Scale effect in mechanical characterization of WC-Co composites

被引:19
|
作者
Sandoval, D. A. [1 ,2 ]
Rinaldi, A. [3 ]
Tarrago, J. M. [4 ,6 ]
Roa, J. J. [1 ,2 ]
Fair, J. [5 ]
Llanes, L. [1 ,2 ]
机构
[1] Univ Politecn Cataluna, EEBE, CIEFMA, Dept Mat Sci & Met, Campus Diagonal Besos, Barcelona 08930, Spain
[2] Univ Politecn Cataluna, Barcelona Res Ctr Multiscale Sci & Engn, Campus Diagonal Besos, Barcelona, Spain
[3] Italian Natl Agcy New Technol Energy & Sustainabl, Rome, Italy
[4] Sandvik Min & Rock Technol, Rock Tools R&D, Stockholm, Sweden
[5] Sandvik Hyper, Coventry, W Midlands, England
[6] Sandvik Hyper, Barcelona 08107, Spain
关键词
WC-Co; Size effect; Micropillar; Uniaxial compression; Plastic deformation; Failure mechanisms; MICROPILLAR COMPRESSION; DEFORMATION; NANOINDENTATION; PLASTICITY; STRENGTH; BINDER; METHODOLOGY; BEHAVIOR;
D O I
10.1016/j.ijrmhm.2017.12.029
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The study of mechanical response of materials at small length scales has gained importance due to the recent advances in micro- and nano-fabrication as well as testing systems. However, most of the reported work has been dedicated to investigate single-crystals or boundary-containing metallic systems, while much less attention has been paid to composite materials, and in particular those combining soft and hard phases. In this work, a systematic procedure is followed for machining micropillars of diameters ranging from 1 to 4 pm in a WC-Co composite with a WC mean grain size around 1 pm, by means of focused ion beam milling. In-situ uniaxial compression of the micropillars and subsequent field emission scanning electron microscopy inspection were conducted. Clear size effects are evidenced. Smaller test specimens (probe size approaching the mean WC size) exhibit deformation/failure mechanisms observed for WC crystals; while for bigger sample sizes, the mechanical response involves several mechanisms directly linked with the microstructural characteristics of the bulk-like cemented carbide material. On the other hand, independent of micropillar size, carbide-carbide or carbide binder interfaces are found to be preferential sites for nucleation of critical damage events.
引用
收藏
页码:157 / 162
页数:6
相关论文
共 50 条
  • [31] The Effect of Substitution of WC by TiC in WC-Co Composite Tool Materials on Microstructure and Mechanical Properties
    Dutkiewicz, Jan
    Rogal, Lukasz
    Bobrowski, P.
    Szutkowska, Gorzata
    Lesniewski, Wojciech
    Dluzewski, Piotr
    CHIANG MAI JOURNAL OF SCIENCE, 2017, 44 (04): : 1714 - 1721
  • [32] Comparative studies on mechanical properties of WC-Co composites sintered by SPS and conventional techniques
    Pristinskiy, Yuri
    Peretyagin, Nikita
    Pinargote, Nestor Washington Solis
    INTERNATIONAL CONFERENCE ON MODERN TRENDS IN MANUFACTURING TECHNOLOGIES AND EQUIPMENT (ICMTMTE 2017), 2017, 129
  • [33] Synthesis and Characterization of Nanostructured WC-Co/Al Powder Prepared by Mechanical Alloying
    Ma, Ning
    Zhang, Keke
    Yin, Danqing
    Zhao, Di
    Zhu, Zhiwei
    Ye, Fuxing
    JOURNAL OF NANOMATERIALS, 2016, 2016
  • [34] Effect of Joining Condition on Plastic Deformation, Microstructure and Bonding Strength for WC-Co to WC-Co
    Gonda, Hidenobu
    Shirai, Yasuhiro
    Yasui, Toshiaki
    Ohashi, Osamu
    Fukumoto, Masahiro
    STEEL RESEARCH INTERNATIONAL, 2010, 81 (09) : 1156 - 1159
  • [35] Indentation hardness and fatigue of the constituents of WC-Co composites
    B̘anda, Marek
    Duszová, Annamaria
    Csanádi, Tamás
    Hvizdoš, Pavol
    Lofaj, František
    Dusza, Ján
    International Journal of Refractory Metals and Hard Materials, 2015, 49 : 178 - 183
  • [36] Indentation hardness and fatigue of the constituents of WC-Co composites
    Blanda, Marek
    Duszová, Annamaria
    Csanádi, Tamás
    Hvizdoš, Pavol
    Lofaj, František
    Dusza, Ján
    International Journal of Refractory Metals and Hard Materials, 2015, 49 (01) : 178 - 183
  • [37] Wear resistance of HIPed steel/WC-Co composites
    Angers, R.
    Dube, D.
    Champagne, B.
    International Journal of Refractory Metals and Hard Materials, 1988, 7 (03) : 149 - 151
  • [38] A computational framework for micromechanical modelling of WC-Co composites
    Machado, Pedro Vinicius Sousa
    Caner, Ferhun C.
    Llanes, Luis
    Pique, Emilio Jimenez
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2023, 111
  • [39] Microwave processing of WC-Co composites and ferroic titanates
    Cheng, JP
    Agrawal, DK
    Komarneni, S
    Mathis, M
    Roy, R
    MATERIALS RESEARCH INNOVATIONS, 1997, 1 (01) : 44 - 52
  • [40] Wear resistance and fracture mechanics of WC-Co composites
    Kaytbay, Saleh
    El-Hadek, Medhat
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2014, 105 (06) : 557 - 565