Indentation Fracture Resistance Vs Conventional Fracture Toughness of Carbon Nanotube/Alumina Nanocomposites

被引:5
|
作者
Sarkar, Soumya [1 ]
Das, Probal Kumar [1 ]
机构
[1] Cent Glass & Ceram Res Inst, CSIR, Nonoxide Ceram & Composites Div, Kolkata 700032, India
关键词
ALUMINA MATRIX; MECHANICAL-PROPERTIES; BRITTLE SOLIDS; NANOTUBES; MICROSTRUCTURE; GRAPHENE;
D O I
10.1007/s11661-015-3086-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Multiwalled carbon nanotube (MWCNT)/alumina (Al2O3) nanocomposites were fabricated using two varieties of CNT to access the effect of morphological variation of the filler on fracture resistance (K (R))/toughness (K (IC)) of studied specimens. Special attention was also given to compare K (R) and K (IC) values for tracing out the primary selection criterion of appropriate indentation fracture (IF) equation used in relatively faster and simpler 'direct crack measurement' (DCM) technique to evaluate K (R) values close to stringent 'single edge notched beam' (SENB) derived K (IC) data. While K (IC) was calculated using the unique expression suitable for specimens tested under four-point flexure, K (R) values were evaluated using a series of IF equations suitable for Palmqvist and/or median crack systems. As far as change in K (R) and/or K (IC) of nanocomposites was concerned, it was noticed that for longer/thicker CNTs having relatively higher internal bamboo structures, much lower amount (0.15 vol pct) was adequate to achieve the highest improvement in K (R) (similar to 87 pct) or K (IC) (similar to 50 pct) over pure Al2O3 ((Laugier) K (R) a parts per thousand 3.83 MPa-m(0.5); K (IC) a parts per thousand 3.48 MPa-m(0.5)) than that required for smaller/thinner CNTs (a parts per thousand yen0.3 vol pct). On contrary, resistance to fracture up to 1.2 vol pct CNT loading was much enhanced in specimens fabricated with smaller/thinner CNTs over those fabricated using longer/thicker CNTs. Comparatively better morphology, adequate CNT dispersion, and higher population of bridging elements in specimens containing smaller/thinner CNTs were the key factors behind such toughness retention. (C) The Minerals, Metals & Materials Society and ASM International 2015
引用
收藏
页码:5072 / 5079
页数:8
相关论文
共 50 条
  • [41] Impact of carbon nanotube defects on fracture mechanisms in ceramic nanocomposites
    Yang, Yingchao
    Ramirez, Cristina
    Wang, Xing
    Guo, Zhixing
    Tokranov, Anton
    Zhao, Ruiqi
    Szlufarska, Izabela
    Lou, Jun
    Sheldon, Brian W.
    CARBON, 2017, 115 : 402 - 408
  • [42] Fatigue and Fracture Toughness of Epoxy Nanocomposites
    Srivastava, I.
    Koratkar, N.
    JOM, 2010, 62 (02) : 50 - 57
  • [43] Fatigue and fracture toughness of epoxy nanocomposites
    I. Srivastava
    N. Koratkar
    JOM, 2010, 62 : 50 - 57
  • [44] Fracture toughness of the sidewall fluorinated carbon nanotube-epoxy interface
    Ganesan, Yogeeswaran
    Salahshoor, Hossein
    Peng, Cheng
    Khabashesku, Valery
    Zhang, Jiangnan
    Cate, Avery
    Rahbar, Nima
    Lou, Jun
    JOURNAL OF APPLIED PHYSICS, 2014, 115 (22)
  • [45] Electrochemical impedance interpretation for the fracture toughness of carbon nanotube/cement composites
    Li, Wei-wen
    Ji, Wei-ming
    Fang, Guo-hao
    Liu, Yu-qing
    Xing, Feng
    Liu, Yu-kai
    Dong, Bi-qin
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 114 : 499 - 505
  • [46] Toughness enhancement for interlaminar fracture composite based on carbon nanotube films
    Yu Y.
    Zhang Y.
    Gao L.
    Qu S.
    Lyu W.
    Hangkong Xuebao/Acta Aeronautica et Astronautica Sinica, 2019, 40 (10):
  • [47] Carbon Nanotube Reinforced Composites: The Smaller Diameter, the Higher Fracture Toughness?
    Chen, Yuli
    Wang, Zhiyong
    Wang, Shengtao
    Zhou, Zhenggang
    Zhang, Jianyu
    Liu, Bin
    JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 2015, 82 (08):
  • [48] INDENTATION FRACTURE OF CEMENTED CARBIDE .2. NATURE OF SURFACE FRACTURE TOUGHNESS
    PERROTT, CM
    WEAR, 1978, 47 (01) : 81 - 91
  • [49] Refined measurements of indentation fracture resistance of alumina using powerful optical microscopy
    Miyazaki, Hiroyuki
    Yoshizawa, Yu-ichi
    CERAMICS INTERNATIONAL, 2014, 40 (02) : 2777 - 2783
  • [50] Fracture toughness of liquid phase sintered SiC by using indentation fracture method
    Jung, HC
    Yoon, HK
    Kim, BA
    Park, JS
    Kohyama, A
    ADVANCES IN FRACTURE AND STRENGTH, PTS 1- 4, 2005, 297-300 : 137 - 142