Research on Wear Behavior of Different Graphite Contents of NBR Under Dry Sliding

被引:0
|
作者
Yang, Fengyan [1 ]
Sun, Yingnan [2 ]
Wang, Shijie [2 ]
机构
[1] Shenyang Univ Technol, Shenyang Aviat Vocat Tech Coll, Sch Mech Engn, Shenyang, Peoples R China
[2] Shenyang Univ Technol, Sch Mech Engn, Shenyang, Peoples R China
关键词
graphite; NBR; dry sliding; friction and wear;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
NBR is an important material used for the stator of progressing cavity pump. The wear mechanisms of different graphite contents of NBR by 45# steel under different loads were investigated. On MPV-600 computer-controlled abrasive wear testing machine, the coefficients of friction were measured continuously. Results showed that wear loss and friction coefficient of NBR decrease with the increasing of graphite contents; at low content of graphite, due to low hardness, large amount of elastic deformation, adhesive wear of NBR can be found, in the high content of graphite, abrasive wear is showed.
引用
收藏
页码:1037 / 1039
页数:3
相关论文
共 50 条
  • [31] Investigation of Dry Sliding Wear Behavior of Different Diamond Segments with Response Surface Methodology
    Bilal Kursuncu
    Azmi Erdoğan
    Derviş Özkan
    Yılmaz Küçük
    Mustafa Sabri Gök
    Gizem Yılmaz
    Journal of Materials Engineering and Performance, 2023, 32 : 10793 - 10804
  • [32] Investigation of Dry Sliding Wear Behavior of Different Diamond Segments with Response Surface Methodology
    Kursuncu, Bilal
    Erdogan, Azmi
    Ozkan, Dervis
    Kucuk, Yilmaz
    Gok, Mustafa Sabri
    Yilmaz, Gizem
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (23) : 10793 - 10804
  • [33] Wear behavior of Fe-Cr-B alloys under dry sliding condition
    Cui, Gongjun
    Wei, Jin
    Wu, Gongxiong
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2015, 67 (04) : 336 - 343
  • [34] Wear behavior of copper-containing ferritic iron under a dry sliding condition
    Syarif, Junaidi
    Iswadi, Agung
    Ghazali, Mariyam Jameelah
    Sajuri, Zainuddin
    Omar, Mohd Zaidi
    JOURNAL OF ZHEJIANG UNIVERSITY-SCIENCE A, 2013, 14 (12): : 906 - 914
  • [35] Wear behavior of copper-containing ferritic iron under a dry sliding condition
    Junaidi SYARIF
    Agung ISWADI
    Mariyam Jameelah GHAZALI
    Zainuddin SAJURI
    Mohd Zaidi OMAR
    Journal of Zhejiang University-Science A(Applied Physics & Engineering), 2013, (12) : 906 - 914
  • [36] The influence of surface crack on the wear behavior of polyamide 66 under dry sliding condition
    Abdelbary, A.
    Abouelwafa, M. N.
    El Fahham, I. M.
    Hamdy, A. H.
    WEAR, 2011, 271 (9-10) : 2234 - 2241
  • [37] Friction and wear behavior of surface nanocrystallized aluminium alloy under dry sliding condition
    Prakash, N. Arun
    Gnanamoorthy, R.
    Kamaraj, M.
    MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2010, 168 (1-3): : 176 - 181
  • [38] Investigation of Wear Behavior for Novel Polyamide 66 Composites Under Dry Sliding Conditions
    Abdullah, Orhan S.
    Hassan, Shaker S.
    Al-Khazraji, Ahmed N.
    INTERNATIONAL JOURNAL OF NANOELECTRONICS AND MATERIALS, 2020, 13 (01): : 9 - 17
  • [39] Wear behavior of high strength and high conductivity Cu alloys under dry sliding
    Gao, Yuan
    Jie, Jin-chuan
    Zhang, Peng-chao
    Zhang, Jian
    Wang, Tong-min
    Li, Ting-ju
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (07) : 2293 - 2300
  • [40] Wear behavior of copper-containing ferritic iron under a dry sliding condition
    Junaidi SYARIF
    Agung ISWADI
    Mariyam Jameelah GHAZALI
    Zainuddin SAJURI
    Mohd Zaidi OMAR
    Journal of Zhejiang University-Science A(Applied Physics & Engineering), 2013, 14 (12) : 906 - 914