicon nitride with aligned reinforcing grains

被引:0
|
作者
Park, DS [1 ]
Kim, CW [1 ]
机构
[1] Korea Inst Machinery & Mat, Ceram Mat Grp, Chang Won City, South Korea
关键词
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Vickers indentation was performed on surfaces of silicon nitride with an aligned microstructure in order to study the interaction between cracks and the microstructure, Although there was not much evidence of crack bridging, the transverse radial cracks were very short, resulting in high fracture toughness values. The longitudinal radial cracks tended to propagate along the grain boundary of the reinforcements and were much longer than the transverse cracks. As the sintering temperature increased, the lateral cracks on the casting surface led to spalling and consumed more energy for the crack formation, making the longitudinal cracks shorter. On the surface normal to the alignment direction, there was no spalling and the indentation cracks became longer as the sintering temperature increased.
引用
收藏
页码:663 / 665
页数:3
相关论文
共 50 条
  • [31] Indentation cracking of monocrystalline silicon considering fracture anisotropy
    Rickhey, Felix
    Marimuthu, Karuppasamy Pandian
    Lee, Kwangmin
    Lee, Hyungyil
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2019, 100 : 128 - 138
  • [32] Study of depth profile of indentation cracks in silicon nitride
    Gondár, E
    Rosko, M
    Zemánková, M
    KOVOVE MATERIALY-METALLIC MATERIALS, 2005, 43 (02): : 124 - 133
  • [33] Statistical properties of indentation toughness for silicon nitride ceramic
    Wang, JQ
    Gong, JH
    Guan, ZD
    RARE METAL MATERIALS AND ENGINEERING, 2002, 31 : 145 - 147
  • [34] Effect of Crack Length on Strength Recovery of Silicon-Carbide-Whisker-Reinforced Silicon Nitride Upon Healing Treatment
    Hu, Jun Feng
    Deng, Xi
    Yang, Yong
    Chen, Zhou
    SCIENCE OF ADVANCED MATERIALS, 2019, 11 (12) : 1723 - 1730
  • [35] CYCLIC FATIGUE-CRACK GROWTH FROM INDENTATION FLAW IN SILICON-NITRIDE INFLUENCE OF EFFECTIVE STRESS RATIO
    CHOI, G
    HORIBE, S
    KAWABE, Y
    ACTA METALLURGICA ET MATERIALIA, 1994, 42 (11): : 3837 - 3842
  • [36] Post-indentation subcritical (slow) crack growth in whisker-reinforced silicon nitride ceramic matrix composites
    Solomah, A.G.
    Tucci, A.
    Esposito, L.
    Ceramic Engineering and Science Proceedings, 1996, 17 (03): : 303 - 313
  • [37] Effect of reinforcing of silicon-nitride matrix with whisker crystals of silicon carbide
    Kelina, I.Yu.
    Ershova, N.I.
    Plyasunkova, L.A.
    2000, Metteks (OOO) : 14 - 19
  • [38] Crack detection in silicon nitride by acoustic microscopy
    Lawrence, C.W.
    Scruby, C.B.
    Briggs, G.A.D.
    Dunhill, A.
    1600, (23):
  • [39] Crack healing in silicon nitride and alumina ceramics
    Natl Inst for Research in Inorganic, Materials, Ibaraki, Japan
    J Mater Sci Lett, 22 (1976-1978):
  • [40] Numerical analysis of crack propagation in silicon nitride
    Karaszewski W.
    Key Engineering Materials, 2011, 490 : 216 - 225